# US 2009/0269539 A1 · Information Recording Medium and Method for Manufacturing Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269539 A1
- Document ID: US20090269539A1
- Status: Published application
- Kind: A1
- Application number: 11/887,588
- Filed: 2006-03-24
- Published: 2009-10-29
- Earliest claimed: 2005-04-01
- Assignees: Panasonic Corporation
- Inventors: Yukako Doi; Rie Kojima; Noboru Yamada
- Web page: https://patentgrep.com/patent/US20090269539A1

## CPC

- G11B 7/243: comprising inorganic materials only, e.g. ablative layers
- G11B 7/266: {Sputtering or spin-coating layers (sputtering in general C23C14/24; spin-coating in general B05D1/005)}
- G11B 2007/24308: {transition metal elements of group 11 (Cu, Ag, Au)}
- G11B 2007/24312: {group 14 elements (e.g. Si, Ge, Sn)}
- G11B 2007/24314: {group 15 elements (e.g. Sb, Bi)}
- G11B 2007/24316: {group 16 elements (i.e. chalcogenides, Se, Te)}
- G11B 2007/25706: {containing transition metal elements (Zn, Fe, Co, Ni, Pt)}
- G11B 2007/25708: {containing group 13 elements (B, Al, Ga)}
- G11B 2007/2571: {containing group 14 elements except carbon (Si, Ge, Sn, Pb)}
- G11B 2007/25715: {containing oxygen}
- Y10T 428/21: Circular sheet or circular blank
- Y10T 428/26: Web or sheet containing structurally defined element or component, the element or component having a specified physical dimension
- Y10T 428/31678: Of metal
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides an information recording medium with high reliability and excellent repeated rewriting performance even when no interface layer is formed and a method for manufacturing the same. Accordingly, the information recording medium for carrying out recording and/or reproducing by light irradiation or electric energy application has a material layer containing at least one element selected from a group GM consisting of Sn and Ga, at least one element selected from a group GL consisting of Ta and Y, and oxygen.

## Claims

### Claim 1

An information recording medium for recording and/or reproducing information by applying light or electric energy, comprising a material layer containing at least one element selected from a group GM consisting of Sn and Ga, at least one element selected from a group GL consisting of Ta and Y, and oxygen.

### Claim 2 (depends on 1)

The information recording medium according to claim 1, wherein the material layer contains a material defined by the following formula: Mh1Oi1Lj1
wherein M denotes at least one element selected from the group GM; L denotes at least one element selected from the group GL; and h1 , i1 , and j1 are expressed on the basis of at % and satisfy the following; 5≦h1≦40, 40≦i1≦70, 0≦j1≦35, and h1+i1+j1=100.

### Claim 3 (depends on 2)

The information recording medium according to claim 2, wherein M in the
formula denotes Sn.

### Claim 4 (depends on 2)

The information recording medium according to claim 2, wherein M in the formula denotes Sn and Ga.

### Claim 5 (depends on 2)

The information recording medium according to claim 2, wherein L in the formula denotes Y.

### Claim 6 (depends on 1)

The information recording medium according to claim 1, wherein the material layer contains an oxide of at least one element selected from the group GM and an oxide of at least one element selected from the group GL.

### Claim 7 (depends on 6)

The information recording medium according to claim 6, wherein the material layer contains a material defined by the following formula:
DxA100-x
wherein D denotes at least one oxide selected from SnO2 and Ga2O3; A denotes at least one oxide selected from Ta2O5 and Y2O3; and x is expressed on the basis of mol % and satisfies 30≦x≦95.

### Claim 8 (depends on 1)

The information recording medium according to claim 1, further comprising a phase-change type recording layer.

### Claim 9 (depends on 8)

The information recording medium according to claim 8, wherein the material layer is in contact with at least one face of the recording layer.

### Claim 10 (depends on 8)

The information recording medium according to claim 8, wherein the recording layer contains at least one material selected from Ge—Sb—Te, Ge—Sn—Sb—Te, Ge—Bi—Te, Ge—Sn—Bi—Te, Ge—Sb—Bi—Te, Ge—In—Bi—Te, Ag—In—Sb—Te, and Sb—Te.

### Claim 11 (depends on 8)

The information recording medium according to claim 8, wherein the recording layer has a thickness of 15 nm or thinner.

### Claim 12 (depends on 1)

A method for manufacturing the information recording medium according to claim 1, comprising forming the material layer by a sputtering method using a sputtering target containing at least one element selected from the group GM consisting of Sn and Ga, at least one element selected from the group GL consisting of Ta and Y, and oxygen.

### Claim 13 (depends on 12)

The method for manufacturing the information recording medium according to claim 12, wherein the sputtering target contains a material defined by the following formula:
Mh2Oi2Lj2
wherein M denotes at least one element selected from the group GM; L denotes at least one element selected from the group GL; and h2, i2, and j2 are expressed on the basis of at % and satisfy the following: 5≦h2≦40, 40≦i2≦70, 0≦j2≦35, and h2+i2+j2=100.

### Claim 14 (depends on 13)

The method for manufacturing the information recording medium according to claim 13, wherein M of the sputtering target contains Sn and/or Ga.

### Claim 15 (depends on 13)

The method for manufacturing the information recording medium according to claim 13, wherein L of the sputtering target contains Y.

### Claim 16 (depends on 12)

The method for manufacturing the information recording medium according to claim 12, wherein the sputtering target contains an oxide of at least one element selected from the group GM and an oxide of at least one element selected from the group GL.

### Claim 17 (depends on 16)

The method for manufacturing the information recording medium according to claim 16, wherein the sputtering target contains 30 mol % or more of an oxide of Sn and/or Ga.

### Claim 18 (depends on 12)

The method for manufacturing the information recording medium according to claim 12, wherein the sputtering target contains a material defined by the following formula:
(D)x(A)100-x
wherein D denotes at least one oxide selected from SnO2 and Ga2O3; A denotes at least one oxide selected from Ta2O5 and Y2O3; and x is expressed on the basis of mol % and satisfies 30≦x≦95.