# US 2009/0266801 A1 · Method of laser welding metal plated plates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266801 A1
- Document ID: US20090266801A1
- Status: Published application
- Kind: A1
- Application number: 12/208,953
- Filed: 2008-09-11
- Published: 2009-10-29
- Earliest claimed: 2008-04-24
- Assignees: TOA Industries Co., Ltd.
- Inventors: Yoshihiro Oku; Taichi Shimizu; Kenichi Kawamata
- Web page: https://patentgrep.com/patent/US20090266801A1

## CPC

- B23K 26/32: taking account of the properties of the material involved
- B23K 26/244: Overlap seam welding
- B23K 2101/34: Coated articles {; Surface treated articles}
- B23K 2101/35: {Surface treated articles}
- B23K 2103/04: Steel {or steel} alloys
- B23K 2103/20: Ferrous alloys and aluminium or alloys thereof
- B23K 2103/50: {Inorganic materials other than metals or composite materials}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The invention provides a method of laser welding zinc plated steel plates which surely realizes excellent welding without a melting defect such as blowholes. By irradiating a line on a superposed portion of a lower plate and an upper plate with a first laser beam having a high energy density and a small irradiation region by moving the first laser beam therealong, steel plate portions in the small irradiation region are melted and zinc on the superposed surfaces around the small irradiation region including in the small irradiation region is evaporated and allowed to escape outside. Then, after the irradiation with the first laser beam, the same line is irradiated with a second laser beam having a lower energy density than the first laser beam and a larger irradiation region than the first laser beam by moving the second laser beam therealong to melt steel plate portions in the larger irradiation region, thereby completing weldbonding.

## Claims

### Claim 1

A method of laser welding, comprising:
providing a first metal plated plate and a second metal plated plate each comprising a base metal plate and a metal plating formed on the base metal plate and having a melting point lower than a melting point of the base metal plate;
placing the first metal plated plate on the second metal plated plate so that at least part of the first metal plated plate is superposed on the second metal plated plate such that at least one of the metal platings is disposed between the two base metal plates;
irradiating a superposed portion of the first and second metal plated plates with a first laser beam along a welding line so as to melt the base metal plates and to evaporate the metal plating disposed between the two base metal plates, the first laser beam forming a first irradiation region on the superposed portion in which the base metal plates are melted and having a first energy density so as to evaporate the metal plating disposed between two non-melted base metal plates outside the first irradiation region, and the first irradiation region traveling along the welding line as the superposed portion is irradiated along the welding line; and
irradiating, after the irradiation with the first laser beam, the superposed portion of the first and second metal plated plates with a second laser beam along the welding line so as to melt the base metal plates, the second laser beam forming a second irradiation region on the superposed portion that is larger than the first irradiation region so that the base metal plates are melted in the second irradiation region and having a second energy density that is lower than the first energy density, and the second irradiation region traveling along the welding line as the superposed portion is irradiated along the welding line.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first irradiation region and the second irradiation region form concentric circles.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first energy density is high enough to form a penetration hole penetrating the metal plated plates in the superposed portion by blowing off the melted base metal plates in the first irradiation region with a metal vapor generated by the irradiation with the first laser beam.

### Claim 4 (depends on 3)

The method of claim 3, wherein the irradiation with the second laser beam melts base metal plates at a sidewall of the penetration hole so as to fill the penetration hole.

### Claim 5 (depends on 1)

The method of claim 1, wherein the base metal plates comprise a steel and the metal platings comprise zinc or aluminum.