# US 2009/0269879 A1 · Metalorganic Chemical Vapor Deposition of Zinc Oxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269879 A1
- Document ID: US20090269879A1
- Status: Published application
- Kind: A1
- Application number: 12/421,133
- Filed: 2009-04-09
- Published: 2009-10-29
- Earliest claimed: 2008-04-25
- Assignees: Lumenz, Inc.
- Inventors: Bunmi T. Adekore; Jonathan Pierce
- Web page: https://patentgrep.com/patent/US20090269879A1

## CPC

- C23C 16/407: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 16/4481: {by evaporation using carrier gas in contact with the source material (C23C16/4486 takes precedence)}
- H10F 71/138: {Manufacture of transparent electrodes, e.g. transparent conductive oxides [TCO] or indium tin oxide [ITO] electrodes}
- H10F 77/244: {made of transparent conductive layers, e.g. transparent conductive oxide [TCO] layers}
- Y02E 10/50: Photovoltaic [PV] energy
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of metalorganic chemical vapor deposition includes converting a condensed matter source to provide a first gas, the source including at least one element selected from the group consisting of gold, silver and potassium. The method further includes providing a second gas comprising zinc and a third gas comprising oxygen, transporting the first gas, the second gas, and the third gas to a substrate, and forming a p-type zinc-oxide based semiconductor layer on the substrate.

## Claims

### Claim 1

A method of metalorganic chemical vapor deposition, the method comprising:
converting a condensed matter source to provide a first gas, the source including at least one element selected from the group consisting of gold, silver and potassium;
providing a second gas comprising zinc and a third gas comprising oxygen;
transporting the first gas, the second gas, and the third gas to a substrate; and
forming a p-type zinc-oxide based semiconductor layer on the substrate.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the condensed matter source is a non-halogenated and non-silylated source.

### Claim 3 (depends on 2)

A method according to claim 2, wherein the non-halogenated and non-silylated condensed matter source is in a solid phase, and converting includes subliming the source.

### Claim 4 (depends on 3)

A method according to claim 3, wherein the source has a vapor pressure ranging from about 10−5 to about 103 torr between about 30° C. to about 300° C.

### Claim 5 (depends on 3)

A method according to claim 3, wherein transporting the first gas includes heating transport lines of the first gas to a temperature of about the source's sublimation temperature or greater.

### Claim 6 (depends on 1)

A method according to claim 1, wherein the source includes a polymerization inhibitor.

### Claim 7 (depends on 6)

A method according to claim 6, wherein the polymerization inhibitor includes inert particles.

### Claim 8 (depends on 7)

A method according to claim 7, wherein the source is a powder interspersed with the inert particles, the inert particles having a size distribution that is of the same order of magnitude as that of the powder.

### Claim 9 (depends on 7)

A method according to claim 7, wherein the source is a liquid or a gel and the inert particles are suspended in the liquid or the gel.

### Claim 10 (depends on 6)

A method according to claim 6, wherein the polymerization inhibitor is selected from the group consisting of quinones and oxygen.

### Claim 11 (depends on 1)

A method according to claim 1, further comprising providing a fourth gas including a surfactant that reacts with the first gas, wherein transporting includes transporting the first gas, the second gas, the third gas, and the fourth gas to the substrate.

### Claim 12 (depends on 11)

A method according to claim 11, wherein the surfactant includes boron.

### Claim 13 (depends on 1)

A method according to claim 1, wherein the condensed matter source includes a halogen or silicon.

### Claim 14 (depends on 13)

A method according to claim 13, wherein the condensed matter source is in a solid phase, and converting includes subliming the source.

### Claim 15 (depends on 14)

A method according to claim 14, wherein the source has a vapor pressure ranging from about 10−5 to about 103 torr between about 30° C. and about 300° C.

### Claim 16 (depends on 13)

A method according to claim 13, wherein the substrate is heated in an elevated temperature environment between about 700° C. to about 850° C.

