# US 2009/0270584 A1 · Heat-shrinkable polyester film and process for production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0270584 A1
- Document ID: US20090270584A1
- Status: Published application
- Kind: A1
- Application number: 12/304,531
- Filed: 2007-06-13
- Published: 2009-10-29
- Earliest claimed: 2006-06-14
- Assignees: Toyo Boseki Kabushiki Kaisha
- Inventors: Takurou Endo; Masayuki Haruta; Norimi Tabota; Katsuhiko Nose
- Web page: https://patentgrep.com/patent/US20090270584A1

## CPC

- B29C 55/146: {firstly transversely to the direction of feed and then parallel thereto}
- B29C 61/003: {characterised by the choice of material}
- B29C 61/06: Making preforms having internal stresses, e.g. plastic memory
- C08J 5/18: Manufacture of films or sheets
- B29K 2067/00: Use of polyesters {or derivatives thereof}, as moulding material
- B29K 2995/0049: Heat shrinkable
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- Y10T 428/1328: Shrinkable or shrunk [e.g., due to heat, solvent, volatile agent, restraint removal, etc.]
- Y10T 428/31786: Of polyester [e.g., alkyd, etc.]
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

In the heat-shrinkable polyester film of the present invention, the main shrinkage direction is the longitudinal direction. In addition, the hot-water heat shrinkage ratios in the longitudinal direction and the width direction when the film is treated in hot water at 90° C. for 10 seconds, the refractive indexes in the longitudinal direction and the width direction and the natural shrinkage ratio after aging at 40° C. and 65% RH for 700 hours or more are each controlled in predetermined ranges. The heat-shrinkable polyester film of the present invention is manufactured by stretching an unstretched film at a ratio of 2.5 times or more and 6.0 times or less in the width direction at a temperature of Tg+5° C. or more and Tg+40° C. or less, passing the film in an intermediate zone that does not execute an active heating operation, heat-treating the film at a temperature of 100° C. or more and 170° C. or less over a period of 1.0 second or more and 10.0 seconds or less, cooling the film to a surface temperature of 30° C. or more and 70° C. or less, stretching the film at a ratio of 2.0 times or more and 7 times or less in the longitudinal direction at a temperature of Tg+5° C. or more and Tg+80° C. or less, and subsequently cooling the film at a cooling rate of 30° C./second or more and 70° C./second or less to a surface temperature of the film of 45° C. or more and 75° C. or less.

## Claims

### Claim 1

A heat-shrinkable polyester film comprising ethylene terephthalate as a main constituent and containing 10% by mole or more of one or more kind(s) of monomer component(s) that become amorphous component(s) in all polyester resin components, being formed in a long shape with a constant width, and a main shrinkage direction thereof being a longitudinal direction, the heat-shrinkable film satisfying the following requirements (1) to (4):
(1) the hot-water heat shrinkage ratio in the longitudinal direction is 15% or more and 80% or less when the film is treated in hot water at 90° C. for 10 seconds;
(2) the hot-water heat shrinkage ratio in a width direction orthogonal to the longitudinal direction is 0% or more and 17% or less when the film is treated in hot water at 90° C. for 10 seconds;
(3) the refractive indexes in the longitudinal direction and the width direction are both 1.570 or more and 1.620 or less; and
(4) the natural shrinkage ratio after aging at 40° C. and 65% RH for 700 hours is 0.05% or more and 1.5% or less.

### Claim 2 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein the hot-water heat shrinkage ratio in the longitudinal direction is 15% or more and less than 40% when the film is treated in hot water at 90° C. for 10 seconds, the refractive index in the longitudinal direction is 1.570 or more and 1.590 or less, and the refractive index in the width direction is 1.570 or more and 1.620 or less.

### Claim 3 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein the main component of the monomer(s) that become amorphous component(s) in all the polyester resin components is any one of neopentyl glycol, 1,4-cyclohexane dimethanol and isophthalic acid.

### Claim 4 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein the Elmendorf ratio is 0.15 or more and 1.5 or less when the Elmendorf tear loads in the longitudinal direction and the width direction are measured after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C.

### Claim 5 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein the right angle tear strength in the width direction per unit thickness after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C. is 100 N/mm or more and 300 N/mm or less.

### Claim 6 (depends on 1)

A method for continuously manufacturing the heat-shrinkable polyester film according to claim 1, comprising stretching an unstretched film at a ratio of 2.5 times or more and 6.0 times or less to the width direction at a temperature of Tg+5° C. or more and Tg+40° C. or less while holding both ends in the width direction using a clip within a tenter, passing the film in an intermediate zone that does not execute an active heating operation, heat-treating the film at a temperature of 100° C. or more and 170° C. or less over a period of 1.0 second or more and 10.0 seconds or less, cooling the film to a surface temperature of 30° C. or more and 70° C. or less, stretching the film at a ratio of 2.0 times or more and 7 times or less in the longitudinal direction at a temperature of Tg+5° C. or more and Tg+80° C. or less, and subsequently cooling the film at a cooling rate of 30° C./second or more and 70° C./second or less to a surface temperature of the film of 45° C. or more and 75° C. or less.

### Claim 7 (depends on 2)

The heat-shrinkable polyester film according to claim 2 wherein the main component of the monomer(s) that become amorphous component(s) in all the polyester resin components is any one of neopentyl glycol, 1,4-cyclohexane dimethanol and isophthalic acid.

