# US 2009/0269873 A1 · Liquid-crystal electro-optical apparatus and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269873 A1
- Document ID: US20090269873A1
- Status: Published application
- Kind: A1
- Application number: 12/500,026
- Filed: 2009-07-09
- Published: 2009-10-29
- Earliest claimed: 1993-07-22
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Toshimitsu KONUMA; Takeshi NISHI; Michio SHIMIZU; Harumi MORI; Kouji MORIYA; Satoshi MURAKAMI
- Web page: https://patentgrep.com/patent/US20090269873A1

## CPC

- G02F 1/141: using ferroelectric liquid crystals
- G02F 1/133711: {by organic films, e.g. polymeric films}
- G02F 1/133788: {by light irradiation, e.g. linearly polarised light photo-polymerisation}
- G02F 1/1416: {Details of the smectic layer structure, e.g. bookshelf, chevron, C1 and C2}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A liquid crystal device comprising: a pair of substrates having an electrode arrangement thereon; an orientation control means provided on at least one of said substrates; and a ferroelectric or antiferroelectric liquid crystal layer interposed between said substrates, said liquid crystal layer being uniaxially oriented by virtue of said orientation control means, wherein means for suppressing an orientation control effect of said orientation control means with respect to said liquid crystal layer is provided between said liquid crystal layer and said orientation control means.

## Claims

### Claim 1

A method for manufacturing a liquid crystal device comprising the steps of:
disposing a mixture comprising a liquid crystal material and a curable resin containing a reaction initiating agent between a pair of substrates wherein at least one of the pair of substrates has an orientation film in contact with the mixture;
orienting the liquid crystal material; and
curing the resin in the mixture so that the resin is formed on a surface of the orientation film.

### Claim 2 (depends on 1)

The method of claim 1 wherein the curable resin includes a monomer at 40% weight or more.

### Claim 3 (depends on 1)

The method of claim 1, wherein the curable resin includes a monomer at 60-90% weight.

### Claim 4 (depends on 1)

The method of claim 1 wherein the curable resin includes a monomer and a concentration of the monomer with respect to the mixture is 2.0% weight or more.

### Claim 5 (depends on 1)

The method of claim 1 wherein the liquid crystal material is a ferroelectric liquid crystal or an antiferroelectric liquid crystal.

### Claim 6 (depends on 1)

The method of claim 1 wherein the resin formed on the surface of the orientation film restrains an orientation control force of the orientation film with respect to the liquid crystal material.

### Claim 7 (depends on 1)

The method of claim 1 wherein the mixture is disposed between the pair of substrates after the pair of substrates are arranged so as to be opposed to each other.

### Claim 8 (depends on 1)

The method of claim 1 wherein further comprising a step of forming a plurality of thin film transistors on one of the pair of substrates.

### Claim 9

A method for manufacturing a liquid crystal device comprising the steps of:
disposing a mixture comprising a liquid crystal material and a curable resin containing a reaction initiating agent between a pair of substrates wherein at least one of the pair of substrates has an orientation film in contact with the mixture;
orienting the liquid crystal material; and
curing the resin in the mixture so that the resin in a form of grains is formed on a surface of the orientation film.

### Claim 10 (depends on 9)

The method of claim 9, wherein the curable resin includes a monomer at 40% weight or more.

### Claim 11 (depends on 9)

The method of claim 9, wherein the curable resin includes a monomer at 60-90% weight.

### Claim 12 (depends on 9)

The method of claim 9, wherein the curable resin includes a monomer and a concentration of the monomer with respect to the mixture is 2.0% weight or more.

### Claim 13 (depends on 9)

The method of claim 9, wherein the liquid crystal material is a ferroelectric liquid crystal or an antiferroelectric liquid crystal.

### Claim 14 (depends on 9)

The method of claim 9, wherein the resin formed on the surface of the orientation film restrains an orientation control force of the orientation film with respect to the liquid crystal material.

### Claim 15 (depends on 9)

The method of claim 9, wherein the mixture is disposed between the pair of substrates after the pair of substrates are arranged so as to be opposed to each other.

### Claim 16 (depends on 9)

The method of claim 9, wherein further comprising a step of forming a plurality of thin film transistors on one of the pair of substrates.

### Claim 17

A method for manufacturing a liquid crystal device comprising the steps of:
disposing a mixture comprising a liquid crystal material and a curable resin containing a reaction initiating agent between a pair of substrates wherein at least one of the pair of substrates has an orientation film in contact with the mixture;
orienting the liquid crystal material; and
curing the resin in the mixture so that the resin in a form of a film is formed on a surface of the orientation film.

