# US 2009/0269875 A1 · Method for manufacturing photoelectric conversion device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269875 A1
- Document ID: US20090269875A1
- Status: Published application
- Kind: A1
- Application number: 12/424,827
- Filed: 2009-04-16
- Published: 2009-10-29
- Earliest claimed: 2008-04-25
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Sho KATO; Satoshi TORIUMI; Fumito ISAKA
- Web page: https://patentgrep.com/patent/US20090269875A1

## CPC

- H10F 71/1395: {for thin-film devices}
- H02S 40/34: comprising specially adapted electrical connection means to be structurally associated with the PV module, e.g. junction boxes
- H10F 10/16: Photovoltaic cells having only PN heterojunction potential barriers
- H10F 10/17: Photovoltaic cells having only PIN junction potential barriers
- H10F 10/172: comprising multiple PIN junctions, e.g. tandem cells
- H10F 19/00: Integrated devices, or assemblies of multiple devices, comprising at least one photovoltaic cell covered by group H10F10/00, e.g. photovoltaic modules
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/1224: {comprising microcrystalline silicon}
- H10F 71/131: {Recrystallisation; Crystallization of amorphous or microcrystalline semiconductors}
- H10F 77/937: {Busbar structures for modules}
- Y02E 10/545: Microcrystalline silicon PV cells
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02E 10/548: Amorphous silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H02S: GENERATION OF ELECTRIC POWER BY CONVERSION OF INFRARED RADIATION, VISIBLE LIGHT OR ULTRAVIOLET LIGHT, e.g. USING PHOTOVOLTAIC [PV] MODULES (obtaining electrical energy from radioactive sources G21H1/12; light sensitive inorganic semiconductor devices H10F; light sensitive organic semiconductor devices H10K30/00; thermoelectric devices H10N10/00; pyroelectric devices H10N15/00)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An embrittlement layer is formed in the single crystal semiconductor substrate and a first impurity semiconductor layer, a first electrode, and an insulating layer are formed on one surface of the single crystal semiconductor substrate. After attaching the insulating layer and a supporting substrate to each other to bond the single crystal semiconductor substrate and the supporting substrate, the single crystal semiconductor substrate is separated along the embrittlement layer to form a stack including a first single crystal semiconductor layer. A first semiconductor layer and a second semiconductor layer are formed over the first single crystal semiconductor layer. A second single crystal semiconductor layer is formed by solid phase growth. A second impurity semiconductor layer having a conductivity type opposite to that of the first impurity semiconductor layer is formed on the second single crystal semiconductor layer. A second electrode is formed on the second impurity semiconductor layer.

## Claims

### Claim 1

A method for manufacturing a photoelectric conversion device, comprising:
forming a first impurity semiconductor layer over a single crystal semicondcutor substrate;
irradiating the single crystal semiconductor substrate with ions to form an embrittlement layer in the single crystal semiconductor substrate;
forming a first electrode over the first impurity semiconductor layer;
forming an insulating layer over the first electrode;
attaching the insulating layer and a supporting substrate to each other to bond the single crystal semiconductor substrate and the supporting substrate and then separating the single crystal semiconductor substrate along the embrittlement layer, whereby a stack including the insulating layer, the first electrode, the first impurity semiconductor layer, and a first single crystal semiconductor layer is provided on the supporting substrate;
forming a first semiconductor layer over the first single crystal semiconductor layer;
forming a second semiconductor layer over the first semiconductor layer under a condition different from that of the first semiconductor layer;
forming a second single crystal semiconductor layer by improving crystallinity of the first semiconductor layer and the second semiconductor layer by solid phase growth;
forming a second impurity semiconductor layer having a conductivity type opposite to that of the first impurity semiconductor layer over the second single crystal semiconductor layer; and
forming a second electrode over the second impurity semiconductor layer.

### Claim 2 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first semiconductor layer and the second semiconductor layer are formed such that crystallinity of the first semiconductor layer is higher than that of the second semiconductor layer.

### Claim 3 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first semiconductor layer and the second semiconductor layer are formed such that hydrogen concentration of the first semiconductor layer is lower than that of the second semiconductor layer.

### Claim 4 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first semiconductor layer is formed to a thickness of from 10 nm to 50 nm.

### Claim 5 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein ions generated with a source gas containing hydrogen are used as the ions.

### Claim 6 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first single crystal semiconductor layer and the second single crystal semiconductor layer are formed such that the total thickness of the first single crystal semiconductor layer and the second single crystal semiconductor layer is 800 nm or more.

### Claim 7 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first impurity semiconductor layer is a p-type impurity semiconductor layer, and
wherein the second impurity semiconductor layer is an n-type impurity semiconductor layer.

### Claim 8 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first semiconductor layer is formed by a plasma chemical vapor deposition method in which a flow ratio of a hydrogen gas to a silane based gas is 50:1 or more.

### Claim 9 (depends on 8)

The method for manufacturing a photoelectric conversion device, according to claim 8,
wherein the silane based gas is silane or disilane.