### Claim 17 (depends on 13)

A method according to claim 13, further comprising annealing the p-type zinc-oxide based semiconductor layer in an elevated temperature environment for a period of time so that at least a portion of the halogen or silicon diffuses out of the layer.

### Claim 18 (depends on 17)

A method according to claim 17, wherein the elevated temperature environment is between about 500° C. to about 1400° C.

### Claim 19 (depends on 17)

A method according to claim 17, wherein the elevated temperature environment is between about 900° C. to about 1100° C. and the period of time is greater than about 1 hour.

### Claim 20 (depends on 17)

A method according to claim 17, wherein annealing is performed at a pressure ranging from about 0.1 mbar to about 2.4 kbar.

### Claim 21 (depends on 17)

A method according to claim 17, wherein annealing is performed in an ambient that includes at least one selected from the group consisting of an inert gas, air, nitrogen, and oxygen.

### Claim 22 (depends on 13)

A method according to claim 13, wherein the substrate includes a first surface and a second surface, and forming a p-type zinc-oxide based semiconductor layer occurs on the first surface, the method further comprising:
abrading the second surface of the substrate; and
annealing the substrate in an elevated temperature environment for a period of time so that at least a portion of the halogen or silicon diffuses away from the first surface towards the second surface.

### Claim 23

A method of depositing a p-type zinc-oxide based semiconductor layer onto a substrate by a metalorganic chemical vapor deposition technique, the method comprising:
converting a non-halogenated and non-silylated condensed matter source to a first gas that provides a p-type dopant, wherein the condensed matter source includes at least one element selected from the group consisting of gold, silver, and potassium and has a vapor pressure ranging from about 10−5 to about 103 torr between about 30° C. to about 300° C.;
supplying reaction gases including the first gas, a second gas comprising zinc, and a third gas comprising oxygen; and
transporting the reaction gases to a surface of a substrate to grow the p-type zinc-oxide based semiconductor layer.

### Claim 24 (depends on 23)

A method according to claim 23, wherein the non-halogenated and non-silylated condensed matter source is in a solid phase, and converting includes subliming the source.

### Claim 25 (depends on 24)

A method according to claim 24, wherein supplying the first gas includes heating transport lines of the first gas to a temperature of about the source's sublimation temperature or greater.

### Claim 26 (depends on 23)

A method according to claim 23, wherein the source includes a polymerization inhibitor.

### Claim 27 (depends on 26)

A method according to claim 26, wherein the polymerization inhibitor includes inert particles.

### Claim 28 (depends on 27)

A method according to claim 27, wherein the source is a powder interspersed with the inert particles, the inert particles having a size distribution that is of the same order of magnitude as that of the powder.

### Claim 29 (depends on 27)

A method according to claim 27, wherein the source is a liquid or a gel and the inert particles are suspended in the liquid or the gel.

### Claim 30 (depends on 26)

A method according to claim 26, wherein the polymerization inhibitor is selected from the group consisting of quinones and oxygen.

### Claim 31

A method of forming a p-type zinc-oxide based semiconductor layer by metalorganic chemical vapor deposition, the method comprising:
converting a condensed matter source to provide a first gas comprising a halogen or silicon, the source including at least one element selected from the group consisting of gold, silver, and potassium;
providing a second gas comprising zinc and a third gas comprising oxygen;
transporting the first gas, the second gas, and the third gas to the substrate to form a zinc-oxide based film; and
annealing the zinc-oxide based film in an elevated temperature environment for a period of time so that at least a portion of the halogen or silicon diffuses out of the film to produce the p-type zinc-oxide based semiconductor layer.

### Claim 32 (depends on 31)

A method according to claim 31, wherein the condensed matter source is in a solid phase, and converting includes subliming the source.

### Claim 33 (depends on 32)

A method according to claim 32, wherein transporting the first gas includes heating transport lines of the first gas to a temperature of about the source's sublimation temperature or greater.

### Claim 34 (depends on 31)

A method according to claim 31, wherein the source includes a polymerization inhibitor.

### Claim 35 (depends on 34)

A method according to claim 34, wherein the polymerization inhibitor includes inert particles.

