# US 2009/0268512 A1 · MRAM with cross-tie magnetization configuration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0268512 A1
- Document ID: US20090268512A1
- Status: Published application
- Kind: A1
- Application number: 12/150,241
- Filed: 2008-04-25
- Published: 2009-10-29
- Earliest claimed: 2008-04-25
- Assignees: MagIC Technologies, Inc.
- Inventors: Tai Min; David Heim
- Web page: https://patentgrep.com/patent/US20090268512A1

## CPC

- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- G11C 11/1675: {Writing or programming circuits or methods}
- H01F 10/325: {the spacer being noble metal}
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- Y10S 977/935: Spin dependent tunnel, SDT, junction, e.g. tunneling magnetoresistance, TMR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The incidence of half-select errors during MRAM programming has been significantly reduced by giving the free layer a shape that approximates an X so that, when the free layer switches, the magnetization in the arms of the X guides the magnetization in the central section (the X's intersection area) causing it to rotate towards the hard axis in two opposing directions. This raises the free layer's switching energy barrier, thereby reducing half-select errors.

## Claims

### Claim 1

A magnetically free layer, having a shape comprising:
a central section having an approximately rectangular shape that includes two opposing short sides that each have a width, two opposing long sides that each have a length, and four corners, from each of which there extends, in a direction that is approximately parallel to a diagonal of said central section, a branch section;
in proportion to its distance from its originating corner, said branch section optionally tilting towards said short side; and
optionally, one or more additional branch sections that originate at one of said short sides and extend away therefrom, there being no branch sections that originate at one of said long sides.

### Claim 2 (depends on 1)

The magnetically free layer described in claim 1 wherein said magnetically free layer is in contact with a non-magnetic layer which, in turn is in contact with a magnetically pinned reference layer, whereby said magnetically free layer is part of a magneto-resistive device selected from the group consisting of MTJ and GMR devices.

### Claim 3 (depends on 1)

The magnetically free layer described in claim 1 wherein each of said short sides measures between 0.01 and 0.5 microns, each of said long sides measures between 0.01 and 0.5 microns, and one of said long sides is between 1.1 and 5 times as long as one of said short sides.

### Claim 4 (depends on 1)

The magnetically free layer described in claim 1 wherein each of said short sides measures between 0.001 and 1.0 microns, each of said long sides measures between 0.001 and 1.0 microns, and one of said long sides is between 1.1 and 10.0 times as long as one of said short sides.

### Claim 5 (depends on 1)

The magnetically free layer described in claim 1 wherein each of said branch sections has an average width between 0.001 and 0.1 microns, a length between 0.001 and 0.1 microns, and an average length to width ratio of between 1.1 and 3.0.

### Claim 6 (depends on 1)

The magnetically free layer described in claim 1 wherein each of said branch sections has an average width between 0.001 and 0.5 microns, a length between 0.001 and 0.5 microns, and an average length to width ratio of between 0.001 and 0.5.

### Claim 7 (depends on 1)

The magnetically free layer described in claim 1 wherein one or more of said branch sections terminates as a point or as a rounded edge.

### Claim 8 (depends on 1)

The magnetically free layer shape described in claim 1 wherein no axis of symmetry is present.

### Claim 9

A method to reduce errors associated with half-selection in an array of magneto-resistive devices that each include a free layer having a hard axis, comprising:
patterning said free layer into a shape that further comprises: a central section having an approximately rectangular shape that includes two opposing short sides that each have a width, two opposing long sides that each have a length, and four corners, from each of which there extends, in a direction that is approximately parallel to a diagonal of said central section, a branch section;
whereby, when said free layer switches, existing magnetization in said branches serves to guide magnetization in said central section to rotate toward said hard axis in two opposing directions; and
thereby raising said free layer's switching energy barrier and thus reducing said half-selection errors.

### Claim 10 (depends on 9)

The method recited in claim 9 wherein, at a hard axis field of zero, said free layer has an easy axis field that is at least 5 times that of an elliptically shaped free layer whose hard axis field is zero.

### Claim 11 (depends on 9)

The method recited in claim 9 wherein each of said short sides measures between 0.01 and 0.5 microns, each of said long sides measures between 0.01 and 0.5 microns, and one of said long sides is between 1.1 and 3.0 times as long as one of said short sides.

### Claim 12 (depends on 9)

The method recited in claim 9 wherein each of said short sides measures between 0.001 and 1.0 microns, each of said long sides measures between 0.001 and 1.0 microns, and one of said long sides is between 1.1 and 10.0 times as long as one of said short sides.

### Claim 13 (depends on 9)

The method recited in claim 9 wherein each of said branch sections has an average width between 0.001 and 0.1 microns, a length between 0.001 and 0.1 microns, and an average length to width ratio of between 1.1 and 3.0.

### Claim 14 (depends on 9)

The method recited in claim 9 wherein each of said branch sections has an average width between 0.001 and 0.5 microns, a length between 0.001 and 0.5 microns, and an average length to width ratio of between 0.001 and 0.5.

### Claim 15 (depends on 9)

The method recited in claim 9 wherein one or more of said branch sections terminates as a point or as a rounded edge.

### Claim 16 (depends on 9)

The method recited in claim 9 wherein there is no axis of symmetry in said free layer shape.

### Claim 17

A Magnetic Random Access Memory (MRAM), including a magnetically free layer having a shape, comprising:
a plurality of magneto-resistive (MR) devices connected to form an array of rows and columns such that each row intersects each column only once, each of said MR devices further comprising a transition layer disposed to lie between a pinned reference layer and said magnetically free layer;
said magnetically free layer further comprising:
a central section having an approximately rectangular shape that includes two opposing short sides that each have a width, two opposing long sides that each have a length, and four corners, from each of which there extends, in a direction that is approximately parallel to a diagonal of said central section, a branch section;
in proportion to its distance from its originating corner, said branch section optionally tilting towards said short side; and
optionally, one or more additional branch sections that originate at one of said short sides and extend away therefrom, there being no branch sections that originate at one of said long sides.

### Claim 18 (depends on 17)

The MRAM described in claim 17 wherein said MR device is selected from the group consisting of MTJ and GMR devices.

### Claim 19 (depends on 17)

The MRAM described in claim 17 wherein each of said short sides measures between 0.01 and 0.5 microns, each of said long sides measures between 0.01 and 0.5 microns, and one of said long sides is between 1.1 and 5 times as long as one of said short sides.

### Claim 20 (depends on 17)

The MRAM described in claim 17 wherein each of said short sides measures between 0.001 and 1.0 microns, each of said long sides measures between 0.001 and 1.0 microns, and one of said long sides is between 1.1 and 10.0 times as long as one of said short sides.

### Claim 21 (depends on 17)

The MRAM described in claim 17 1 wherein one or more of said branch sections terminates as a point or as a rounded edge.

### Claim 22 (depends on 17)

The MRAM described in claim 17 wherein no axis of symmetry is present in said magnetically free layer shape.