### Claim 8 (depends on 7)

The heat-shrinkable polyester film according to claim 7, wherein the right angle tear strength in the width direction per unit thickness after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C. is 100 N/mm or more and 300 N/mm or less.

### Claim 9 (depends on 7)

The heat-shrinkable polyester film according to claim 7, wherein the Elmendorf ratio is 0.15 or more and 1.5 or less when the Elmendorf tear loads in the longitudinal direction and the width direction are measured after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C.

### Claim 10 (depends on 9)

The heat-shrinkable polyester film according to claim 9, wherein the right angle tear strength in the width direction per unit thickness after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C. is 100 N/mm or more and 300 N/mm or less.

### Claim 11 (depends on 2)

The heat-shrinkable polyester film according to claim 2, wherein the Elmendorf ratio is 0.15 or more and 1.5 or less when the Elmendorf tear loads in the longitudinal direction and the width direction are measured after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C.

### Claim 12 (depends on 3)

The heat-shrinkable polyester film according to claim 3, wherein the Elmendorf ratio is 0.15 or more and 1.5 or less when the Elmendorf tear loads in the longitudinal direction and the width direction are measured after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C.

### Claim 13 (depends on 2)

The heat-shrinkable polyester film according to claim 2, wherein the right angle tear strength in the width direction per unit thickness after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C. is 100 N/mm or more and 300 N/mm or less.

### Claim 14 (depends on 3)

The heat-shrinkable polyester film according to claim 3, wherein the right angle tear strength in the width direction per unit thickness after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C. is 100 N/mm or more and 300 N/mm or less.

### Claim 15 (depends on 4)

The heat-shrinkable polyester film according to claim 4, wherein the right angle tear strength in the width direction per unit thickness after the film is shrunk by 10% in the longitudinal direction in hot water at 80° C. is 100 N/mm or more and 300 N/mm or less.

### Claim 16 (depends on 2)

A method for continuously manufacturing the heat-shrinkable polyester film according to claim 2, comprising stretching an unstretched film at a ratio of 2.5 times or more and 6.0 times or less to the width direction at a temperature of Tg+5° C. or more and Tg+40° C. or less while holding both ends in the width direction using a clip within a tenter, passing the film in an intermediate zone that does not execute an active heating operation, heat-treating the film at a temperature of 100° C. or more and 170° C. or less over a period of 1.0 second or more and 10.0 seconds or less, cooling the film to a surface temperature of 30° C. or more and 70° C. or less, stretching the film at a ratio of 2.0 times or more and 7 times or less in the longitudinal direction at a temperature of Tg+5° C. or more and Tg+80° C. or less, and subsequently cooling the film at a cooling rate of 30° C./second or more and 70° C./second or less to a surface temperature of the film of 45° C. or more and 75° C. or less.

### Claim 17 (depends on 3)

A method for continuously manufacturing the heat-shrinkable polyester film according to claim 3, comprising stretching an unstretched film at a ratio of 2.5 times or more and 6.0 times or less to the width direction at a temperature of Tg+5° C. or more and Tg+40° C. or less while holding both ends in the width direction using a clip within a tenter, passing the film in an intermediate zone that does not execute an active heating operation, heat-treating the film at a temperature of 100° C. or more and 170° C. or less over a period of 1.0 second or more and 10.0 seconds or less, cooling the film to a surface temperature of 30° C. or more and 70° C. or less, stretching the film at a ratio of 2.0 times or more and 7 times or less in the longitudinal direction at a temperature of Tg+5° C. or more and Tg+80° C. or less, and subsequently cooling the film at a cooling rate of 30° C./second or more and 70° C./second or less to a surface temperature of the film of 45° C. or more and 75° C. or less.

### Claim 18 (depends on 4)

A method for continuously manufacturing the heat-shrinkable polyester film according to claim 4, comprising stretching an unstretched film at a ratio of 2.5 times or more and 6.0 times or less to the width direction at a temperature of Tg+5° C. or more and Tg+40° C. or less while holding both ends in the width direction using a clip within a tenter, passing the film in an intermediate zone that does not execute an active heating operation, heat-treating the film at a temperature of 100° C. or more and 170° C. or less over a period of 1.0 second or more and 10.0 seconds or less, cooling the film to a surface temperature of 30° C. or more and 70° C. or less, stretching the film at a ratio of 2.0 times or more and 7 times or less in the longitudinal direction at a temperature of Tg+5° C. or more and Tg+80° C. or less, and subsequently cooling the film at a cooling rate of 30° C./second or more and 70° C./second or less to a surface temperature of the film of 45° C. or more and 75° C. or less.

### Claim 19 (depends on 5)

A method for continuously manufacturing the heat-shrinkable polyester film according to claim 5, comprising stretching an unstretched film at a ratio of 2.5 times or more and 6.0 times or less to the width direction at a temperature of Tg+5° C. or more and Tg+40° C. or less while holding both ends in the width direction using a clip within a tenter, passing the film in an intermediate zone that does not execute an active heating operation, heat-treating the film at a temperature of 100° C. or more and 170° C. or less over a period of 1.0 second or more and 10.0 seconds or less, cooling the film to a surface temperature of 30° C. or more and 70° C. or less, stretching the film at a ratio of 2.0 times or more and 7 times or less in the longitudinal direction at a temperature of Tg+5° C. or more and Tg+80° C. or less, and subsequently cooling the film at a cooling rate of 30° C./second or more and 70° C./second or less to a surface temperature of the film of 45° C. or more and 75° C. or less.