# US 2009/0269659 A1 · Injection molded article and method for the manufacture thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269659 A1
- Document ID: US20090269659A1
- Status: Published application
- Kind: A1
- Application number: 12/267,060
- Filed: 2008-11-07
- Published: 2009-10-29
- Earliest claimed: 2008-04-28
- Assignees: Sabic Innovative Plastics IP B.V.
- Inventors: Juha-Matti Levasalmi
- Web page: https://patentgrep.com/patent/US20090269659A1

## CPC

- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- B29C 45/0001: {characterised by the choice of material}
- C08L 71/12: Polyphenylene oxides
- H01M 50/121: Organic material
- H01M 50/136: Flexibility or foldability
- H01M 50/143: Fireproof; Explosion-proof
- B29L 2031/7146: {Battery-cases}
- C08L 25/08: Copolymers of styrene (C08L29/08, C08L35/06, C08L55/02 take precedence)
- Y02E 60/10: Energy storage using batteries
- Y02W 30/84: Recycling of batteries or fuel cells
- Y10T 428/13: Hollow or container type article [e.g., tube, vase, etc.]
- Y10T 428/1303: Paper containing [e.g., paperboard, cardboard, fiberboard, etc.]
- Y10T 428/1352: Polymer or resin containing [i.e., natural or synthetic]
- Y10T 428/1359: Three or more layers [continuous layer]
- Y10T 428/139: Open-ended, self-supporting conduit, cylinder, or tube-type article
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Injection molded articles having large, thin sections are prepared by injection molding of a composition that includes specific amounts of poly(arylene ether) and a rubber-modified polystyrene. The specific component amounts provide the composition with a shear thinning index of 6 to 17 measured at a temperature of 260 to 300° C. and shear rates of 100 and 10,000 second−1.

## Claims

### Claim 1

An injection molded article,
wherein a portion of the injection molded article comprises
a first dimension of at least 10 centimeters,
a second dimension of at least 10 centimeters, and
a third dimension of less than 1 centimeter;
wherein the injection molded article is a product of injection molding an injection molding composition comprising
30 to 60 weight percent of a poly(arylene ether) having an intrinsic viscosity of 0.3 to 0.55 deciliter/gram measured at 25° C. in chloroform,
20 to 60 weight percent of a rubber-modified polystyrene, and
10 to 20 weight percent of a triaryl phosphate that is a liquid at one atmosphere and at least one temperature in the range 25 to 50° C.;
wherein all weight percents are based on the total weight of the injection molding composition; and
wherein the injection molding composition has a shear thinning index of 6 to 17 measured at shear rates of 100 and 10,000 second−1 at a temperature of 260 to 300° C. according to ASTM D3835.

### Claim 2 (depends on 1)

The injection molded article of claim 1, wherein the shear thinning index at 260° C. is 12 to 17.

### Claim 3 (depends on 1)

The injection molded article of claim 1, wherein the shear thinning index at 280° C. is 10 to 14.

### Claim 4 (depends on 1)

The injection molded article of claim 1, wherein the shear thinning index at 300° C. is 6 to 12.

### Claim 5 (depends on 1)

The injection molded article of claim 1, wherein the first dimension is 10 to 100 centimeters, the second dimension is 10 to 100 centimeters, and the third dimension is 0.02 to 1 centimeter.

### Claim 6 (depends on 1)

The injection molded article of claim 1, wherein the first dimension is 30 to 100 centimeters, the second dimension is 30 to 100 centimeters, and the third dimension is 0.1 to 0.5 centimeter.

### Claim 7 (depends on 1)

The injection molded article of claim 1, wherein the first and second dimensions define a plane.

### Claim 8 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a viscosity less than 1000 Pascal-seconds measured at 260° C. and a shear rate of 100 second−1 according to ASTM D3835.

### Claim 9 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a viscosity less than 600 Pascal-seconds measured at 280° C. and a shear rate of 100 second−1 according to ASTM D3835.

### Claim 10 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a viscosity less than 400 Pascal-seconds measured at 300° C. and a shear rate of 100 second−1 according to ASTM D3835.

### Claim 11 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a viscosity of 200 to 1000 Pascal-seconds measured at a temperature of 260 to 300° C. and a shear rate of 100 second−1 according to ASTM D3835.

