# US 2009/0269880 A1 · Method for manufacturing thin film transistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269880 A1
- Document ID: US20090269880A1
- Status: Published application
- Kind: A1
- Application number: 12/447,199
- Filed: 2007-11-09
- Published: 2009-10-29
- Earliest claimed: 2006-11-21
- Assignees: Canon Kabushiki Kaisha
- Inventors: Naho Itagaki; Tatsuya Iwasaki; Toru Den
- Web page: https://patentgrep.com/patent/US20090269880A1

## CPC

- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for manufacturing a thin film transistor containing an channel layer 11 having indium oxide, including forming an indium oxide film as an channel layer and subjecting the formed indium oxide film to an annealing in an oxidizing atmosphere.

## Claims

### Claim 1

A method for manufacturing a thin film transistor including a channel layer comprised of indium oxide, comprising forming an indium oxide film to provide said channel layer and subjecting the formed indium oxide film to an annealing step in an oxidizing atmosphere of 150° C. or more to 450° C. or less wherein the indium oxide film is amorphous prior to the annealing step and is crystalline after the annealing step.

### Claim at position 2

-3. (canceled)

### Claim 4 (depends on 1)

The method for manufacturing a thin film transistor according to claim 1, wherein the indium oxide film is formed by sputtering.

### Claim 5 (depends on 4)

The method for manufacturing a thin film transistor according to claim 4, wherein the step of forming the indium oxide film is carried out in an oxygen atmosphere having less oxygen concentration than the oxidizing atmosphere in the annealing step.

### Claim 6 (depends on 1)

The method for manufacturing a thin film transistor according to claim 1, wherein the indium oxide film prior to the annealing step in the oxidizing atmosphere has a resistivity of between 1 Ωcm and 500 Ωcm.

### Claim 7 (depends on 6)

The method for manufacturing a thin film transistor according to claim 6, wherein the indium oxide film after the annealing step in the oxidizing atmosphere has a resistivity of between more than 1 Ωcm and 500 Ω cm or less.