# US 2009/0270239 A1 · Black Complex Oxide Particles, Process for Producing the Same, Black Pastes, and Black Matrixes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0270239 A1
- Document ID: US20090270239A1
- Status: Published application
- Kind: A1
- Application number: 11/887,557
- Filed: 2006-03-27
- Published: 2009-10-29
- Earliest claimed: 2005-04-01
- Inventors: Koichi Katsuyama; Takashi Nakashima; Hiroyuki Shimamura
- Web page: https://patentgrep.com/patent/US20090270239A1

## CPC

- C09C 1/0009: {Pigments for ceramics (C09C1/0015, C09C1/0078 take precedence)}
- C09C 1/00: Treatment of specific inorganic materials other than fibrous fillers (tenebrescent materials C09K9/00; luminescent materials C09K11/00); Preparation of carbon black
- C09D 7/61: inorganic
- C09D 7/67: {Particle size smaller than 100 nm}
- C09D 7/68: {Particle size between 100-1000 nm}
- C09D 7/69: {Particle size larger than 1000 nm}
- C09D 11/037: characterised by the pigment
- C09D 17/007: {Metal oxide}
- C01P 2002/54: one element only
- C01P 2004/20: extending in two dimensions, e.g. plate-like
- C01P 2004/41: octahedron-like
- C01P 2004/45: Aggregated particles or particles with an intergrown morphology
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/12: Surface area
- C01P 2006/19: Oil-absorption capacity, e.g. DBP values
- C01P 2006/40: Electric properties
- C01P 2006/42: Magnetic properties
- C01P 2006/62: L* (lightness axis)
- C01P 2006/63: a* (red-green axis)
- C01P 2006/64: b* (yellow-blue axis)
- C08K 3/22: of metals
- C08K 7/00: Use of ingredients characterised by shape
- C09C: TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS, TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES (treatment of materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone C04B14/00, C04B18/00, C04B20/00); PREPARATION OF CARBON BLACK {; PREPARATION OF INORGANIC MATERIALS WHICH ARE NO SINGLE CHEMICAL COMPOUNDS AND WHICH ARE MAINLY USED AS PIGMENTS OR FILLERS}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The complex oxide particles of the present invention have a black hue, and contains 35 to 70% by weight of cobalt and 5 to 40% by weight of manganese. The molar ratio of cobalt to manganese Co/Mn is 0.5 to 14. The average particle diameter of primary particles is 0.05 to 0.3 μm. The particles have a shape of octahedral form. The particles are produced preferably through wet oxidation. No firing process is performed. The particles contain substantially no metal elements other than cobalt and manganese. The complex oxide particles of the present invention are suitably used as a black pigment for coating material, ink, toner, and rubbers or plastics.

## Claims

### Claim 1

Black complex oxide particles comprising 35 to 70% by weight of cobalt and 5 to 40% by weight of manganese, having a cobalt to manganese molar ratio Co/Mn of 0.5 to 14, a particle diameter of 0.05 to 0.3 μm averaged for the number of primary particles observed with a scanning electron microscope, and a shape of octahedral form.

### Claim 2 (depends on 1)

The black complex oxide particles according to claim 1, wherein the coefficient of variation of primary particle diameter in a particle size distribution on the basis of the number of primary particles observed with a scanning electron microscope is 40% or less.

### Claim 3 (depends on 1)

The black complex oxide particles according to claim 1, wherein the maximum particle diameter Dmax of aggregated particles in the particle size distribution on the basis of the number of particles, as measured by laser diffraction scattering method, is 4 μm or less.

### Claim 4 (depends on 1)

The black complex oxide particles according to claim 1, having a volumetric electrical resistance of 1×104Ω·cm or more.

### Claim 5 (depends on 1)

The black complex oxide particles according to claim 1, wherein the black complex oxide particles are produced without a firing process.

### Claim 6 (depends on 1)

The black complex oxide particles according to claim 1, comprising substantially no metal elements other than cobalt and manganese.

### Claim 7 (depends on 1)

The black complex oxide particles according to claim 1, having a saturation magnetization of 3 Am2/kg or less.

### Claim 8 (depends on 1)

The black complex oxide particles according to claim 1, having a BET specific surface area of 5 to 30 m2/g.

### Claim 9 (depends on 1)

Black slurry comprising the black complex oxide particles according to claim 1 and an organic solvent.

### Claim 10

A black paste comprising:
the black complex oxide particles according to clam 1;
a coating film-forming component including a resin; and
a glass frit.

### Claim 11 (depends on 10)

A black matrix formed from the black paste according to claim 10.

### Claim 12 (depends on 1)

A process for producing the black complex oxide particles according to claim 1, comprising:
mixing and neutralizing an aqueous solution of mixed metal salts dissolving water-soluble cobalt and manganese salts with alkali; and
oxidizing the resultant metal hydroxide slurry with an oxidative gas while the temperature is kept at 60 to 95° C. and the pH is kept at 10 to 13.