# US 2009/0269692 A1 · Method of manufacturing toner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269692 A1
- Document ID: US20090269692A1
- Status: Published application
- Kind: A1
- Application number: 12/428,493
- Filed: 2009-04-23
- Published: 2009-10-29
- Earliest claimed: 2008-04-24
- Assignees: Ricoh Company, Ltd.
- Inventors: Junichi AWAMURA; Akinori SAITOH; Osamu UCHINOKURA; Tomomi SUZUKI
- Web page: https://patentgrep.com/patent/US20090269692A1

## CPC

- G03G 9/0806: {whereby chemical synthesis of at least one of the toner components takes place}
- G03G 9/0804: {whereby the components are brought together in a liquid dispersing medium}
- G03G 9/0819: {characterised by the dimensions of the particles}
- G03G 9/0821: {characterised by physical parameters (magnetic parameters G03G9/083)}
- G03G 9/0827: {characterised by their shape, e.g. degree of sphericity}
- G03G 9/08755: {Polyesters}
- G03G 9/08793: {Crosslinked polymers}
- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G 9/09716: {treated with organic compounds}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A method of manufacturing the toner comprising dispersing at least one of a binder resin or a precursor thereof, a coloring agent and a releasing agent in an organic solvent to obtain an oil phase,dispersing the oil phase in an aqueous medium with a shearing force to obtain a dispersion emulsion, wherein the dispersion emulsion process has plural stages and the shear speed A of the emulsification process of stage n is faster than the shear speed B of the emulsification process of stage n+1.

## Claims

### Claim 1

A method of manufacturing a toner comprising:
dispersing at least one of a binder resin and/or a precursor thereof, a coloring agent and a releasing agent in an organic solvent to obtain an oil phase; and
dispersing the oil phase in an aqueous medium with a shearing force to obtain a dispersion emulsion;
wherein the dispersion emulsion process has plural stages and the shear speed A of the emulsification process of stage n is faster than the shear speed B of the emulsification process of stage n+1.

### Claim 2 (depends on 1)

The method of manufacturing a toner according to claim 1,
wherein the shear speed of the emulsification process of the first stage is from 20,000 (1/S) to 140,000 (1/S).

### Claim 3 (depends on 1)

The method of manufacturing a toner according to claim 1,
dispersing at least one of a binder resin or a precursor comprises a modified polyester thereof, a coloring agent, a releasing agent in an organic solvent to obtain an oil phase;
dissolving a compound which elongates or cross-links with the precursor in the oil phase;
dispersing the oil phase in an aqueous medium comprises a particulate dispersion agent to obtain a dispersion emulsion;
conducting cross-linking reaction and elongation reaction of the precursor in the emulsified liquid dispersion; and
removing the organic solvent.

### Claim 4 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein the binder resin comprises a polyester resin.

### Claim 5 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein a content of the polyester resin in the binder resin ranges from 50 to 100% by weight.

### Claim 6 (depends on 4)

The method of manufacturing a toner according to claim 4, wherein a weight average molecular weight of portion of the polyester resin which is soluble in tetrahydrofuran (THF) ranges from 1,000 to 30,000.

### Claim 7 (depends on 6)

The method of manufacturing a toner according to claim 6, wherein the polyester resin is a polyester resin having an acid group which has an acid value of from 1.0 to 50.0 (KOHmg/g).

### Claim 8 (depends on 7)

The method of manufacturing a toner according to claim 7, wherein the polyester resin has a glass transition temperature of from 35 to 65° C.

### Claim 9 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein the precursor is a polymer having a portion reactive with a compound having an active hydrogen and a weight average molecular weight of the polymer having a portion reactive with a compound having an active hydrogen ranges from 3,000 to 20,000.

### Claim 10 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein the toner has an acid value of from 0.5 to 40.0 (KOHmg/g).

### Claim 11 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein the toner has a glass transition temperature of from 40 to 70° C.

### Claim 12 (depends on 1)

The method of manufacturing a toner according to claim 1,
wherein a laminar inorganic mineral having ions between layers in which at least part of the ions are modified by an organic ion is dissolved or dispersed in the oil phase.

### Claim 13 (depends on 1)

The toner according to claim 1, wherein the toner has a volume average particle diameter is from 3 to 7 μm.

### Claim 14 (depends on 1)

The toner according to claim 1, wherein the dispersion emulsion process has from 2 to 5 stages.

### Claim 15 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein the toner has a ratio (Dv/Dn) of a volume average particle diameter (Dv) to a number average particle diameter (Dn) of 1.30 or lower.

### Claim 16 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein the toner particle having a particle diameter of 2 μm or smaller is not greater than 20% by number.

### Claim 17 (depends on 1)

The method of manufacturing a toner according to claim 1, wherein the toner particle having a circularity of 0.93 to 0.97 on average.