# US 2009/0269706 A1 · Method for forming resist pattern

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269706 A1
- Document ID: US20090269706A1
- Status: Published application
- Kind: A1
- Application number: 11/813,512
- Filed: 2005-12-13
- Published: 2009-10-29
- Earliest claimed: 2005-01-26
- Assignees: Tokyo Ohka Kogyo Co., Ltd.
- Inventors: Takeyoshi Mimura; Tomohiko Hayashi
- Web page: https://patentgrep.com/patent/US20090269706A1

## CPC

- G03F 7/0397: {the macromolecular compound having an alicyclic moiety in a side chain}
- G03F 7/0382: {the macromolecular compound being present in a chemically amplified negative photoresist composition}
- G03F 7/322: {Aqueous alkaline compositions}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A method for forming a resist pattern that includes the steps of: forming a resist film on a substrate using a resist composition including a resin component (A) that exhibits changed alkali solubility under the action of acid and an acid generator component (B) that generates acid upon exposure; selectively exposing the resist film; and developing the resist film using an alkali developing solution for a developing time of less than 30 seconds, thereby forming a resist pattern.

## Claims

### Claim 1

A method for forming a resist pattern comprising the steps of:
forming a resist film on a substrate using a resist composition including a resin component (A) that exhibits changed alkali solubility under action of acid and an acid generator component (B) that generates acid upon exposure;
selectively exposing said resist film; and
developing said resist film using an alkali developing solution for a developing time of less than 30 seconds, thereby forming a resist pattern.

### Claim 2 (depends on 1)

A method for forming a resist pattern according to claim 1, wherein said exposure is conducted using an ArF excimer laser.

### Claim 3 (depends on 2)

A method for forming a resist pattern according to claim 2, wherein said resin component (A) includes a structural unit (a) derived from an acrylate ester.

### Claim 4 (depends on 3)

A method for forming a resist pattern according to claim 3, wherein said resin component (A) includes a structural unit (a1) derived from an acrylate ester that contains an acid-dissociable, dissolution-inhibiting group.

### Claim 5 (depends on 4)

A method for forming a resist pattern according to claim 4, wherein said resin component (A) includes a structural unit (a2) derived from an acrylate ester that contains a lactone ring.

### Claim 6 (depends on 4)

A method for forming a resist pattern according to claim 4, wherein said resin component (A) includes a structural unit (a3) derived from an acrylate ester that contains a polar group-containing polycyclic group.

### Claim 7 (depends on 5)

A method for forming a resist pattern according to claim 5, wherein said resin component (A) includes a structural unit (a3) derived from an acrylate ester that contains a polar group-containing polycyclic group.

### Claim 8 (depends on 1, 7)

A method for forming a resist pattern according to any one of claim 1 through claim 7, wherein said resist composition also includes a nitrogen-containing organic compound.