# US 2009/0269507 A1 · Selective cobalt deposition on copper surfaces

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269507 A1
- Document ID: US20090269507A1
- Status: Published application
- Kind: A1
- Application number: 12/111,921
- Filed: 2008-04-29
- Published: 2009-10-29
- Earliest claimed: 2008-04-29
- Inventors: Sang-Ho Yu; Kevin Moraes; Seshadri Ganguli; Hua Chung; See-Eng Phan
- Web page: https://patentgrep.com/patent/US20090269507A1

## CPC

- C23C 16/16: from metal carbonyl compounds
- C23C 16/0218: {in a reactive atmosphere (C23C16/0227 takes precedence)}
- C23C 16/0245: {by etching with a plasma}
- C23C 16/18: from metallo-organic compounds
- C23C 16/4554: {Plasma being used non-continuously in between ALD reactions (C23C16/56 takes precedence)}
- C23C 16/45542: {Plasma being used non-continuously during the ALD reactions}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/432: {using selective deposition}
- H10P 14/44: Physical vapour deposition [PVD]
- H10P 70/27: {during, before or after processing of conductive materials, e.g. polysilicon or amorphous silicon layers}
- H10P 70/277: {the processing being a planarisation of conductive layers}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/038: {covering conductive structures (H10W20/037 takes precedence)}
- H10W 20/0523: {by irradiating with ultraviolet or particle radiation}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments of the invention provide processes to selectively form a cobalt layer on a copper surface over exposed dielectric surfaces. In one embodiment, a method for capping a copper surface on a substrate is provided which includes positioning a substrate within a processing chamber, wherein the substrate contains a contaminated copper surface and a dielectric surface, exposing the contaminated copper surface to a reducing agent while forming a copper surface during a pre-treatment process, exposing the substrate to a cobalt precursor gas to selectively form a cobalt capping layer over the copper surface while leaving exposed the dielectric surface during a vapor deposition process, and depositing a dielectric barrier layer over the cobalt capping layer and the dielectric surface. In another embodiment, a deposition-treatment cycle includes performing the vapor deposition process and subsequently a post-treatment process, which deposition-treatment cycle may be repeated to form multiple cobalt capping layers.

## Claims

### Claim 1

A method for capping a copper surface on a substrate, comprising:
positioning a substrate within a processing chamber, wherein the substrate comprises a contaminated copper surface and a dielectric surface;
exposing the contaminated copper surface to a reducing agent while forming a metallic copper surface during a pre-treatment process;
exposing the substrate to a cobalt precursor gas to selectively form a cobalt capping layer over the metallic copper surface while leaving exposed the dielectric surface during a vapor deposition process; and
depositing a dielectric barrier layer over the cobalt capping layer and the dielectric surface.

### Claim 2 (depends on 1)

The method of claim 1, further comprising chemically reducing copper oxides on the contaminated copper surface to form the metallic copper surface during the pre-treatment process.

### Claim 3 (depends on 1)

The method of claim 1, wherein the contaminated copper surface is exposed to the reducing agent and a plasma is ignited during the pre-treatment process, the reducing agent comprises a reagent selected from the group consisting of nitrogen (N2), ammonia (NH3), hydrogen (H2), ammonia/nitrogen mixture, and combinations thereof.

### Claim 4 (depends on 3)

The method of claim 3, wherein the contaminated copper surface is exposed to the plasma for a time period within a range from about 5 seconds to about 15 seconds.

### Claim 5 (depends on 1)

The method of claim 1, wherein the reducing agent comprises hydrogen gas, the pre-treatment process is a thermal process, and the substrate is heated to a temperature within a range from about 200° C. to about 400° C. during the thermal process.

### Claim 6 (depends on 1)

The method of claim 1, further comprising exposing the cobalt capping layer to a reagent and a plasma during a post-treatment process prior to depositing the dielectric barrier layer, the reagent is selected from the group consisting of nitrogen (N2), ammonia (NH3), hydrogen (H2), ammonia/nitrogen mixture, and combinations thereof.

### Claim 7 (depends on 6)

The method of claim 6, wherein a deposition-treatment cycle comprises performing the vapor deposition process and subsequently the post-treatment process, and the deposition-treatment cycle is performed 2, 3, or more times to deposit multiple cobalt capping layers.

### Claim 8 (depends on 7)

The method of claim 7, wherein each of the cobalt capping layers is deposited to a thickness within a range from about 3 Å to about 5 Å during each of the deposition-treatment cycles.

### Claim 9 (depends on 1)

The method of claim 1, wherein the cobalt capping layer has a thickness within a range from about 4 Å to about 20 Å.

### Claim 10 (depends on 1)

The method of claim 1, wherein the cobalt capping layer has a thickness of less than about 10 Å.

### Claim 11 (depends on 10)

The method of claim 10, wherein the substrate is exposed to a deposition gas comprising the cobalt precursor gas and hydrogen gas during the vapor deposition process, the vapor deposition process is a thermal chemical vapor deposition process or an atomic layer deposition process.

### Claim 12 (depends on 1)

The method of claim 1, wherein the cobalt precursor gas comprises a cobalt precursor which has the general chemical formula (CO)xCoyLz, wherein:
X is 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, or 12;
Y is 1, 2, 3, 4, or 5;
Z is 1, 2, 3, 4, 5, 6, 7, or 8; and
L is a ligand independently selected from the group consisting of cyclopentadienyl, alkylcyclopentadienyl, methylcyclopentadienyl, pentamethylcyclopentadienyl, pentadienyl, alkylpentadienyl, cyclobutadienyl, butadienyl, allyl, ethylene, propylene, alkenes, dialkenes, alkynes, nitrosyl, ammonia, derivatives thereof, and combinations thereof.

