# US 2009/0267184 A1 · Metal-insulator-metal (mim) capacitor structure and methods of fabricating same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0267184 A1
- Document ID: US20090267184A1
- Status: Published application
- Kind: A1
- Application number: 12/257,582
- Filed: 2008-10-24
- Published: 2009-10-29
- Earliest claimed: 2001-10-09
- Assignees: NXP B.V.; Koninklijke Philips Electronics N.V.
- Inventors: Michael Olewine; Kevin Saiz
- Web page: https://patentgrep.com/patent/US20090267184A1

## CPC

- H10D 1/692: {Electrodes}
- H10D 86/85: characterised by only passive components
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/496: {Capacitor integral with wiring layers}
- H10W 20/039: {also covering sidewalls of the conductive structures}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A Metal-Insulator-Metal (MIM) capacitor structure and method of fabricating the same in an integrated circuit improve capacitance density in a MIM capacitor structure by utilizing a sidewall spacer extending along a channel defined between a pair of legs that define portions of the MIM capacitor structure. Each of the legs includes top and bottom electrodes and an insulator layer interposed therebetween, as well as a sidewall that faces the channel. The sidewall spacer incorporates a conductive layer and an insulator layer interposed between the conductive layer and the sidewall of one of the legs, and the conductive layer of the sidewall spacer is physically separated from the top electrode of the MIM capacitor structure. In addition, the bottom electrode of a MIM capacitor structure may be ammonia plasma treated prior to deposition of an insulator layer thereover to reduce oxidation of the electrode. Furthermore, a multi-rate etching process may be used to etch the top electrode and insulator layer of an MIM structure, using a first, higher rate to perform an anisotropic etch up to a point proximate an interface between the conductive and dielectric materials respectively defining the top electrode and insulator layer of the MIM structure, and then using a second, lower rate to perform an anisotropic etch to a point proximate an etch stop layer defined on the bottom electrode of the MIM structure.

## Claims

### Claim at position 1

1-19. (canceled)

### Claim at position 2

20-29. (canceled)

### Claim at position 3

30-38. (canceled)

### Claim 39

A method of fabricating a metal-insulator-metal (MIM) capacitor structure in an integrated circuit, the method comprising ammonia plasma treating a surface of a bottom electrode of the MIM capacitor structure prior to depositing an insulator layer over the bottom electrode to improve the surface barrier characteristic to oxygen.

### Claim 40 (depends on 39)

The method of claim 39, wherein the bottom electrode comprises titanium nitride disposed at the surface of the bottom electrode.

### Claim 41 (depends on 40)

The method of claim 40, wherein the insulator layer comprises tantalum pentoxide.

### Claim 42 (depends on 40)

The method of claim 40, wherein ammonia plasma treating comprises bombarding the titanium nitride surface with nitrogen ions to inhibit oxidation of the titanium nitride surface.

### Claim 43 (depends on 40)

The method of claim 40, wherein ammonia plasma treating is performed in a plasma enhanced chemical vapor deposition tool.

### Claim 44 (depends on 43)

The method of claim 43, wherein ammonia plasma treating is performed in an atmosphere comprising ammonia and an inert gas.

### Claim 45 (depends on 44)

The method of claim 44, wherein ammonia plasma treating is performed in an atmosphere having a pressure of about 10 milliTorr to about 10 Torr and a bottom electrode temperature of about 300 to about 500 EC.

### Claim 46 (depends on 43)

The method of claim 43, wherein ammonia plasma treating includes applying RF power including up to about 50% low frequency RF power.

### Claim 47

A metal-insulator-metal (MIM) capacitor structure for use in an integrated circuit, the MIM capacitor structure comprising:
(a) top and bottom electrodes, wherein the bottom electrode includes an ammonia plasma treated surface; and
(b) an insulator layer interposed between the top electrode and the ammonia plasma treated surface of the bottom electrode.

### Claim 48 (depends on 47)

The MIM capacitor structure of claim 47, wherein the ammonia plasma treated surface comprises titanium nitride.

### Claim 49 (depends on 48)

The MIM capacitor structure of claim 48, wherein the insulator layer comprises tantalum pentoxide.

### Claim 50 (depends on 48)

The MIM capacitor structure of claim 48, wherein the ammonia plasma treated surface is substantially free of titanium oxide as a result of bombardment of the ammonia plasma treated surface with nitrogen ions.

### Claim at position 16

51-62. (canceled)