# US 2009/0269574 A1 · Functional multilayer anisotropic conductive adhesive film and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269574 A1
- Document ID: US20090269574A1
- Status: Published application
- Kind: A1
- Application number: 12/137,868
- Filed: 2008-06-12
- Published: 2009-10-29
- Earliest claimed: 2008-04-29
- Assignees: Guangdong Dongbond Technology Co., Ltd.
- Inventors: Ping LIU
- Web page: https://patentgrep.com/patent/US20090269574A1

## CPC

- C09J 7/29: Laminated material (metallised plastics C09J7/22)
- C08K 2201/001: Conductive additives
- C09J 2203/326: for bonding electronic components such as wafers, chips or semiconductors
- C09J 2301/41: additives as essential feature of the carrier layer
- C09J 2433/00: Presence of (meth)acrylic polymer
- Y10T 428/14: Layer or component removable to expose adhesive
- Y10T 428/25: Web or sheet containing structurally defined element or component and including a second component containing structurally defined particles
- Y10T 428/254: Polymeric or resinous material
- Y10T 428/31515: As intermediate layer
- Y10T 428/31924: Including polyene monomers
- Y10T 428/31928: Ester, halide or nitrile of addition polymer
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A functional multilayer anisotropic conductive adhesive film, capable of bonding and package 0.18-0.13 micron IC chips and high density COF, includes a monomer layer, a reinforcing layer, a low-temperature, hot-melt resin layer, and a conductive particle layer, successively bonded by coating and drying processes. The monomer layer comprises a copolymer of butyl acrylate, methyl acrylate, glycol acrylate, and tetramethyl butyl peroxy-2-ethyl hexanoate. The reinforcing layer comprises long chain imidazole derivatives. The hot-melt resin layer comprises polymer of tocopheroxyl, novolac epoxy, acrylic rubbers and elastic mixture of acrylic rubbers and styrene-butadiene rubbers. The conductive particle layer comprises conductive particles and micro-encapsulating resin for receiving the conductive particles. Diameter of the conductive particles is selected from the group consisting of 3.00 μm±0.05, 3.25 μm±0.05, 3.50 μm±0.05, 3.75 μm±0.05 and 4.00 μm±0.05.

## Claims

### Claim 1

A functional multilayer anisotropic conductive adhesive film comprising:
a monomer layer, comprising a copolymer of butyl acrylate, methyl acrylate, glycol acrylate, and tetramethyl butyl peroxy-2-ethyl hexanoate;
a reinforcing layer, comprising long chain imidazole derivatives;
a low-temperature, hot-melt resin layer, comprising polymer of tocopheroxyl, novolac epoxy, acrylic rubbers and elastic mixture of acrylic rubbers and styrene-butadiene rubbers; and
a conductive particle layer, comprising conductive particles and low-temperature, hot-melt, micro-encapsulating resin for receiving the conductive particles, diameter of the conductive particles selected from the group consisting of 3.00 μm±0.05, 3.25 μm±0.05, 3.50 μm±0.05, 3.75 μm±0.05 and 4.00 μm±0.05;
wherein the monomer layer, the reinforcing layer, the resin layer and the conductive particle layer are successively bonded by coating and drying processes.

### Claim 2 (depends on 1)

The functional multilayer anisotropic conductive adhesive film as in claim 1, wherein in polymerization of the resin layer, the tocopheroxyl is YP-70, and is present in an amount of 10-30 parts by weight;
the novolac epoxy is selected from the group consisting of F-55, F-51 and F-44, and is present in an amount of 10-20 parts by weight;
bulk density of the acrylic rubbers is 0.48±0.1 g/cc, volatility<1.0%, Tg −30° C., and the acrylic rubbers are present in an amount of 10-20 parts by weight;
the styrene-butadiene rubbers in the elastic mixture is SBR1502, the elastic mixture is present in an amount of 5-10 parts by weight; and
the long chain imidazole derivatives in the reinforcing layer are a synthesis of 2,4-diamino-6-[-2-undecyl imidazolyl(1)]-ethyl-cis-triazine, 1-cyanoethyl-2-undecyl-imidazole trimellitate, and isocyanate derivative, and are present in an amount of 0.75-5 parts by weight.

