# US 2009/0266716 A1 · Method of fabricating a bipolar electrode for use in a semi fuel cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266716 A1
- Document ID: US20090266716A1
- Status: Published application
- Kind: A1
- Application number: 12/386,184
- Filed: 2009-04-10
- Published: 2009-10-29
- Earliest claimed: 2004-08-11
- Assignees: The United States of America as represented by the Secretary of the Navy
- Inventors: Charles J. Patrissi; Maria G. Medeiros; Louis G. Carreiro; Steven P. Tucker; Russell R. Bessette; Craig M. Deschenes
- Web page: https://patentgrep.com/patent/US20090266716A1

## CPC

- C25D 3/50: of platinum group metals
- C23C 28/021: {including at least one metal alloy layer}
- C23C 28/023: {only coatings of metal elements only}
- C25D 5/54: Electroplating of non-metallic surfaces (C25D7/12 takes precedence)
- C25D 5/623: {Porosity of the layers}
- H01M 4/8631: {Bipolar electrodes}
- H01M 4/8803: {Supports for the deposition of the catalytic active composition (H01M4/90 takes precedence)}
- Y02E 60/50: Fuel cells
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A bipolar electrode fabricated with a combination of materials that will physically separate the catholyte from the metal anode of the electrode while providing high electrical conductivity between the metal anode and the catalyst cathode. This is accomplished by layering the catalyst cathode over a composite of conductive adhesive and conductive foil that is then affixed to the metal anode.

## Claims

### Claim 1

A method of fabricating a bipolar electrode comprising the steps of:
applying a thin coating of adhesive to a first surface of foil having two surfaces;
curing said adhesive by allowing it to dry;
electrochemically depositing a catalyst on the dry adhesive; and
affixing the second opposite surface of the foil to a metal anode.

### Claim 2 (depends on 1)

The method of claim 1 wherein the adhesive has sufficient cohesive and adhesive strength to maintain the integrity of the bipolar electrode in a low pH, oxidizing environment and has high electrical conductivity.

### Claim 3 (depends on 1)

The method of claim 1 wherein the adhesive is a carbon based screen printing ink.

### Claim 4 (depends on 1)

The method of claim 1 wherein applying the adhesive comprises:
disposing the adhesive over the first surface of the foil;
applying a mesh over the adhesive;
pressing the mesh onto the first surface of the foil; and
removing excess adhesive from the mesh.

### Claim 5 (depends on 3)

The method of claim 3 wherein curing said adhesive by allowing it to dry comprises:
drying the adhesive at room temperature for at least 24 hours; and
heating the adhesive to at least 110° C. for at least one hour.

### Claim 6 (depends on 1)

The method of claim 1 wherein the catalyst is made of a palladium iridium alloy.

### Claim 7 (depends on 6)

The method of claim 6 wherein electrochemically depositing the catalyst on the dry adhesive comprises:
placing the dry adhesive and foil on a solid backing;
clamping an open frame on the dry adhesive and foil to hold the foil in place while at the same time define a geometric area upon which to deposit the catalyst;
exposing the adhesive to a plating electrolyte; and
using a cyclic potential sweep to plate the catalyst to the adhesive.

### Claim 8 (depends on 7)

The method of claim 7 wherein the electrolyte comprises 2 mM PdCl2, 2 mM Na2IrCl6.6H2O, 0.1 M KCl and 0.1 M HCl;

### Claim 9 (depends on 7)

The method of claim 7 wherein the cyclic potential sweep comprises between −0.15 and −0.30 Volts, versus an Ag/AgCl reference electrode at 70° C. at 1 mV/s for 5 to 100 cycles as needed.

### Claim 10 (depends on 1)

The method of claim 1 wherein affixing the second opposite surface of the foil to the metal anode comprises:
cleaning the metal anode to the bare metal with an abrasive;
coating the second opposite surface of the foil with adhesive;
pressing the second opposite surface of the foil together with the metal anode; and
curing the adhesive.

### Claim 11 (depends on 10)

The method of claim 10 wherein coating the second opposite surface of the foil with adhesive further comprises:
applying a mesh over the adhesive so that excess adhesive can be scraped off the foil;
pressing the mesh onto the second opposite surface of the foil; and
scraping off excess adhesive from the mesh.

### Claim 12 (depends on 10)

The method of claim 10 wherein pressing the second opposite surface of the foil together with the metal anode comprises applying a pressing force of 1 to 10 lb/square inch for a period of 1 hour.

### Claim 13 (depends on 10)

The method of claim 10 wherein curing the adhesive comprises heating the adhesive at least 110° C. for at least 1 minutes to effect full cure.