### Claim 13 (depends on 1)

The method of claim 1, wherein the cobalt precursor gas comprises a cobalt precursor selected from the group consisting of tricarbonyl allyl cobalt, cyclopentadienyl cobalt bis(carbonyl), methylcyclopentadienyl cobalt bis(carbonyl), ethylcyclopentadienyl cobalt bis(carbonyl), pentamethylcyclopentadienyl cobalt bis(carbonyl), dicobalt octa(carbonyl), nitrosyl cobalt tris(carbonyl), bis(cyclopentadienyl) cobalt, (cyclopentadienyl) cobalt (cyclohexadienyl), cyclopentadienyl cobalt (1,3-hexadienyl), (cyclobutadienyl) cobalt (cyclopentadienyl), bis(methylcyclopentadienyl) cobalt, (cyclopentadienyl) cobalt (5-methylcyclopentadienyl), bis(ethylene) cobalt (pentamethylcyclopentadienyl), derivatives thereof, complexes thereof, plasmas thereof, and combinations thereof.

### Claim 14 (depends on 13)

The method of claim 13, wherein the cobalt precursor comprises cyclopentadienyl cobalt bis(carbonyl).

### Claim 15

A method for capping a copper surface on a substrate, comprising:
positioning a substrate within a processing chamber, wherein the substrate comprises a copper oxide surface and a dielectric surface;
exposing the copper oxide surface to an ammonia plasma or a hydrogen plasma while forming a metallic copper surface during a pre-treatment process;
exposing the substrate to a cobalt precursor gas to selectively form a cobalt capping layer over the metallic copper surface while leaving exposed the dielectric surface during a vapor deposition process;
exposing the cobalt capping layer to a plasma during a post-treatment process; and
depositing a dielectric barrier layer over the cobalt capping layer and the dielectric surface.

### Claim 16 (depends on 15)

The method of claim 15, wherein a deposition-treatment cycle comprises performing the vapor deposition process and subsequently the post-treatment process, and the deposition-treatment cycle is performed 2, 3, or more times to deposit multiple cobalt capping layers.

### Claim 17 (depends on 16)

The method of claim 16, wherein each of the cobalt capping layers is deposited to a thickness within a range from about 3 Å to about 5 Å during each of the deposition-treatment cycles.

### Claim 18 (depends on 15)

The method of claim 15, wherein the copper oxide surface is exposed to the ammonia plasma or the hydrogen plasma for a time period within a range from about 5 seconds to about 15 seconds during a pre-treatment process.

### Claim 19 (depends on 15)

The method of claim 15, wherein a reagent and the plasma are exposed to the cobalt capping layer during the post-treatment process, and the reagent is selected from the group consisting of nitrogen (N2), ammonia (NH3), hydrogen (H2), ammonia/nitrogen mixture, and combinations thereof.

### Claim 20

A method for capping a copper surface on a substrate, comprising:
positioning a substrate within a processing chamber, wherein the substrate comprises a copper oxide surface and a dielectric surface;
exposing the copper oxide surface to an ammonia plasma or a hydrogen plasma while forming a metallic copper surface during a pre-treatment process;
exposing the substrate to a cobalt precursor gas and hydrogen gas to selectively form a cobalt capping layer over the metallic copper surface while leaving exposed the dielectric surface during a vapor deposition process; and
exposing the cobalt capping layer to a plasma and a reagent selected from the group consisting of nitrogen (N2), ammonia (NH3), hydrogen (H2), ammonia/nitrogen mixture, and combinations thereof during a post-treatment process.

### Claim 21 (depends on 20)

The method of claim 20, wherein a deposition-treatment cycle comprises performing the vapor deposition process and subsequently the post-treatment process, and the deposition-treatment cycle is performed 2, 3, or more times to deposit multiple cobalt capping layers.

### Claim 22 (depends on 21)

The method of claim 21, wherein each of the cobalt capping layers is deposited to a thickness within a range from about 3 Å to about 5 Å during each of the deposition-treatment cycles.

### Claim 23 (depends on 20)

The method of claim 20, further comprising depositing a dielectric barrier layer over the cobalt capping layer and the dielectric surface.

### Claim 24

A method for capping a copper surface on a substrate, comprising:
positioning a substrate within a processing chamber, wherein the substrate comprises a contaminated copper surface and a dielectric surface;
exposing the contaminated copper surface to a reducing agent while forming a metallic copper surface during a pre-treatment process;
depositing a cobalt capping material over the metallic copper surface while leaving exposed the dielectric surface during a deposition-treatment cycle, comprising:
exposing the substrate to a cobalt precursor gas to selectively form a first cobalt layer over the metallic copper surface while leaving exposed the dielectric surface during a vapor deposition process;
exposing the first cobalt layer to a plasma comprising nitrogen, ammonia, an ammonia/nitrogen mixture, or hydrogen during a treatment process;
exposing the substrate to the cobalt precursor gas to selectively form a second cobalt layer over the first cobalt layer while leaving exposed the dielectric surface during the vapor deposition process;
exposing the second cobalt layer to the plasma during the treatment process; and
depositing a dielectric barrier layer over the cobalt capping material and the dielectric surface.

### Claim 25 (depends on 24)

The method of claim 24, further comprising:
exposing the substrate to the cobalt precursor gas to selectively form a third cobalt layer over the second cobalt layer while leaving exposed the dielectric surface during the vapor deposition process; and
exposing the third cobalt layer to the plasma during the treatment process.