### Claim 36 (depends on 35)

A method according to claim 35, wherein the source is a powder interspersed with the inert particles, the inert particles having a size distribution that is of the same order of magnitude as that of the powder.

### Claim 37 (depends on 35)

A method according to claim 35, wherein the source is a liquid or a gel and the inert particles are suspended in the liquid or the gel.

### Claim 38 (depends on 34)

A method according to claim 34, wherein the polymerization inhibitor is selected from the group consisting of quinones and oxygen.

### Claim 39 (depends on 31)

A method according to claim 31, further comprising providing a fourth gas including a surfactant that reacts with the first gas, wherein transporting includes transporting the first gas, the second gas, the third gas, and the fourth gas to the substrate to form a zinc-oxide based film.

### Claim 40 (depends on 39)

A method according to claim 39, wherein the surfactant includes boron.

### Claim 41 (depends on 31)

A method according to claim 31, wherein the elevated temperature environment is between about 500° C. to about 1400° C.

### Claim 42 (depends on 31)

A method according to claim 31, wherein the elevated temperature environment is between about 900° C. to about 1100° C. and the period of time is greater than about 1 hour.

### Claim 43 (depends on 31)

A method according to claim 31, wherein annealing is performed at a pressure ranging from about 0.1 mbar to about 2.4 kbar.

### Claim 44 (depends on 31)

A method according to claim 31, wherein annealing is performed in an ambient that includes at least one selected from the group consisting of an inert gas, air, and oxygen.

### Claim 45

A method of forming a p-type zinc-oxide based semiconductor layer on a substrate by metalorganic chemical vapor deposition, the method comprising:
heating the substrate in an elevated temperature environment between about 700° C. to about 850° C.;
converting a condensed matter source to provide a first gas comprising a halogen or silicon, the source including at least one element selected from the group consisting of gold, silver, and potassium;
providing a second gas comprising zinc and a third gas comprising oxygen; and
transporting the first gas, the second gas, and the third gas to a surface of the substrate to grow the p-type zinc-oxide based semiconductor layer.

### Claim 46 (depends on 45)

A method according to claim 45, wherein the condensed matter source is in a solid phase, and converting includes subliming the source.

### Claim 47 (depends on 45)

A method according to claim 45, further comprising providing a fourth gas including a surfactant that reacts with the first gas, transporting includes transporting the first gas, the second gas, the third gas, and the fourth gas to the substrate to grow the p-type zinc-oxide based semiconductor layer.

### Claim 48 (depends on 47)

A method according to claim 47, wherein the surfactant includes boron.

### Claim 49 (depends on 45)

A method according to claim 45, further comprising annealing the p-type zinc-oxide based semiconductor layer in an elevated temperature environment for a period of time so that at least a portion of the halogen or silicon diffuses out of the layer.

### Claim 50

A method of metalorganic chemical vapor deposition, the method comprising:
converting a condensed matter source to provide a first gas, the source including at least one p-type dopant element;
providing a second gas comprising zinc and a third gas comprising oxygen;
transporting the first gas, the second gas, and the third gas to a substrate; and
forming a p-type zinc-oxide based semiconductor layer on the substrate.

### Claim 51 (depends on 50)

A method according to claim 50, wherein the p-type dopant element includes at least one element selected from the group consisting of gold, silver, and potassium.

### Claim 52

A metalorganic chemical vapor deposition system for p-type zinc oxide comprising:
a condensed matter source including at least one p-type dopant element;
a first source comprising zinc;
a second source comprising oxygen;
a chemical vapor deposition reactor chamber connected to the condensed matter source, the first source, and the second source; and
a heated transport line connecting the condensed matter source to the chemical vapor deposition reactor chamber.

### Claim 53 (depends on 52)

The system of claim 52, further comprising:
a heater containing the condensed matter source.

### Claim 54 (depends on 52)

The system of claim 52, wherein the at least one p-type dopant element is selected from the group consisting of gold, silver, and potassium.