### Claim 3 (depends on 1)

The functional multilayer anisotropic conductive adhesive film as in claim 1, wherein content of the conductive particles is 30-40 parts by weight per 500 parts by total weight of the anisotropic conductive adhesive film.

### Claim 4 (depends on 1)

The functional multilayer anisotropic conductive adhesive film as in claim 1, wherein content of the conductive particles is 5-10 parts by weight per 500 parts by the total weight of the anisotropic conductive adhesive film, and wherein weight ratio of the butyl acrylate, the methyl acrylate, the glycol acrylates, and the tetramethyl butyl peroxy-2-ethyl hexonate is set in 7:3:2:1 according to requirement of corresponding chipset.

### Claim 5

A preparation method of functional multilayer anisotropic conductive adhesive film, adopting suspension polymerization means, comprising the following steps:
A, mixing and stirring tocopheroxyl, novolac epoxy, and solvent;
B, adding acrylic rubbers and elastic mixture of acrylic rubbers and styrene-butadiene rubbers into the admixture obtained from step A, stirring;
C, adding acrylic rubbers and solvent into the admixture obtained from step B, dissolving and stirring;
D, waiting as viscosity of the polymer obtained from step C naturally reduces to a degree that no more polymerization occurs, a later use coating stuff for a low-temperature, hot-melt resin layer obtained;
E, stirring long chain imidazole derivatives to form a later use coating stuff for a reinforcing layer;
F, a stirring apparatus stirring micro-encapsulating resin, and then combining conductive particles in a conductive particle layer;
G, mixing butyl acrylate, methyl acrylate and glycol acrylate, under presence of tetramethyl butyl peroxy-2-ethyl hexanoate, a copolymer formed, after stirring and foam breaking, a later use coating stuff for a monomer layer obtained;
H, coating process carried out under temperature of 100° C.-135° C. to successively form the conductive particle layer, low-temperature, hot-melt resin layer, the reinforcing layer, and the monomer layer, thereby the functional multilayer anisotropic conductive adhesive film of the present invention obtained.

### Claim 6 (depends on 5)

The preparation method of functional multilayer anisotropic conductive adhesive film as in claim 5, wherein,
the tocopheroxyl is YP-70, and is present in an amount of 10-30 parts by weight;
the novolac epoxy is selected from the group consisting of F-51 and F-44, and is present in an amount of 10-20 parts by weight;
bulk density of the acrylic rubbers is 0.48±0.1 g/cc, volatility<1.0%, Tg −30° C., solution viscosity under temperature of 25° C. is 5000-10000 mPa·S, and the acrylic rubbers are present in an amount of 10-20 parts by weight;
the styrene-butadiene rubbers in the elastic mixture are SBR1502, Mooney viscosity of natural rubber is ML100° C. (1+4)45-55, stretching stress 300%, mpa (35 minutes) 14.1-18.6, tensile strength mpa (35 minutes)>23.7, elongation at break % (35 minutes)>415; the elastic mixture is present in an amount of 5-10 parts by weight;
the long chain imidazole derivatives are a synthesis of 2,4-diamino-6-[-2-undecyl imidazolyl (1)]-ethyl-cis-triazine, 1-cyanoethyl-2-undecyl-imidazole trimellitate, and isocyanate derivative; and are present in an amount of 0.75-5 parts by weight;
diameter of the conductive particles is selected from the group consisting of 3.00 μm±0.05, 3.25 μm±0.05, 3.50 μm±0.05, 3.75 μm±0.05 and 4.00 μm±0.05, content of the conductive particles is 30-40 parts by weight per 500 parts by total weight of the anisotropic conductive adhesive film;
content of monomer in the monomer layer is 5-10 parts by weight per 500 parts by the total weight of the anisotropic conductive adhesive film, wherein weight ratio of the butyl acrylate, the methyl acrylate, the glycol acrylates, and the tetramethyl butyl peroxy-2-ethyl hexanoate is set in 7:3:2:1 according to requirement of corresponding chipset.