### Claim 12 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a melt volume flow rate of 40 to 70 cubic centimeters per 10 minutes, measured at 280° C. with a 5 kilogram load according to ISO 1133.

### Claim 13 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a heat distortion temperature of 81 to 100° C., measured at 1.82 megapascals according to ASTM D648.

### Claim 14 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a flexural modulus of at least 2500 megapascals, measured at 23° C. according to ISO 178.

### Claim 15 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a flexural modulus of 2500 to 3000 megapascals, measured at 23° C. according to ISO 178.

### Claim 16 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a notched Izod impact strength of at least 50 joules/meter2 measured at 23° C. according to ISO 180.

### Claim 17 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition exhibits a notched Izod impact strength of 50 to 200 joules/meter2 measured at 23° C. according to ISO 180.

### Claim 18 (depends on 1)

The injection molded article of claim 1, wherein the injection molded article exhibits a mold shrinkage of less than or equal to 0.7 percent, measured at 23° C.

### Claim 19 (depends on 1)

The injection molded article of claim 1, wherein the injection molded article exhibits a mold shrinkage of 0.4 to 0.7 percent, measured at 23° C.

### Claim 20 (depends on 1)

The injection molded article of claim 1, wherein the rubber-modified polystyrene comprises 88 to 94 weight percent polystyrene and 6 to 12 weight percent polybutadiene.

### Claim 21 (depends on 1)

The injection molded article of claim 1, wherein the triaryl phosphate is resorcinol bis(diphenyl phosphate), bisphenol A bis(diphenyl phosphate), or a mixture thereof.

### Claim 22 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition further comprises 0.5 to 5 weight percent of a polystyrene-polybutadiene-polystyrene triblock copolymer.

### Claim 23 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition further comprises an additive selected from the group consisting of stabilizers, antioxidants, mold release agents, processing aids, drip retardants, colorants, fragrances, and mixtures thereof.

### Claim 24 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition excludes polyamides, polyesters, polyolefin homopolymers, poly(alkenyl aromatic) homopolymers, poly(phenylene sulfide)s, and hydrogenated block copolymers of an alkenyl aromatic and a conjugated diene.

### Claim 25 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition excludes any polymer other than the poly(arylene ether), the rubber-modified polystyrene, and a polystyrene-polybutadiene-polystyrene triblock copolymer, provided that the injection molding composition can comprise up to 2 weight percent of a polymeric mold release agent and/or up to 0.5 weight percent of a fluoropolymer-containing additive.

### Claim 26 (depends on 1)

The injection molded article of claim 1, wherein the injection molded article is a battery case.

### Claim 27 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition comprises at least 5 weight percent of recycled content.

### Claim 28 (depends on 1)

The injection molded article of claim 1, wherein the injection molding composition comprises 5 to 50 weight percent of recycled content.

### Claim 29 (depends on 28)

The injection molded article of claim 28, wherein the recycled content comprises material that has been recycled 1 to 10 times.

### Claim 30 (depends on 1)

The injection molded article of claim 1, wherein the injection molded article is a battery case; and wherein the recycled content comprises 0.1 to 2 weight percent lead based on the weight of the recycled content.

### Claim 31 (depends on 1)

The injection molded article of claim 1, wherein the injection molded article is a battery case; and wherein the injection molding composition comprises 0.1 to 2 weight percent lead based on the total weight of the injection molding composition.

### Claim 32 (depends on 1)

The injection molded article of claim 1,
wherein the injection molded article is a battery case comprising at least one essentially planar section having
a first dimension of 30 to 100 centimeters,
a second dimension of 30 to 100 centimeters, and
a third dimension of 0.1 to 0.5 centimeter;
wherein the injection molding composition comprises
45 to 55 weight percent of the poly(arylene ether); wherein the poly(arylene ether) comprises a poly(2,6-dimethyl-1,4-phenylene ether) having an intrinsic viscosity of 0.3 to 0.43 deciliter/gram measured at 25° C. in chloroform,
25 to 31 weight percent of the rubber-modified polystyrene, and
12 to 20 weight percent of the triaryl phosphate flame retardant; and
wherein the injection molding composition exhibits
a shear thinning index of 12 to 17 measured at shear rates of 100 and 10,000 second−1 at a temperature of 260° C. according to ASTM D3835
a viscosity of 600 to 1000 Pascal-seconds measured at a temperature of 260° C. and a shear rate of 100 second−1 according to ASTM D3835,
a melt volume flow rate of 30 to 60 cubic centimeters per 10 minutes measured at 280° C. with a 5 kilogram load according to ISO 1133,
a heat distortion temperature of 81 to 100° C., measured at 1.82 megapascals according to ASTM D648, and
a mold shrinkage of 0.4 to 0.7 percent, measured at 23° C.

