# US 2009/0269864 A1 · Method for fabricating a semiconductor device by considering the extinction coefficient during etching of an interlayer insulating film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269864 A1
- Document ID: US20090269864A1
- Status: Published application
- Kind: A1
- Application number: 12/253,035
- Filed: 2008-10-16
- Published: 2009-10-29
- Earliest claimed: 2007-10-17
- Assignees: Spansion LLC
- Inventors: Seiji Yokoyama; Yuuichirou Sekimoto; Shinichi Imada
- Web page: https://patentgrep.com/patent/US20090269864A1

## CPC

- H10P 50/73: {using masks for insulating materials}
- H10B 43/30: characterised by the memory core region
- H10P 50/283: {by chemical means}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- H10W 20/074: {of dielectric parts comprising thin functional dielectric layers, e.g. dielectric etch-stop, barrier, capping or liner layers}
- Y10S 438/952: Utilizing antireflective layer
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The present invention is directed to a method for manufacturing a semiconductor device by forming an ultraviolet radiation absorbing film of a silicon-rich film above a semiconductor substrate, measuring an extinction coefficient of the ultraviolet radiation absorbing film of a silicon-rich film for ultraviolet radiation, and etching the ultraviolet radiation absorbing film of a silicon-rich film under an etching condition using an oxygen gas flow rate corresponding to the extinction coefficient.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, the method comprising:
forming a silicon-rich film above a semiconductor substrate;
measuring an extinction coefficient of the silicon-rich film for ultraviolet radiation; and
etching the silicon-rich film under an etching condition using an oxygen gas flow rate corresponding to the extinction coefficient.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the silicon-rich film includes at least one of a silicon-rich oxide film and a silicon-rich nitride film.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, further comprising:
forming a first insulating film between the semiconductor substrate and the silicon-rich film;
forming a first opening by etching a part of the first insulating film below an etched area in the silicon-rich film under an etching condition using an oxygen gas flow rate corresponding to the extinction coefficient; and
forming a second opening by etching the first insulating film below the first opening under an etching condition using a predefined oxygen gas flow rate.

### Claim 4 (depends on 3)

The method for manufacturing a semiconductor device according to claim 3, wherein the first insulating film is an oxide film.

### Claim 5 (depends on 3)

The method for manufacturing a semiconductor device according to claim 3, further comprising:
forming a bit line so as to extend in the semiconductor substrate; wherein
forming of the first opening comprises forming the first opening above the bit line, and
forming of the second opening comprises forming the second opening by etching the first insulating film below the first opening so as to run through the silicon-rich film and the first insulating film and expose the bit line.

### Claim 6 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, further comprising:
forming an oxide-nitride-oxide (ONO) film comprises a charge storage layer between the semiconductor substrate and the first insulating film; and
forming an anti-reflection film on the silicon-rich film; wherein
the silicon-rich film is an ultraviolet absorbing film that absorbs ultraviolet radiation, and the first insulating film is an interlayer insulating film,
forming the first opening comprises forming the first opening by etching the anti-reflection film, the ultraviolet absorbing film, and a part of the interlayer insulating film, and
forming the second opening comprises forming the second opening by etching the interlayer insulating film and the ONO film below the first opening so as to run through the anti-reflection film, the ultraviolet absorbing film, the interlayer insulating film, and the ONO film and expose the bit line.

### Claim 7 (depends on 3)

The method for manufacturing a semiconductor device according to claim 3, further comprising:
forming a wiring layer between the semiconductor substrate and the first insulating film; wherein forming the first opening comprises forming the first opening above the wiring layer, and
forming the second opening comprises forming the second opening by etching the first insulating film below the first opening so as to run through the silicon-rich film and the first insulating film and expose the wiring layer.

### Claim 8 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the silicon-rich film is an anti-reflection film.

### Claim 9 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, further comprising:
forming a plug metal by embedding metal in the second opening.

### Claim 10 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein etching of the silicon-rich film is performed with a gas containing hydrogen and fluorine.