### Claim 10 (depends on 8, 9)

The method for manufacturing a photoelectric conversion device, according to claim 8 or 9,
wherein the plasma chemical vapor deposition method is performed under a pressure of from 1 Pa to 103 Pa.

### Claim 11 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first impurity semicondcutor layer and the second impurity semiconductor layer are formed by an ion implantation method or an ion doping method.

### Claim 12 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1,
wherein the first single crystal semiconductor layer is irradiated with a laser beam to repair or remove a crystal defect included in the first single crystal semicondcutor layer.

### Claim 13 (depends on 1)

The method for manufacturing a photoelectric conversion device, according to claim 1, wherein the second single crystal semicondcutor layer is formed by heating the first semiconductor layer and the second semiconductor layer by rapid thermal annealing.

### Claim 14

A method for manufacturing a photoelectric conversion device, comprising:
irradiating a single crystal semiconductor substrate with ions to form an embrittlement layer in the single crystal semiconductor substrate;
forming a first impurity semiconductor layer over the single crystal semicondcutor substrate;
forming a first electrode over the first impurity semiconductor layer;
forming an insulating layer over the first electrode;
attaching the insulating layer and a supporting substrate to each other to bond the single crystal semiconductor substrate and the supporting substrate and then separating the single crystal semiconductor substrate along the embrittlement layer, whereby a stack including the insulating layer, the first electrode, the first impurity semiconductor layer, and a first single crystal semiconductor layer is provided on the supporting substrate;
forming a first semiconductor layer over the first single crystal semiconductor layer;
forming a second semiconductor layer over the first semiconductor layer under a condition different from that of the first semiconductor layer;
forming a second single crystal semiconductor layer by improving crystallinity of the first semiconductor layer and the second semiconductor layer by solid phase growth;
forming a second impurity semiconductor layer having a conductivity type opposite to that of the first impurity semiconductor layer over the second single crystal semiconductor layer; and
forming a second electrode over the second impurity semiconductor layer.

### Claim 15 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first semiconductor layer and the second semiconductor layer are formed such that crystallinity of the first semiconductor layer is higher than that of the second semiconductor layer.

### Claim 16 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first semiconductor layer and the second semiconductor layer are formed such that hydrogen concentration of the first semiconductor layer is lower than that of the second semiconductor layer.

### Claim 17 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first semiconductor layer is formed to a thickness of from 10 nm to 50 nm.

### Claim 18 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein ions generated with a source gas containing hydrogen are used as the ions.

### Claim 19 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first single crystal semiconductor layer and the second single crystal semiconductor layer are formed such that the total thickness of the first single crystal semiconductor layer and the second single crystal semiconductor layer is 800 nm or more.

### Claim 20 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first impurity semiconductor layer is a p-type impurity semiconductor layer, and
wherein the second impurity semiconductor layer is an n-type impurity semiconductor layer.

### Claim 21 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first semiconductor layer is formed by a plasma chemical vapor deposition method in which a flow ratio of a hydrogen gas to a silane based gas is 50:1 or more.

### Claim 22 (depends on 21)

The method for manufacturing a photoelectric conversion device, according to claim 21,
wherein the silane based gas is silane or disilane.

### Claim 23 (depends on 21)

The method for manufacturing a photoelectric conversion device, according to claim 21,
wherein the plasma chemical vapor deposition method is performed under a pressure of from 1 Pa to 103 Pa.

### Claim 24 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first impurity semicondcutor layer and the second impurity semiconductor layer are formed by an ion implantation method or an ion doping method.

### Claim 25 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14,
wherein the first single crystal semiconductor layer is irradiated with a laser beam to repair or remove a crystal defect included in the first single crystal semicondcutor layer.

### Claim 26 (depends on 14)

The method for manufacturing a photoelectric conversion device, according to claim 14, wherein the second single crystal semicondcutor layer is formed by heating the first semiconductor layer and the second semiconductor layer by rapid thermal annealing.

### Claim 27

A method for manufacturing a photoelectric conversion device, comprising:
forming a first electrode over a single crystal semicondcutor substrate;
irradiating the single crystal semiconductor substrate with ions to form an embrittlement layer in the single crystal semiconductor substrate;
forming a first impurity semiconductor layer over the single crystal semicondcutor substrate;
forming an insulating layer over the first electrode;
attaching the insulating layer and a supporting substrate to each other to bond the single crystal semiconductor substrate and the supporting substrate and then separating the single crystal semiconductor substrate along the embrittlement layer, whereby a stack including the insulating layer, the first electrode, the first impurity semiconductor layer, and a first single crystal semiconductor layer is provided on the supporting substrate;
forming a first semiconductor layer over the first single crystal semiconductor layer;
forming a second semiconductor layer over the first semiconductor layer under a condition different from those of the first semiconductor layer;
forming a second single crystal semiconductor layer by improving crystallinity of the first semiconductor layer and the second semiconductor layer by solid phase growth;
forming a second impurity semiconductor layer having a conductivity type opposite to that of the first impurity semiconductor layer over the second single crystal semiconductor layer; and
forming a second electrode over the second impurity semiconductor layer.

