# US 2009/0267118 A1 · Method for forming carbon silicon alloy (csa) and structures thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0267118 A1
- Document ID: US20090267118A1
- Status: Published application
- Kind: A1
- Application number: 12/111,377
- Filed: 2008-04-29
- Published: 2009-10-29
- Earliest claimed: 2008-04-29
- Assignees: International Business Machines Corporation
- Inventors: Ashima B. Chakravarti; Abhishek Dube; Rainer Loesing; Dominic J. Schepis
- Web page: https://patentgrep.com/patent/US20090267118A1

## CPC

- H10P 14/3408: {Silicon carbide}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/27: {using selective deposition, e.g. simultaneous growth of monocrystalline and non-monocrystalline semiconductor materials}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods for forming carbon silicon alloy (CSA) and structures thereof are disclosed. The method provides improvement in substitutionality and deposition rate of carbon in epitaxially grown carbon silicon alloy layers (i.e., substituted carbon in Si lattice). In one embodiment of the disclosed method, a carbon silicon alloy layer is epitaxially grown on a substrate at an intermediate temperature with a silicon precursor, a carbon (C) precursor in the presence of an etchant and a trace amount of germanium material (e.g., germane (GeH4)). The intermediate temperature increases the percentage of substitutional carbon in epitaxially grown CSA layer and avoids any tendency for silicon carbide to form. The presence of the trace amount of germanium material, of approximately less than 1% to approximately 5%, in the resulting epitaxial layer, has an effect of stabilizing and enhancing deposition/growth rate without compromising the tensile stress of CSA layer formed thereby.

## Claims

### Claim 1

A method for forming a carbon silicon alloy (CSA) layer on a substrate, the method comprising:
depositing a carbon silicon alloy layer on a silicon portion of the substrate, the depositing including mixing a silicon (Si) precursor, a carbon (C) precursor and a germanium material (Ge) in a carrier gas; and
etching any carbon silicon alloy material formed on any non-silicon portion of the substrate with an etchant.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the Si precursor, C precursor and germanium material (Ge) includes a proportional relationship of 5000(Si):100(C):1(Ge).

### Claim 3 (depends on 1)

The method according to claim 1, wherein the germanium material includes germane or methylgermane (MeGeH3).

### Claim 4 (depends on 3)

The method according to claim 3, wherein the germanium material ranges from approximately 0.02% by volume to approximately 0.05% by volume.

### Claim 5 (depends on 1)

The method according to claim 1, further comprising annealing the substrate in the presence of hydrogen before the depositing.

### Claim 6 (depends on 5)

The method according to claim 5, further comprising cooling the substrate to a temperature ranging from approximately 550° C. to approximately 700° C.

### Claim 7 (depends on 6)

The method according to claim 6, further comprising cooling the substrate to a temperature ranging from approximately 600° C. to approximately 650° C.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the silicon precursor includes silicon tetrachloride (SiCl4), trichlorosilane (SiHCl3), dichlorosilane (SiH2Cl2), silane (SiH4), or disilane (Si2H6).

### Claim 9 (depends on 1)

The method according to claim 1, wherein the carbon (C) precursor is an organo silane material including methyl silane and ethylene.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the etchant includes chlorine and hydrogen chloride.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising repeating the depositing and the etching.

### Claim 12 (depends on 1)

The method according to claim 1, furthering comprising doping the carbon silicon alloy layer with arsenic and phosphorous to form a phosphorous arsenic junction therein.

### Claim 13

A semiconductor structure comprising:
a carbon silicon alloy layer disposed on a substrate, the carbon silicon alloy layer including: substitutional carbon (C) incorporated in a silicon (Si) lattice; and approximately less than 1% to approximately 5% of germanium (Ge) therein.

### Claim 14 (depends on 13)

The structure of claim 13, wherein the carbon silicon alloy is an epitaxial fill in a recess in a silicon portion of the substrate, the carbon silicon alloy has a proportional relationship of 5000(Si):100(C):1(Ge).

### Claim 15 (depends on 14)

The structure of claim 14, wherein the epitaxial fill in the recess forms a source-drain region for a gate conductor.

### Claim 16 (depends on 13)

The structure of claim 13, wherein the carbon silicon alloy layer is a continuous layer free of crystalline dislocations.

### Claim 17 (depends on 16)

The structure of claim 16, wherein the carbon silicon alloy further includes a phosphorous-arsenic junction.

### Claim 18

A semiconductor structure comprising:
a gate disposed on a substrate, the substrate including a source-drain region below the gate, wherein the source-drain region includes a carbon silicon alloy (CSA) layer with approximately less than 1% to approximately 5% germanium (Ge) incorporated therein.

### Claim 19 (depends on 18)

The structure of claim 18, wherein the carbon silicon alloy includes a proportional relationship of 5000(Si):100(C):1 (Ge).

### Claim 20 (depends on 19)

The structure of claim 19, wherein the carbon silicon alloy layer includes a phosphorous-arsenic junction therein.