# US 2009/0269872 A1 · Array substrate for liquid crystal display device and method of fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269872 A1
- Document ID: US20090269872A1
- Status: Published application
- Kind: A1
- Application number: 12/385,753
- Filed: 2009-04-17
- Published: 2009-10-29
- Earliest claimed: 2005-11-09
- Assignees: LG. Philips LCD Co., Ltd.
- Inventors: Seok-Woo LEE; Yong-In PARK
- Web page: https://patentgrep.com/patent/US20090269872A1

## CPC

- G02F 1/136213: {Storage capacitors associated with the pixel electrode}
- G02F 1/13454: {Drivers integrated on the active matrix substrate (G02F1/136277 takes precedence)}
- G02F 1/136231: {for reducing the number of lithographic steps}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

An array substrate for a liquid crystal display (LCD) device includes a substrate including a display region and a non-display region, a driving circuit in the non-display region, at least a first thin film transistor (TFT) in the display region, a storage capacitor in the display region including a first storage electrode, a second storage electrode, and a third storage electrode, wherein the first storage electrode includes a first semiconductor layer and a counter electrode, and the third storage electrode includes a first transparent electrode pattern and a first metal pattern, a gate line and a data line crossing each other to define a pixel region in the display region, and a pixel electrode connected to the first TFT in the pixel region.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A method of fabricating an array substrate for a liquid crystal display (LCD) device, comprising:
preparing a substrate to include a display region and a non-display region;
forming a first semiconductor layer and a second semiconductor layer in the non-display region of the substrate, and a third semiconductor layer and a fourth semiconductor layer in the display region of the substrate, the first semiconductor layer including a first region and a second region, the second semiconductor layer including a third region, a fourth region, and a fifth region, and the third semiconductor layer including a sixth region, a seventh region, and an eighth region;
forming a counter electrode on the fourth semiconductor layer to define a first storage electrode;
forming a first gate electrode over the first region of the first semiconductor layer, a first metal pattern covering the second semiconductor layer, and a second metal pattern covering the third semiconductor layer and the counter electrode;
doping the second region of the first semiconductor layer with high concentration p-type impurities;
forming a second gate electrode over the third region of the second semiconductor layer, a third gate electrode over the sixth region of the third semiconductor layer, and a second storage electrode over the first storage electrode, wherein the second gate electrode formed from the first metal pattern, and the third gate electrode and the second storage electrode are formed from the second metal pattern;
doping the fifth region of the second semiconductor layer and the eighth region of the third semiconductor layer with high concentration n-type impurities, and the fourth region of the second semiconductor layer and the seventh region of the third semiconductor layer with low concentration n-type impurities;
forming an interlayer insulating layer to cover the first, second, and third gate electrodes and the second storage electrode, the interlayer insulating layer having first and second contact holes exposing the second region of the first semiconductor layer, third and fourth contact holes exposing the fifth region of the second semiconductor layer, and fifth and sixth contact holes exposing the eighth region of the third semiconductor layer; and
forming first, second, and third source electrodes, first, second, and third drain electrodes, a third storage electrode, and a pixel electrode on the interlayer insulating layer, the first source electrode and the first drain electrode contacting the second region of the first semiconductor layer through the first and second contact holes, respectively, the second source electrode and second drain electrode contacting the fifth region of the second semiconductor layer through the third and fourth contact holes, respectively, the third source electrode and the third drain electrode contacting the eighth region of the third semiconductor layer through the fifth and sixth contact holes.

### Claim 16 (depends on 15)

The method according to claim 15, wherein each of the first, second, and third source electrodes, the first, second, and third drain electrodes, and the third storage electrode includes a transparent electrode and a opaque electrode, and the pixel electrode is an extension of the transparent electrode of the third drain electrode.

### Claim 17 (depends on 15)

The method according to claim 15, wherein the step of forming the interlayer insulating layer includes:
forming a first interlayer insulating layer of silicon oxide; and
forming a second interlayer insulating layer of silicon nitride on the first interlayer insulating layer.

### Claim 18 (depends on 17)

The method according to claim 17, further comprising heating the substrate after the first interlayer insulating layer is formed.

### Claim 19 (depends on 15)

The method according to claim 15, wherein the steps of forming the first, second, third, and fourth semiconductor layers and the first storage electrode include:
forming a polycrystalline silicon layer, a first conductive metal layer, and a first PR layer;
disposing a first mask having first, second, and third masking areas over the first PR layer, wherein the second masking area has a transmittance greater than the third masking area but less than the first masking area;
forming a first PR pattern and a second PR-pattern in the non-display region, and a third PR pattern and a fourth PR pattern in the display region by exposing and developing the first PR layer, such that the first and second PR patterns are spaced apart from each other, and the fourth PR pattern is connected to the third PR pattern and has a height greater than the first, second, and third PR patterns;
forming third, fourth, and fifth metal patterns, the first, second, third, and fourth semiconductor layers, and the counter electrode by removing the first metal layer and the polycrystalline silicon layer exposed by the first, second, and third PR patterns, wherein the third metal pattern and the first semiconductor layer correspond to the first PR pattern, the fourth metal pattern and the second semiconductor layer correspond to the second PR pattern, the fifth metal pattern and the third semiconductor layer correspond to the third PR pattern, and the counter electrode and the fourth semiconductor layer correspond to the fourth PR pattern;
exposing the third, fourth, and fifth metal pattern by ashing the first, second, and third PR patterns; and
removing the third, fourth, and fifth metal patterns and the fourth PR pattern.

