# US 2009/0270263 A1 · PROCESS FOR PRODUCING TAPE-SHAPED Re-TYPE (123) SUPERCONDUCTOR

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0270263 A1
- Document ID: US20090270263A1
- Status: Published application
- Kind: A1
- Application number: 12/376,099
- Filed: 2007-06-12
- Published: 2009-10-29
- Earliest claimed: 2006-08-23
- Assignees: International Superconductivity Technology Center, The Juridical Foundation; Swcc Showa Cable Systems Co., Ltd.
- Inventors: Yuji Aoki; Koichi Nakaoka; Junko Matsuda; Masateru Yoshizumi; Teruo Izumi; Yuh Shiohara
- Web page: https://patentgrep.com/patent/US20090270263A1

## CPC

- H10N 60/0324: {from a solution}
- C23C 18/1216: {Metal oxides (C23C18/1212 takes precedence)}
- C23C 18/1225: {Deposition of multilayers of inorganic material}
- C23C 18/1241: {Metallic substrates}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

This invention provides a production process of a tape-shaped superconductor which can realize high Jc and Ic values by virtue of the elimination of the cause of generation of cracks and deterioration of an electrical connectivity in crystal grain boundaries. In producing an Re-base (123) superconductor on a substrate by an MAD process, the use of a raw material solution having a Re:Ba:Cu molar ratio of 1:X:3, wherein X is a Ba molar ratio satisfying X<2 (preferably 1.0≦X≦1.8, especially 1.3≦x≦1.7), can realize the production of a thick-film tape-shaped superconductor having a superconductivity of Jc=3.20 MA/cm2 and Ic=525 A/cm (X=1.5).

## Claims

### Claim 1

A process for producing a tape-shaped Re-type (123) superconductor by giving a calcination heat-treatment after coating raw material solution including metal elements which compose the Re-type (123) superconductor (ReBa2Cu3OY, wherein, Re is at least more than one kind of element selected from Y, Nd, Sm, Gd, Eu, Yb, Pr or Ho) onto a substrate, and subsequently giving a heat treatment for producing the superconductor, comprising the step of:
using the raw material solution of the molar ratio of Ba of the range of X<2 when the molar ratio of Re, Ba and Cu in said raw material solution is Re:Ba:Cu=1:X:3.

### Claim 2 (depends on 1)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 1, wherein the molar ratio of Ba in the raw material solution is 1.0≦X≦1.8.

### Claim 3 (depends on 1)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 1, wherein the molar ratio of Ba in the raw material solution is 1.3≦X≦1.7.

### Claim 4 (depends on 3)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 3, wherein the raw material solution consists of the mixed solution of the organic solvent and any one or more kinds of trifluoroacetate, naphthenate, octylic acid salt, neodecanoic acid salt, isononanoic acid salt.

### Claim 5 (depends on 4)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 4, wherein the raw material solution consists of the mixed solution of the organic solvent and Y-TFA salt (trifluoroacetate), Ba-TFA salt including fluoride and naphthenate of Cu.

### Claim 6 (depends on 1)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 1, wherein the substrate is a biaxially-oriented substrate.

### Claim 7 (depends on 1)

The process for producing the tape-shaped Re-type (123) superconductor according to any one of claim 1, wherein the substrate is a composite substrate that a high oriented intermediate layer is formed onto the biaxially-oriented substrate.

### Claim 8 (depends on 1)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 1, wherein the raw material solution consists of the mixed solution of the organic solvent and any one or more kinds of trifluoroacetate, naphthenate, octylic acid salt, neodecanoic acid salt, isononanoic acid salt.

### Claim 9 (depends on 8)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 8, wherein the raw material solution consists of the mixed solution of the organic solvent and Y-TFA salt (trifluoroacetate), Ba-TFA salt including fluoride and naphthenate of Cu.

### Claim 10 (depends on 2)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 2, wherein the raw material solution consists of the mixed solution of the organic solvent and any one or more kinds of trifluoroacetate, naphthenate, octylic acid salt, neodecanoic acid salt, isononanoic acid salt.

### Claim 11 (depends on 10)

The process for producing the tape-shaped Re-type (123) superconductor according to claim 10, wherein the raw material solution consists of the mixed solution of the organic solvent and Y-TFA salt (trifluoroacetate), Ba-TFA salt including fluoride and naphthenate of Cu.