### Claim 28 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first semiconductor layer and the second semiconductor layer are formed such that crystallinity of the first semiconductor layer is higher than that of the second semiconductor layer.

### Claim 29 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first semiconductor layer and the second semiconductor layer are formed such that hydrogen concentration of the first semiconductor layer is lower than that of the second semiconductor layer.

### Claim 30 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first semiconductor layer is formed to a thickness of from 10 nm to 50 nm.

### Claim 31 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein ions generated with a source gas containing hydrogen are used as the ions.

### Claim 32 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first single crystal semiconductor layer and the second single crystal semiconductor layer are formed such that the total thickness of the first single crystal semiconductor layer and the second single crystal semiconductor layer is 800 nm or more.

### Claim 33 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first impurity semiconductor layer is a p-type impurity semiconductor layer, and
wherein the second impurity semiconductor layer is an n-type impurity semiconductor layer.

### Claim 34 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first semiconductor layer is formed by a plasma chemical vapor deposition method in which a flow ratio of a hydrogen gas to a silane based gas is 50:1 or more.

### Claim 35 (depends on 34)

The method for manufacturing a photoelectric conversion device, according to claim 34,
wherein the silane based gas is silane or disilane.

### Claim 36 (depends on 34)

The method for manufacturing a photoelectric conversion device, according to claim 34,
wherein the plasma chemical vapor deposition method is performed under a pressure of from 1 Pa to 103 Pa.

### Claim 37 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first impurity semicondcutor layer and the second impurity semiconductor layer are formed by an ion implantation method or an ion doping method.

### Claim 38 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27,
wherein the first single crystal semiconductor layer is irradiated with a laser beam to repair or remove a crystal defect included in the first single crystal semicondcutor layer.

### Claim 39 (depends on 27)

The method for manufacturing a photoelectric conversion device, according to claim 27, wherein the second single crystal semicondcutor layer is formed by heating the first semiconductor layer and the second semiconductor layer by rapid thermal annealing.

### Claim 40

A method for manufacturing a photoelectric conversion device, comprising:
forming a first electrode and a first impurity semiconductor layer over a single crystal semicondcutor substrate;
irradiating the single crystal semiconductor substrate with ions to form an embrittlement layer in the single crystal semiconductor substrate;
forming an insulating layer over the first electrode;
attaching the insulating layer and a supporting substrate to each other to bond the single crystal semiconductor substrate and the supporting substrate and then separating the single crystal semiconductor substrate along the embrittlement layer, whereby a stack including the insulating layer, the first electrode, the first impurity semiconductor layer, and a first single crystal semiconductor layer is provided on the supporting substrate;
forming a first semiconductor layer over the first single crystal semiconductor layer;
forming a second semiconductor layer over the first semiconductor layer under a condition different from that of the first semiconductor layer;
improving crystallinity of the first semiconductor layer and the second semiconductor layer by solid phase growth;
forming a second impurity semiconductor layer having a conductivity type opposite to that of the first impurity semiconductor layer over the second semiconductor layer; and
forming a second electrode over the second impurity semiconductor layer.

### Claim 41 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first semiconductor layer and the second semiconductor layer are formed such that crystallinity of the first semiconductor layer is higher than that of the second semiconductor layer.

### Claim 42 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first semiconductor layer and the second semiconductor layer are formed such that hydrogen concentration of the first semiconductor layer is lower than that of the second semiconductor layer.

### Claim 43 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first semiconductor layer is formed to a thickness of from 10 nm to 50 nm.

### Claim 44 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein ions generated with a source gas containing hydrogen are used as the ions.

### Claim 45 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first single crystal semiconductor layer, the first semiconductor layer, and the second semiconductor layer are formed such that the total thickness thereof is 800 nm or more.

### Claim 46 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first impurity semiconductor layer is a p-type impurity semiconductor layer, and
wherein the second impurity semiconductor layer is an n-type impurity semiconductor layer.

### Claim 47 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first semiconductor layer is formed by a plasma chemical vapor deposition method in which a flow ratio of a hydrogen gas to a silane based gas is 50:1 or more.

### Claim 48 (depends on 47)

The method for manufacturing a photoelectric conversion device, according to claim 47,
wherein the silane based gas is silane or disilane.

### Claim 49 (depends on 47)

The method for manufacturing a photoelectric conversion device, according to claim 47,
wherein the plasma chemical vapor deposition method is performed under a pressure of from 1 Pa to 103 Pa.

### Claim 50 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first impurity semicondcutor layer and the second impurity semiconductor layer are formed by an ion implantation method or an ion doping method.

### Claim 51 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the first single crystal semiconductor layer is irradiated with a laser beam to repair or remove a crystal defect included in the first single crystal semicondcutor layer.

### Claim 52 (depends on 40)

The method for manufacturing a photoelectric conversion device, according to claim 40,
wherein the improving of crystallinity is performed by heating the first semiconductor layer and the second semiconductor layer by rapid thermal annealing.