### Claim 20 (depends on 19)

The method according to claim 19, further comprising forming a buffer layer between the substrate and the polycrystalline silicon layer.

### Claim 21 (depends on 15)

The method according to claim 15, wherein the forming the first gate electrode, the first metal pattern, and the second metal pattern includes:
forming a gate insulating layer, a second conductive metal layer, and a second PR layer on the first, second, and third semiconductor layers and the counter electrode;
forming fifth, sixth, and seventh PR patterns by exposing and developing the second PR layer using a second mask having a fourth and fifth masking areas, the fifth PR pattern corresponding to the first semiconductor layer and has a smaller size than the first semiconductor layer, the sixth PR pattern corresponding to the second semiconductor layer, the seventh PR pattern corresponding to the third and fourth semiconductor layers, and the fourth masking area having a greater transmittance than the fifth masking area; and
forming the first gate, the first metal pattern, and the second metal pattern by removing the second conductive metal layer exposed by the fifth, sixth, and seventh PR patterns.

### Claim 22 (depends on 15)

The method according to claim 15, wherein the steps of forming the second gate electrode, the third gate electrode, and doping the fourth, fifth, seventh, and eighth regions include:
forming a third PR layer on the first gate electrode and the first and second metal pattern;
forming eighth, ninth, tenth, and eleventh PR patterns by exposing and developing the third PR pattern using a third mask, the eight PR pattern covering the first semiconductor layer, the ninth PR pattern corresponding to the third and fourth regions of the second semiconductor layer, the tenth PR pattern corresponding to the sixth and seventh regions of the third semiconductor layer, and the eleventh PR pattern covering the fourth semiconductor layer;
removing the first and second metal patterns exposed by the eighth, ninth, tenth, and eleventh PR patterns;
doping the fifth region and the eighth region with high concentration n-type impurities;
exposing the first metal pattern corresponding to the fourth region of the second semiconductor layer, the second metal pattern corresponding to the seventh region of the third semiconductor layer, and ends of the second metal pattern corresponding to the counter electrode by ashing the eighth, ninth, tenth, and eleventh PR patterns;
forming the second gate electrode corresponding to the third region of the second semiconductor layer, the third gate electrode corresponding to the sixth region of the third semiconductor layer, and the second storage electrode corresponding to the counter electrode by removing the first and second metal patterns exposed by ashing the eighth, ninth, tenth, and eleventh PR patterns;
doping the fourth region and the seventh region with low concentration n-type impurities; and
removing the eighth, ninth, tenth, and eleventh PR patterns.

### Claim 23 (depends on 15)

The method according to claim 15, wherein the steps of forming the first, second, and third source electrodes, the first, second, and third drain electrodes, the third storage electrode, and the pixel electrode include:
forming a transparent electrode layer, a third conductive metal layer, and a fourth PR layer on the interlayer insulating layer;
disposing a fourth mask having sixth, seventh, and eighth masking areas over the fourth PR layer, the seventh masking area having a transmittance greater than the eighth masking area but less than the sixth masking area;
forming a twelfth PR pattern on the first and second contact holes, a thirteenth PR pattern on the third and fourth contact holes, a fourteenth PR pattern on the fifth and sixth contact holes, a fifteenth PR pattern over the second storage electrode, and a sixteenth PR pattern in the pixel region by exposing and developing the fourth PR layer using the fourth mask, the sixteenth PR pattern having a smaller height than the twelfth, thirteenth, fourteenth, and fifteenth PR patterns and being connected to the fifteenth PR pattern;
forming the first, second, and third source electrode and the first, second, and third drain electrode by removing the transparent electrode layer and the third conductive metal layer exposed by the twelfth, thirteenth, fourteenth, and fifteenth PR patterns;
ashing the twelfth, thirteenth, fourteenth, fifteenth, and sixteenth PR pattern such that the third conductive metal layer on the pixel electrode is exposed; and
forming the third storage electrode over the second storage electrode and the pixel electrode in the pixel region by removing the third conductive metal layer in the pixel region.

### Claim 24 (depends on 15)

The method according to claim 15, wherein the third storage electrode extends from the third drain electrode and is disposed over the second storage electrode, and the pixel electrode extends from the storage electrode into the pixel region.