# US 2009/0267260 A1 · Method of producing polymer film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0267260 A1
- Document ID: US20090267260A1
- Status: Published application
- Kind: A1
- Application number: 12/088,244
- Filed: 2006-09-26
- Published: 2009-10-29
- Earliest claimed: 2005-09-28
- Assignees: FUJIFILM Corporation
- Inventors: Naoki Nakamura
- Web page: https://patentgrep.com/patent/US20090267260A1

## CPC

- B29C 41/28: by depositing flowable material on an endless belt
- B29K 2001/00: Use of cellulose, modified cellulose or cellulose derivatives, e.g. viscose, as moulding material
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A casting dope (27) is cast onto a running casting belt (46) to form a casting film (69). Drying devices are disposed in both surface side of the casting belt (46), so as to dry the casting film (69). The casting film (69) is conveyed through drying zones in which drying temperatures are respectively determined according to the content of remaining solvent in the casting film (69) on the basis of the graph of film production limit line that is different between the main compound of the solvent. Then the drive conditions of each drying device were set, such that the drying of the casting film (69) might be made at the drying temperature. Thus the drying temperatures are previously determined adequately to the content of remaining solvent. Therefore, the drying of the casting film can be made without a large luck of supply with the thermal energy, and the like.

## Claims

### Claim 1

A producing method of a polymer film comprising steps of:
casting onto a casting surface of a endlessly running support a dope containing a polymer and a solvent, so as to form a casting film;
feeding out an drying air from an outlet of an air feeding device confronting to said casting surface, said outlet being directed in a running direction of said support;
heating said support by a heating device confronting to a rear surface of said support;
determining setting temperatures of said air feeding device and said heating device according to a content of remaining solvent in said casting film at starting the drying by said air feeding device and said heating device, in reference with a relation between a temperature of said support and said content of remaining solvent;
peeling said casting film as a polymer film from said support; and
drying said polymer film.

### Claim 2 (depends on 1)

A producing method described in claim 1, wherein said setting temperature of said heating device is almost constant in the range of 40° C. to 100° C.

### Claim 3 (depends on 2)

A producing method described in claim 2, wherein said air feeding device and said heating device are respectively plural, and said setting temperature of each of said air feeding devices and said heating devices is adjusted independently.

### Claim 4 (depends on 1)

A producing method described in claim 1,
wherein a main solvent compound of said solvent is dichloromethane, and
wherein when a content of remaining dichloromethane in said casting film is W (mass %), the setting temperature of said air feeding device and said heating device is set such that the temperature T (° C.) of said support may satisfy a condition (I):
T≦4.5×10−4×W2−0.25×W+61. (I)

### Claim 5 (depends on 1)

A producing method described in claim 1,
wherein a main solvent compound of said solvent is methyl acetate, and
wherein when a content of remaining methyl acetate in said casting film is W (mass %), the setting temperature of said air feeding device and said heating device is set such that the temperature T (° C.) of said support may satisfy a condition (II):
T≦6.6×10−4×W2−0.4×W+87 (II)

### Claim 6 (depends on 1)

A producing method described in claim 1, wherein the peeling of said casting film is performed when said content of remaining solvent decreases to at most a predetermine value.