### Claim 7 (depends on 5)

The preparation method of functional multilayer anisotropic conductive adhesive film as in claim 5, wherein the long chain imidazole derivatives in the reinforcing layer is obtained by the following processes: mixing the 2,4-diamino-6-[-2-undecyl imidazolyl(1)]-ethyl-cis-triazine, and 1-cyanoethyl-2-undecyl-imidazole trimellitate with a weight ratio of 1:1, keeping them reacting for 3 hours, and then heating reactant from the mixing process up to 50° C., adding toluene-2,4-diisocyanate and solvent into the reactant from mixing process with a weight ratio of 0.8:60:30, and keeping reacting for 5 hours.

### Claim 8 (depends on 5)

The preparation method of functional multilayer anisotropic conductive adhesive film as in claim 5, wherein preparation of the elastic mixture to improve its thermal aging property is that: mixing and preparing the acrylic rubbers and the styrene-butadiene rubbers with weight ratio of 10:5, and then physically admixing trace meta-alkaline reinforcing agent containing silica, silane coupling agent, and quaternary ammonium salt, in accordance with a weight ratio of 1:0.2:0.3.

### Claim 9 (depends on 5)

The preparation method of functional multilayer anisotropic conductive adhesive film as in claim 5, wherein the solvent is obtained by mixing toluene and ethyl acetate with a weight ratio of 4:6, and a solution is prepared with the reactant thereof by a weight concentration of 20%-40%.

### Claim 10 (depends on 2)

The functional multilayer anisotropic conductive adhesive film as in claim 2, wherein content of the conductive particles is 30-40 parts by weight per 500 parts by total weight of the anisotropic conductive adhesive film.

### Claim 11 (depends on 2)

The functional multilayer anisotropic conductive adhesive film as in claim 2, wherein content of the conductive particles is 5-10 parts by weight per 500 parts by the total weight of the anisotropic conductive adhesive film, and wherein weight ratio of the butyl acrylate, the methyl acrylate, the glycol acrylates, and the tetramethyl butyl peroxy-2-ethyl hexonate is set in 7:3:2:1 according to requirement of corresponding chipset.

### Claim 12 (depends on 6)

The preparation method of functional multilayer anisotropic conductive adhesive film as in claim 6, wherein the long chain imidazole derivatives in the reinforcing layer is obtained by the following processes: mixing the 2,4-diamino-6-[-2-undecyl imidazolyl(1)]-ethyl-cis-triazine, and 1-cyanoethyl-2-undecyl-imidazole trimellitate with a weight ratio of 1:1, keeping them reacting for 3 hours, and then heating reactant from the mixing process up to 50° C., adding toluene-2,4-diisocyanate and solvent into the reactant from mixing process with a weight ratio of 0.8:60:30, and keeping reacting for 5 hours.

### Claim 13 (depends on 6)

The preparation method of functional multilayer anisotropic conductive adhesive film as in claim 6, wherein preparation of the elastic mixture to improve its thermal aging property is that: mixing and preparing the acrylic rubbers and the styrene-butadiene rubbers with weight ratio of 10:5, and then physically admixing trace meta-alkaline reinforcing agent containing silica, silane coupling agent, and quaternary ammonium salt, in accordance with a weight ratio of 1:0.2:0.3.

### Claim 14 (depends on 6)

The preparation method of functional multilayer anisotropic conductive adhesive film as in claim 6, wherein the solvent is obtained by mixing toluene and ethyl acetate with a weight ratio of 4:6, and a solution is prepared with the reactant thereof by a weight concentration of 20%-40%.