# US 2009/0269015 A1 · Optical fiber provided with reliable coating layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0269015 A1
- Document ID: US20090269015A1
- Status: Published application
- Kind: A1
- Application number: 11/659,500
- Filed: 2006-07-28
- Published: 2009-10-29
- Earliest claimed: 2006-07-28
- Assignees: Furukawa Electric Co., Ltd.
- Inventors: Yasuo Nakajima; Hiroki Tanaka; Yoshihiro Arashitani; Takayoshi Ono
- Web page: https://patentgrep.com/patent/US20090269015A1

## CPC

- C03C 25/1065: Multiple coatings
- C03C 25/106: Single coatings
- G02B 6/02395: {Glass optical fibre with a protective coating, e.g. two layer polymer coating deposited directly on a silica cladding surface during fibre manufacture (G02B6/02052, G02B6/02057, G02B6/024, G02B6/032, G02B6/105, G02B6/14 take precedence; coating on fibre gratings G02B6/02104; multilayer core or cladding G02B6/036; reinforcing splice joints G02B6/2558; optical cables, i.e. comprising protective structures external to the protective coating such as a jacket or plural coated optical fibres G02B6/44; coating of glass to obtain optical fibres C03C25/104)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

An optical fiber is provided, which is unlikely to cause interlayer delamination between a glass optical fiber and a primary coating layer even when it is immersed in water. The optical fiber of the present invention includes a glass optical fiber 1 consisting of a core and a cladding, a primary coating layer 2 overlaid on the glass optical fiber, and a secondary coating layer 3 overlaid on the primary coating layer, wherein the relaxation modulus of the secondary coating layer is set at 400 MPa or less.

## Claims

### Claim 1

An optical fiber comprising a glass optical fiber consisting of a core and a cladding, a primary coating layer overlaid on said glass optical fiber, and a secondary coating layer provided on said primary coating layer, characterized in that the relaxation modulus of said secondary coating layer is 400 MPa or less.

### Claim 2 (depends on 1)

The optical fiber according to claim 1, characterized in that a silane coupling agent of 1.0 or more parts per hundred of resin is added to a resin used for the primary coating layer.