### Claim 18 (depends on 17)

The method of claim 17, wherein the curable resin includes a monomer at 40% weight or more.

### Claim 19 (depends on 17)

The method of claim 17, wherein the curable resin includes a monomer at 60-90% weight.

### Claim 20 (depends on 17)

The method of claim 17, wherein the curable resin includes a monomer and a concentration of the monomer with respect to the mixture is 2.0% weight or more.

### Claim 21 (depends on 17)

The method of claim 17, wherein the liquid crystal material is a ferroelectric liquid crystal or an antiferroelectric liquid crystal.

### Claim 22 (depends on 17)

The method of claim 17, wherein the resin formed on the surface of the orientation film restrains an orientation control force of the orientation film with respect to the liquid crystal material.

### Claim 23 (depends on 17)

The method of claim 17 wherein the mixture is disposed between the pair of substrates after the pair of substrates are arranged so as to be opposed to each other.

### Claim 24 (depends on 17)

The method of claim 17 wherein further comprising a step of forming a plurality of thin film transistors on one of the pair of substrates.

### Claim 25

A method for manufacturing a liquid crystal device comprising the steps of:
disposing a mixture comprising a liquid crystal material and a curable resin containing a reaction initiating agent between a pair of substrates wherein at least one of the pair of substrates has an orientation film in contact with the mixture;
orienting the liquid crystal material; and
curing the resin in the mixture by ultraviolet irradiation so that the resin is formed on a surface of the orientation film.

### Claim 26 (depends on 25)

The method of claim 25 wherein the liquid crystal material is a ferroelectric liquid crystal or an antiferroelectric liquid crystal.

### Claim 27 (depends on 25)

The method of claim 25 wherein the resin formed on the surface of the orientation film restrains an orientation control force of the orientation film with respect to the liquid crystal material.

### Claim 28 (depends on 25)

The method of claim 25 wherein the mixture is disposed between the pair of substrates after the pair of substrates are arranged so as to be opposed to each other.

### Claim 29 (depends on 25)

The method of claim 25 wherein further comprising a step of forming a plurality of thin film transistors on one of the pair of substrates.

### Claim 30

A method for manufacturing a liquid crystal device comprising the steps of:
disposing a mixture comprising a liquid crystal material and a curable resin containing a reaction initiating agent between a pair of substrates wherein at least one of the pair of substrates has an orientation film in contact with the mixture;
orienting the liquid crystal material; and
curing the resin in the mixture by ultraviolet irradiation so that the resin in a form of grains is formed on a surface of the orientation film.

### Claim 31 (depends on 30)

The method of claim 30, wherein the liquid crystal material is a ferroelectric liquid crystal or an antiferroelectric liquid crystal.

### Claim 32 (depends on 30)

The method of claim 30, wherein the resin formed on the surface of the orientation film restrains an orientation control force of the orientation film with respect to the liquid crystal material.

### Claim 33 (depends on 30)

The method of claim 30, wherein the mixture is disposed between the pair of substrates after the pair of substrates are arranged so as to be opposed to each other.

### Claim 34 (depends on 30)

The method of claim 30, wherein further comprising a step of forming a plurality of thin film transistors on one of the pair of substrates.

### Claim 35

A method for manufacturing a liquid crystal device comprising the steps of:
disposing a mixture comprising a liquid crystal material and a curable resin containing a reaction initiating agent between a pair of substrates wherein at least one of the pair of substrates has an orientation film in contact with the mixture;
orienting the liquid crystal material; and
curing the resin in the mixture by ultraviolet irradiation so that the resin in a form of a film is formed on a surface of the orientation film.

### Claim 36 (depends on 35)

The method of claim 35, wherein the liquid crystal material is a ferroelectric liquid crystal or an antiferroelectric liquid crystal.

### Claim 37 (depends on 35)

The method of claim 35, wherein the resin formed on the surface of the orientation film restrains an orientation control force of the orientation film with respect to the liquid crystal material.

### Claim 38 (depends on 35)

The method of claim 35, wherein the mixture is disposed between the pair of substrates after the pair of substrates are arranged so as to be opposed to each other.

### Claim 39 (depends on 35)

The method of claim 35, wherein further comprising a step of forming a plurality of thin film transistors on one of the pair of substrates.