# US 2009/0274982 A1 · Method of making a semiconductor device using negative photoresist

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0274982 A1
- Document ID: US20090274982A1
- Status: Published application
- Kind: A1
- Application number: 12/112,058
- Filed: 2008-04-30
- Published: 2009-11-05
- Earliest claimed: 2008-04-30
- Assignees: Freescale Semiconductor, Inc.
- Inventors: Willard E. Conley
- Web page: https://patentgrep.com/patent/US20090274982A1

## CPC

- H10P 50/73: {using masks for insulating materials}
- H10W 20/081: {by forming openings in the dielectric parts}
- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Negative photoresist over an insulating layer is exposed to radiation according to a pattern for an opening in the insulating layer for filling conductive material. A post of the negative photoresist is left over the location where the opening in the insulating layer is to be formed. A developable hard mask is formed over the post by a spin-on process so that the hard mask over the post is much thinner than directly over the insulating layer. An etch back is performed to remove the hard mask from over the post so that the post of negative photoresist is thus exposed. The post is removed to form an opening in the hard mask. An etch is performed to form the opening in the insulating layer aligned to the opening in the hard mask. The opening in the insulating layer is filled with the conductive material.

## Claims

### Claim 1

A method of forming openings in the fabrication of a device comprising:
forming an anti-reflective coating layer overlying a target layer in which desired openings are to be formed;
forming a negative photoresist layer overlying the anti-reflective coating layer;
exposing the negative photoresist layer with focused exposure energy according to a given positive pattern mask of the openings to be formed, wherein exposing according to the positive pattern mask creates exposed portions and unexposed portions of the negative photoresist layer;
developing the exposed negative photoresist layer, wherein developing removes unexposed portions of the negative photoresist layer to uncover corresponding portions of the anti-reflective coating layer, and wherein the exposed portions of the negative photoresist layer remain to create a negative pattern mask of the positive pattern mask;
forming a spin-on developable hard mask layer overlying the negative pattern mask and the uncovered portions of the anti-reflective coating layer;
removing the spin-on developable hard mask layer overlying the negative pattern mask by at least an amount sufficient to uncover the patterned negative photoresist layer;
removing the negative pattern mask, wherein removing the negative pattern mask forms a subsequent positive pattern mask out of a remainder portion of the spin-on developable hard mask layer; and
etching the anti-reflection coating layer and the target layer according to the subsequent positive pattern mask, wherein etching forms the desired openings within the target layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the steps of forming the anti-reflective coating layer, forming the negative photoresist layer, exposing the negative photoresist layer, developing the exposed negative photoresist layer, forming the spin-on developable hard mask layer, removing the spin-on developable hard mask layer overlying the negative patter mask are all performed within a same photo cluster.

### Claim 3 (depends on 1)

The method of claim 1, wherein the anti-reflective coating layer comprises a silicon anti-reflective coating.

### Claim 4 (depends on 1)

The method of claim 1, wherein the exposure energy comprises energy in the range of 1-200 mJ/cm2.

### Claim 5 (depends on 4)

The method of claim 4, further wherein the exposure energy comprises energy in the range of 20-30 mJ/cm2.

### Claim 6 (depends on 1)

The method of claim 1, wherein developing the exposed negative photoresist layer comprises using an aqueous developer solution.

### Claim 7 (depends on 1)

The method of claim 1, wherein removing the spin-on developable hard mask layer includes developing the spin-on developable hard mask layer in an aqueous solution until the spin-on developable hard mask layer is of a thickness less than a thickness of the patterned negative photoresist layer overlying the anti-reflective coating layer.

### Claim 8 (depends on 7)

The method of claim 7, further wherein the aqueous solution comprises a high pH developer solution.

### Claim 9 (depends on 8)

The method of claim 8, further wherein the high pH developer solution comprises tetra methyl ammonium hydroxide (TMAH) and water.

### Claim 10 (depends on 1)

The method of claim 1, wherein removing the negative pattern mask includes using an etch having selectivity to the subsequent positive pattern mask.

### Claim 11 (depends on 10)

The method of claim 10, further wherein the etch comprises a plasma etch.

### Claim 12 (depends on 1)

The method of claim 1, wherein etching the anti-reflective coating layer and the target layer includes using an etch having selectivity to the subsequent positive pattern mask.

### Claim 13 (depends on 12)

The method of claim 12, further wherein the etch comprises a plasma etch.

### Claim 14 (depends on 1)

The method of claim 1, further comprising:
removing the subsequent positive pattern mask overlying the target layer; and
forming a conductive material within the desired openings of the target layer.

