# US 2009/0267064 A1 · Semiconductor thin film and method for manufacturing same, and thin film transistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0267064 A1
- Document ID: US20090267064A1
- Status: Published application
- Kind: A1
- Application number: 12/093,827
- Filed: 2006-10-16
- Published: 2009-10-29
- Earliest claimed: 2005-11-18
- Assignees: Idemitsu Kosan Co., Ltd.
- Inventors: Koki Yano; Kazuyoshi Inoue; Nobuo Tanaka; Tokie Tanaka
- Web page: https://patentgrep.com/patent/US20090267064A1

## CPC

- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- C01G 19/00: Compounds of tin
- C01P 2006/40: Electric properties
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The present invention provides a semiconductor thin film which can be manufactured at a relatively low temperature even on a flexible resin substrate. As a semiconductor thin film having a low carrier concentration, a high Hall mobility and a large energy band gap, an amorphous film containing zinc oxide and tin oxide is formed to obtain a carrier density of 10+17 cm−3 or less, a Hall mobility of 2 cm2/V·sec or higher, and an energy band gap of 2.4 eV or more. Then, the amorphous film is oxidized to form a transparent semiconductor thin film 40.

## Claims

### Claim 1

A semiconductor thin film made by an amorphous film containing zinc oxide, and tin oxide and whose specific resistance is 10 Ωm to 107 Ωm.

### Claim 2 (depends on 1)

The semiconductor thin film according to claim 1, wherein the film is a non-degenerate semiconductor thin film having a carrier density of 10+17 cm−3 or less, a Hall mobility of 2 cm2/V·sec or higher, and an energy band gap of 2.4 eV or more.

### Claim 3 (depends on 1)

The semiconductor thin film according to claim 1, wherein atom ratio between zinc [Zn] and tin [Sn] in the amorphous film is expressed as Zn/(Zn+Sn)=0.40 to 0.95.

### Claim 4 (depends on 1)

The semiconductor thin film according to claim 1, wherein transmittance of wavelength of 550 nm is 75% or higher.

### Claim 5 (depends on 1)

A transparent oxide semiconductor thin film according to claim 1, wherein work function is 3.5 to 6.5 eV.

### Claim 6

A method of manufacturing a semiconductor thin film, comprising:
a step of forming an amorphous film containing zinc oxide and tin oxide by physical film forming method; and
a step of performing a post process in which temperature in a film surface in the presence of oxygen becomes a temperature equal to or higher than a substrate temperature at the time of the film formation.

### Claim 7 (depends on 1)

A thin film transistor comprising the semiconductor thin film according to claim 1.