# US 2009/0269867 A1 · Method of manufacturing nitride semiconductor and nitride semiconductor element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269867 A1
- Document ID: US20090269867A1
- Status: Published application
- Kind: A1
- Application number: 12/310,372
- Filed: 2007-08-23
- Published: 2009-10-29
- Earliest claimed: 2006-08-24
- Assignees: Rohm Co., Ltd.
- Inventors: Yukio Shakuda
- Web page: https://patentgrep.com/patent/US20090269867A1

## CPC

- C30B 25/14: Feed and outlet means for the gases; Modifying the flow of the reactive gases
- C30B 25/183: {being provided with a buffer layer, e.g. a lattice matching layer}
- C30B 29/403: {AIII-nitrides}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10H 20/814: having reflecting means, e.g. semiconductor Bragg reflectors
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a method of manufacturing a nitride semiconductor capable of improving the crystallinity and the surface state of the nitride semiconductor crystal formed on top of a high-temperature AlN buffer layer. An AlN buffer layer is formed on top of a growth substrate, and then nitride semiconductor crystals are grown on top of the AlN buffer layer. In a stage of manufacturing the nitride semiconductor, the crystal of the AlN buffer layer is grown at a high temperature of 900° C. or higher. In addition, an Al-source material of the AlN buffer layer is started to be supplied first to a reaction chamber and continues to be supplied without interruption, and then a N-source material is supplied intermittently.

## Claims

### Claim 1

A method of manufacturing a nitride semiconductor in which a nitride semiconductor crystal is grown on top of an AlN buffer layer, the method characterized in that
the AlN buffer layer is formed by starting supply of an Al-source material at a growth temperature of 900° C. or higher, and then by supplying a N-source material intermittently and continuing to supply the Al-source material without interruption.

### Claim 2 (depends on 1)

The method of manufacturing a nitride semiconductor according to claim 1 characterized in that the AlN buffer layer is formed to have a film thickness of 20 Å or smaller.

### Claim 3 (depends on 2)

The method of manufacturing a nitride semiconductor according to claim 2 characterized in that the crystal growth of a GaN layer to be formed on top of the AlN buffer layer is carried out at a growth pressure of 150 Torr or higher and a growth temperature of 900° C. or higher.

### Claim 4

A nitride semiconductor element in which at least an AlN buffer layer and a GaN layer are formed sequentially on top of a growth substrate, the nitride semiconductor element characterized in that
the AlN buffer layer is formed to have a film thickness of 20 Å or smaller, and so that, in a crystal-growth process of a GaN-based semiconductor layer to be formed on top of the GaN layer, a minimum value of reflectance oscillation of light from the crystal growth surface is set at 4% or smaller until a sum of the film thickness starting from the semiconductor layer next to the growth substrate reaches 1 μm.

### Claim 5 (depends on 4)

The nitride semiconductor element according to claim 4 characterized in that a GaN-based laminate including the GaN-based semiconductor layer is formed.

### Claim 6 (depends on 1)

The method of manufacturing a nitride semiconductor according to claim 1 characterized in that the crystal growth of a GaN layer to be formed on top of the AlN buffer layer is carried out at a growth pressure of 150 Torr or higher and a growth temperature of 900° C. or higher.