### Claim 15 (depends on 1)

The method of claim 1, wherein the target layer comprises an interlevel dielectric layer of a semiconductor substrate structure, wherein the semiconductor substrate structure comprises a semiconductor substrate including circuitry, an insulating layer overlying the semiconductor substrate, and at least one contact area within the insulating layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the interlevel dielectric having a thickness on the order of 150 nm, the anti-reflective coating having a thickness on the order of 35 nm, the negative photoresist layer having a thickness in a range on the order of 40-70 nm, and the spin-on developable hard mask layer having a thickness in the range on the order of 30-60 nm.

### Claim 17 (depends on 1)

The method of claim 1, wherein the desired openings comprise contact openings having a dimension on the order of less than 100 nm.

### Claim 18 (depends on 17)

The method of claim 17, further wherein the dimension of the desired openings comprises a diameter on the order of 45-50 nm.

### Claim 19

A method of forming openings in the fabrication of a device comprising:
forming an anti-reflective coating layer overlying a target layer in which desired openings are to be formed, wherein the target layer comprises an interlevel dielectric layer of a semiconductor substrate structure, wherein the semiconductor substrate structure comprises a semiconductor substrate including circuitry, an insulating layer overlying the semiconductor substrate, and at least one contact area within the insulating layer, wherein the interlevel dielectric having a thickness on the order of 150 nm, the anti-reflective coating having a thickness on the order of 35 nm, the negative photoresist layer having a thickness in a range on the order of 40-70 nm, and the spin-on developable hard mask layer having a thickness in the range on the order of 30-60 nm;
forming a negative photoresist layer overlying the anti-reflective coating layer;
exposing the negative photoresist layer with focused exposure energy according to a given positive pattern mask of the openings to be formed, wherein exposing according to the positive pattern mask creates exposed portions and unexposed portions of the negative photoresist layer;
developing the exposed negative photoresist layer, wherein developing removes unexposed portions of the negative photoresist layer to uncover corresponding portions of the anti-reflective coating layer, and wherein the exposed portions of the negative photoresist layer remain to create a negative pattern mask of the positive pattern mask;
forming a spin-on developable hard mask layer overlying the negative pattern mask and the uncovered portions of the anti-reflective coating layer;
removing the spin-on developable hard mask layer overlying the negative pattern mask by at least an amount sufficient to uncover the patterned negative photoresist layer;
removing the negative pattern mask, wherein removing the negative pattern mask forms a subsequent positive pattern mask out of a remainder portion of the spin-on developable hard mask layer; and
etching the anti-reflection coating layer and the target layer according to the subsequent positive pattern mask, wherein etching forms the desired openings within the target layer, wherein the steps of forming the anti-reflective coating layer, forming the negative photoresist layer, exposing the negative photoresist layer, developing the exposed negative photoresist layer, forming the spin-on developable hard mask layer, removing the spin-on developable hard mask layer overlying the negative patter mask are all performed within a same photo cluster.

### Claim 20

A method of forming openings in the fabrication of a device comprising:
forming an anti-reflective coating layer overlying a target layer in which desired openings are to be formed, wherein the target layer comprises an interlevel dielectric layer of a semiconductor substrate structure, wherein the semiconductor substrate structure comprises a semiconductor substrate including circuitry, an insulating layer overlying the semiconductor substrate, and at least one contact area within the insulating layer, and wherein the desired openings comprise contact openings having a dimension on the order of less than 100 nm;
forming a negative photoresist layer overlying the anti-reflective coating layer;
exposing the negative photoresist layer with focused exposure energy according to a given positive pattern mask of the openings to be formed, wherein exposing according to the positive pattern mask creates exposed portions and unexposed portions of the negative photoresist layer;
developing the exposed negative photoresist layer, wherein developing removes unexposed portions of the negative photoresist layer to uncover corresponding portions of the anti-reflective coating layer, and wherein the exposed portions of the negative photoresist layer remain to create a negative pattern mask of the positive pattern mask;
forming a spin-on developable hard mask layer overlying the negative pattern mask and the uncovered portions of the anti-reflective coating layer;
removing the spin-on developable hard mask layer overlying the negative pattern mask by at least an amount sufficient to uncover the patterned negative photoresist layer;
removing the negative pattern mask, wherein removing the negative pattern mask forms a subsequent positive pattern mask out of a remainder portion of the spin-on developable hard mask layer; and
etching the anti-reflection coating layer and the target layer according to the subsequent positive pattern mask, wherein etching forms the desired openings within the target layer, wherein the steps of forming the anti-reflective coating layer, forming the negative photoresist layer, exposing the negative photoresist layer, developing the exposed negative photoresist layer, forming the spin-on developable hard mask layer, removing the spin-on developable hard mask layer overlying the negative patter mask are all performed within a same photo cluster.