### Claim 33 (depends on 32)

The injection molded article of claim 32, wherein the injection molding composition further exhibits a UL 94 Vertical Burning Test rating of V-0 or V-1, measured at a sample thickness in the range of 1.5 to 3 millimeters.

### Claim 34

A method of injection molding, comprising:
injection molding an injection molding composition to form an injection molded article;
wherein a portion of the injection molded article comprises
a first dimension of at least 10 centimeters,
a second dimension of at least 10 centimeters, and
a third dimension of less than 1 centimeter;
wherein the injection molded article is a product of injection molding an injection molding composition comprising
30 to 60 weight percent of a poly(arylene ether) having an intrinsic viscosity of 0.3 to 0.55 deciliter/gram measured at 25° C. in chloroform,
20 to 60 weight percent of a rubber-modified polystyrene, and
10 to 20 weight percent of a triaryl phosphate that is a liquid at one atmosphere and at least one temperature in the range 25 to 50° C.;
wherein all weight percents are based on the total weight of the injection molding composition; and
wherein the injection molding composition has a shear thinning index of 6 to 17 measured at shear rates of 100 and 10,000 second−1 at a temperature of 260 to 300° C. according to ASTM D3835.

### Claim 35 (depends on 34)

The method of injection molding of claim 34, wherein said injection molding comprises using a barrel temperature of 260 to 300° C. and a mold temperature of 50 to 90° C.

### Claim 36 (depends on 34)

The method of injection molding of claim 34,
wherein the injection molded article is a battery case comprising at least one essentially planar section having
a first dimension of 30 to 100 centimeters,
a second dimension of 30 to 100 centimeters, and
a third dimension of 0.1 to 0.5 centimeter;
wherein the injection molding composition comprises
45 to 55 weight percent of the poly(arylene ether); therein the poly(arylene ether) comprises a poly(2,6-dimethyl-1,4-phenylene ether) having an intrinsic viscosity of 0.3 to 0.43 deciliter/gram measured at 25° C. in chloroform,
25 to 31 weight percent of the rubber-modified polystyrene, and
12 to 20 weight percent of the triaryl phosphate flame retardant; and
wherein the injection molding composition exhibits
a shear thinning index of 12 to 17 measured at shear rates of 100 and 10,000 second−1 at a temperature of 260° C. according to ASTM D3835
a viscosity of 600 to 1000 Pascal-seconds measured at a temperature of 260° C. and a shear rate of 100 second−1 according to ASTM D3835,
a melt volume flow rate of 30 to 60 cubic centimeters per 10 minutes measured at 280° C. with a 5 kilogram load according to ISO 1133,
a heat distortion temperature of 81 to 100° C., measured at 1.82 megapascals according to ASTM D648, and
a mold shrinkage of 0.4 to 0.7 percent, measured at 23° C.;
wherein said injection molding comprises using a barrel temperature of 260 to 300° C. and a mold temperature of 50 to 90° C.

### Claim 37 (depends on 34)

The method of injection molding of claim 34, wherein the injection molding composition comprises at least 1 weight percent of recycled content.

### Claim 38 (depends on 34)

The method of injection molding of claim 34, wherein the injection molding composition comprises 5 to 50 weight percent of recycled content.

### Claim 39 (depends on 38)

The method of injection molding of claim 38, wherein the recycled content comprises 0.1 to 2 weight percent lead based on the weight of the recycled content.

### Claim 40 (depends on 36)

The method of injection molding of claim 36, wherein the injection molding composition comprises 0.1 to 2 weight percent lead based on the total weight of the injection molding composition.

### Claim 41 (depends on 34)

An injection molded article prepared by the method of claim 34.