# US 2009/0267029 A1 · Indium-oxide-based transparent conductive film and method for producing the film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0267029 A1
- Document ID: US20090267029A1
- Status: Published application
- Kind: A1
- Application number: 11/886,071
- Filed: 2007-04-02
- Published: 2009-10-29
- Earliest claimed: 2006-03-31
- Assignees: Mitsui Mining & Smelting Co., Ltd.
- Inventors: Seichiro Takahashi; Norihiko Miyashita
- Web page: https://patentgrep.com/patent/US20090267029A1

## CPC

- C23C 14/086: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C04B 35/453: based on zinc, tin, or bismuth oxides or solid solutions thereof with other oxides, e.g. zincates, stannates or bismuthates
- C04B 35/457: based on tin oxides or stannates
- C04B 35/62685: {characterised by the order of addition of constituents or additives}
- C04B 35/638: Removal thereof
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- H01B 1/08: oxides
- C04B 2235/3215: Barium oxides or oxide-forming salts thereof
- C04B 2235/3284: Zinc oxides, zincates, cadmium oxides, cadmiates, mercury oxides, mercurates or oxide forming salts thereof
- C04B 2235/3286: Gallium oxides, gallates, indium oxides, indates, thallium oxides, thallates or oxide forming salts thereof, e.g. zinc gallate
- C04B 2235/3293: Tin oxides, stannates or oxide forming salts thereof, e.g. indium tin oxide [ITO]
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/77: Density
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

The invention provides a transparent conductive film which exhibits low resistance and high transmittance, is an amorphous film, can be relatively readily patterned by etching with a weak acid, and can be relatively readily crystallized, and a method for producing the film. The transparent conductive film deposited from a sputtering target containing a sintered oxide including indium oxide, barium, and, in accordance with needs, tin, characterized in that the film contains indium oxide, barium, and, in accordance with needs, tin.

## Claims

### Claim 1

A transparent conductive film deposited from a
sputtering target comprising a sintered oxide including indium oxide, barium, and, in accordance with needs, tin, characterized in that the film comprises indium oxide, barium, and, in accordance with needs, tin.

### Claim 2 (depends on 1)

A transparent conductive film as described in claim 1, which is deposited from a sputtering target containing barium in an amount of 0.00001 mol or more and less than 0.10 mol, with respect to 1 mol of indium.

### Claim 3 (depends on 2)

A transparent conductive film as described in claim 2, which is deposited from a sputtering target containing tin in an amount of 0 to 0.3 mol, with respect to 1 mol of indium.

### Claim 4 (depends on 1)

A transparent conductive film as described in claim 1, which exhibits a resistivity of 1.0×10−4 to 1.0×10−3 Ωcm.

### Claim 5 (depends on 1)

A transparent conductive film as described in claim 1, which has been deposited in an amorphous state.

### Claim 6 (depends on 1)

A transparent conductive film as described in claim 1, which has been deposited in an amorphous state, and, subsequently, crystallized through annealing.

### Claim 7 (depends on 6)

A transparent conductive film as described in claim 6, which has been crystallized through annealing at 100 to 400° C.

### Claim 8 (depends on 6)

A transparent conductive film as described in claim 6, which exhibits, after crystallization through annealing, an average transmittance at a wavelength of 400 to 500 nm of 85% or higher.

### Claim 9 (depends on 1)

A transparent conductive film as described in claim 1, wherein the ratio (y) by mole of tin to indium is (−2.9×10−2 Ln(x)−6.7×10−2) or more and (−2.0×10−1 Ln(x)4.6×10−1) or less, wherein x represents a molar ratio of barium to indium, with the case of y=0 being excluded.

### Claim 10 (depends on 1)

A transparent conductive film as described in claim 1, wherein the ratio (y) by mole of tin to indium is (−2.9×10−2 Ln(x)−6.7×10−2) or more and (−2.0×10−1 Ln(x)−4.6×10−1) or less, and is 0.22 or less, wherein x represents a molar ratio of barium to indium, with the case of y=0 being excluded.

### Claim 11 (depends on 10)

A transparent conductive film as described in claim 10, wherein the ratio (y) by mole of tin to indium is (5.9×10−2 Ln(x)+4.9×−1) or less, wherein x represents a molar ratio of barium to indium.

### Claim 12 (depends on 11)

A transparent conductive film of according to claim 11, wherein the ratio (y) by mole of tin to indium is 0.08 or more, and the ratio (x) by mole of barium to indium is 0.025 or less.

### Claim 13

A method for producing a transparent conductive film which is amorphous and which contains indium oxide, barium, and, in accordance with needs, tin, characterized in that the method comprises depositing a film from a sputtering target comprising a sintered oxide including indium oxide, barium, and, in accordance with needs, tin.

### Claim 14 (depends on 13)

A transparent conductive film production method as described in claim 13, wherein the film is deposited in an amorphous state, and, subsequently, the amorphous film is crystallized through annealing.

### Claim 15 (depends on 14)

A transparent conductive film production method as described in claim 14, wherein the amorphous film is etched with a weakly acidic etchant and, subsequently, crystallized through annealing.

### Claim 16 (depends on 14)

A transparent conductive film production method as described in claim 14, wherein annealing for crystallization is performed at 100 to 400° C.

### Claim 17 (depends on 14)

A transparent conductive film production method as described in claim 14, wherein the transparent conductive film exhibits, after crystallization through annealing, an average transmittance at a wavelength of 400 to 500 nm of 85% or higher.

### Claim 18 (depends on 14)

A transparent conductive film production method as described in claim 14, wherein the transparent conductive film exhibits a resistivity of 1.0×10−4 to 1.0×10−3 Ωcm.

### Claim 19 (depends on 13)

A transparent conductive film production method as described in claim 13, wherein the film is deposited from a sputtering target having a molar ratio (y) of tin to indium of (−2.9×10−2 Ln(x)−6.7×10−2) or more and (−2.0×10−1 Ln(x)−4.6×10−1) or less, wherein x represents a molar ratio of barium to indium, with the case of y=0 being excluded.

### Claim 20 (depends on 13)

A transparent conductive film production method as described in claim 13, wherein the film is deposited from a sputtering target having a molar ratio (y) of tin to indium of (−2.9×10−2 Ln(x)−6.7×10−2) or more and (−2.0×10−1 Ln(x)−4.6×10−1) or less, and 0.22 or less, wherein x represents a molar ratio of barium to indium, with the case of y=0 being excluded.

### Claim 21 (depends on 20)

A transparent conductive film production method as described in claim 20, wherein the film is deposited from a sputtering target having a molar ratio (y) of tin to indium of (5.9×10−2 Ln(x)+4.9×10−1) or less, wherein x represents a molar ratio of barium to indium.

### Claim 22 (depends on 21)

A transparent conductive film production method as described in claim 21, wherein the film is deposited from a sputtering target having a molar ratio (y) of tin to indium of 0.08 or more, and a molar ratio (x) of barium to indium of 0.025 or less.

### Claim 23 (depends on 19)

A transparent conductive film production method as described in claim 19, wherein, from the relationship between oxygen partial pressure for depositing a film and resistivity of the film which has undergone annealing, an oxygen partial pressure which provides annealed film with the lowest resistivity is derived, and film deposition is performed at the derived oxygen partial pressure.