# US 2009/0268768 A1 · Method of making nitride semiconductor laser, method of making epitaxial wafer, and nitride semiconductor laser

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0268768 A1
- Document ID: US20090268768A1
- Status: Published application
- Kind: A1
- Application number: 12/429,322
- Filed: 2009-04-24
- Published: 2009-10-29
- Earliest claimed: 2008-04-25
- Assignees: Sumitomo Electric Industries, Ltd.
- Inventors: Masaki UENO; Takashi KYONO
- Web page: https://patentgrep.com/patent/US20090268768A1

## CPC

- H01S 5/34333: {with a well layer based on Ga(In)N or Ga(In)P, e.g. blue laser}
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2908: {Nitrides}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H01S 2302/00: Amplification / lasing wavelength
- H01S 2304/04: MOCVD or MOVPE
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of making a nitride semiconductor laser comprises forming a first InGaN film for an active layer on a gallium nitride based semiconductor region, and the first InGaN film has a first thickness. In the formation of the first InGaN film, a first gallium raw material, a first indium raw material, and a first nitrogen raw material are supplied to a reactor to deposit a first InGaN for forming the first InGaN film at a first temperature, and the first InGaN has a thickness thinner than the first thickness. Next, the first InGaN is heat-treated at a second temperature lower than the first temperature in the reactor, while supplying a second indium raw material and a second nitrogen raw material to the reactor. Then, after the heat treatment, a second InGaN is deposited at least once to form the first InGaN film.

## Claims

### Claim 1

A method of making a nitride semiconductor laser, comprising the step of forming a first InGaN film for an active layer on a gallium nitride based semiconductor region, the first InGaN film having a first thickness;
forming a first InGaN film comprising the steps of:
supplying a first gallium raw material, a first indium raw material, and a first nitrogen raw material to a reactor to deposit a first InGaN for forming the first InGaN film at a first temperature, the first InGaN having a thickness thinner than the first thickness;
heat-treating the first InGaN at a second temperature higher than the first temperature in the reactor, while supplying a second indium raw material and a second nitrogen raw material to the reactor; and
after the heat treatment, depositing a second InGaN at least once to form the first InGaN film.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the second indium raw material is an organic metal material.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the second nitrogen raw material comprises at least one of ammonia and amines.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the first InGaN film includes one of a well layer and a barrier layer of the active layer.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the first InGaN film includes a well layer of the active layer, and depositing the second InGaN comprises repeating the deposition of InGaN and the heat-treating thereof alternately until the formation of the first InGaN film is completed.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the first InGaN film includes a well layer of the active layer, and a molar fraction of indium of the first InGaN film ranges from 0.25 to 0.35.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the first InGaN film includes a barrier layer of the active layer, and a molar fraction of indium of the first InGaN film ranges from 0.02 to 0.08.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising the steps of:
forming a second InGaN film for the active layer, the second InGaN film having a second thickness, one of the first and second InGaN films being formed on another of the first and second InGaN films,
forming a second InGaN film comprising the steps of:
supplying a third gallium raw material, a third indium raw material, and a third nitrogen raw material to the reactor to deposit a third InGaN for forming the second InGaN film at a third temperature, the third InGaN having a thickness thinner than the second thickness;
heat-treating the third InGaN at a fourth temperature higher than the third temperature, while supplying a fourth indium raw material and a fourth nitrogen raw material to the reactor; and
performing the deposition of a fourth InGaN and the heat treatment of the fourth InGaN at least once until the deposition of the second InGaN film is completed, to form the second InGaN film;
wherein one of the first and second InGaN films is formed for a well layer of the active layer, and another of the first and second InGaN films is formed for a barrier layer of the active layer.

### Claim 9 (depends on 1)

The method according to claim 1, further comprising:
preparing a wafer of a hexagonal crystalline material, an angle formed between the primary surface of the wafer and a c-plane of the hexagonal crystalline material ranges from 15 degrees to 30 degrees.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the first InGaN film is formed for the well layer of the active layer at the first temperature ranging from 630° C. to 780° C.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising:
preparing a wafer of a hexagonal crystalline material, wherein the primary surface of the wafer is a polar plane of the hexagonal crystalline material.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the first InGaN film is formed for the well layer of the active layer at the first temperature ranging from 680° C. to 830° C.

### Claim 13 (depends on 1)

The method according to claim 1, further comprising:
preparing a wafer of a hexagonal crystalline material, wherein the primary surface of the wafer is a nonpolar plane of the hexagonal crystalline material.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the first InGaN film is formed for the well layer of the active layer at the first temperature ranging from 650° C. to 800° C.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the active layer has a quantum well structure and provides a full width not exceeding 40 nm at the half maximum in a photoluminescence spectrum of the active layer.

### Claim 16 (depends on 1)

The method according to claim 1, wherein a laser emission wavelength of the group III nitride semiconductor laser is equal to or longer than 490 nm.

### Claim 17

A method of making an epitaxial wafer for a nitride semiconductor laser comprising the steps of:
forming a first conductivity type gallium nitride based semiconductor region on a wafer;
after forming the first conductivity type gallium nitride based semiconductor region, forming an InGaN film for an active layer on the wafer, the InGaN film having a first thickness; and
after forming the active layer, forming a second conductivity type gallium nitride based semiconductor region;
forming an InGaN film comprising the steps of:
supplying a first gallium raw material, a first indium raw material and a first nitrogen raw material to a reactor to deposit a first InGaN for the InGaN film at a first temperature, the first InGaN having a thickness thinner than the first thickness;
heat-treating the first InGaN at a second temperature higher than the first temperature, while supplying a second indium raw material and a second nitrogen raw material to the reactor; and
after the heat treatment, depositing a second InGaN at least once to form the InGaN film.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the InGaN film includes a well layer of the active layer, and depositing a second InGaN comprises repeating the deposition and the heat treatment of InGaN alternately until the deposition of the InGaN film having the first thickness is completed.

### Claim 19

A group III nitride semiconductor laser comprising:
a first conductivity type group III nitride semiconductor layer;
a second conductivity type of group III nitride semiconductor layer; and
an active layer having multiple InxGa1-xN well layers and plural barrier layers, the active layer being provided between the first conductivity type group III nitride semiconductor layer and the second conductivity type group III nitride semiconductor layer, a molar ratio x of indium of the InxGa1-xN well layer is equal to or more than 0.24; and
wherein a distribution of indium content in the InxGa1-xN well layers has a maximum and a minimum, and the maximum and the minimum reside within a range from −15% to +15% of an average of the indium content in the well layers.

### Claim 20 (depends on 19)

The group III nitride semiconductor laser according to claim 19, wherein each well layer comprises a plurality of InxGa1-xN thin films, and the plurality of InxGa1-xN thin films have the substantially same indium content.