## CPC

- C08F 214/184: {with fluorinated vinyl ethers}
- C08F 214/26: Tetrafluoroethene
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

In a process for the manufacture of perfluoroelastomers, a weak organic acid, e.g. glacial acetic acid, is employed to coagulate an acidic perfluoroelastomer dispersion.

## Claims

### Claim 1

A coagulation process for the production of perfluoroelastomers, said process comprising:
(A) providing an aqueous dispersion comprising a perfluoroelastomer, said perfluoroelastomer comprising copolymerized units of tetrafluoroethylene, 15 to 65 mole percent of a perfluoro(alkyl vinyl ether) and 0.1 to 5 mole percent of a cure site monomer, said dispersion having a 1.5<pH<7; and
(B) adding to said aqueous dispersion an organic acid having a pKa between 3.5 and 5 thereby coagulating said perfluoroelastomer.

### Claim 2 (depends on 1)

A coagulation process of claim 1 wherein said perfluoro(alkyl vinyl ether) is perfluoro(methyl vinyl ether).

### Claim 3 (depends on 2)

A coagulation process of claim 2 wherein said cure site monomer is a nitrile-containing cure site monomer.

### Claim 4 (depends on 1)

A coagulation process of claim 1 wherein said perfluoroelastomer comprises copolymerized units of tetrafluoroethylene, 25 to 60 mole percent of a perfluoro(alkyl vinyl ether) and 0.3 to 1.5 mole percent of a cure site monomer.

### Claim 5 (depends on 1)

A coagulation process of claim 1 wherein said aqueous dispersion has a pH between 2 and 5.

### Claim 6 (depends on 1)

A coagulation process of claim 1 further comprising isolating said coagulated perfluoroelastomer from said dispersion and washing said coagulated perfluoroelastomer with deionized water until conductance measured on water passed through said coagulated perfluoroelastomer is less than 50 μS.

### Claim 7 (depends on 6)

A coagulation process of claim 6 further comprising heating said washed, coagulated perfluoroelastomer to a temperature between 70° and 300° C. in order to volatilize organic acid contained therein.