# US 2009/0266714 A1 · Method for Forming Multi-Layer Coating Film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266714 A1
- Document ID: US20090266714A1
- Status: Published application
- Kind: A1
- Application number: 11/887,587
- Filed: 2006-04-07
- Published: 2009-10-29
- Earliest claimed: 2005-04-07
- Inventors: Toshio Kaneko; Satoshi Okamoto; Masanobu Futsuhara; Makoto Doi; Eisaku Okada; Takehiro Nito
- Web page: https://patentgrep.com/patent/US20090266714A1

## CPC

- C25D 13/22: Servicing or operating {apparatus or multistep processes}
- C09D 5/4492: {containing special additives, e.g. grinding agents}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The present invention is to provide a method for forming a multi-layer coating film, which can combine a pre-treating step conducted for a metal substrate, before electrodeposition coating, and an electrodeposition coating step. The method comprises: a step of dipping a material to be coated in an aqueous coating composition comprising (A) a rare earth metal compound, (B) a base resin having a cationic group, and (C) a curing agent, wherein a content of the rare earth metal compound (A) in the aqueous coating composition is limited to specific range; a pre-treating step of applying a voltage of less than 50 V in the aqueous coating composition, wherein the material to be coated is used as a cathode; and an electrodeposition coating of applying a voltage of 50 to 450 V in the aqueous coating composition, wherein the material to be coated is used as a cathode.

## Claims

### Claim 1

A method for forming a multi-layer coating film comprising:
dipping a material to be coated in an aqueous coating composition comprising (A) a rare earth metal compound, (B) a base resin having a cationic group, and (C) a curing agent, wherein a content of the rare earth metal compound (A) in the aqueous coating composition is 0.05 to 10% by weight in terms of rare earth metal, based on the solid content of the coating composition;
a pre-treatment which comprises applying a voltage of less than 50 V in the aqueous coating composition, wherein the material to be coated is used as a cathode; and
an electrodeposition coating of applying a voltage of 50 to 450 V in the aqueous coating composition, wherein the material to be coated is used as a cathode.

### Claim 2 (depends on 1)

The method for forming a multi-layer coating film of claim 1, wherein aqueous coating composition further comprises (D) a copper compound or (E) a zinc compound.

### Claim 3 (depends on 1)

The method for forming a multi-layer coating film of claim 1, wherein, in the pre-treatment, an electrolytic reaction product derived from the rare earth metal compound (A) is present in an amount of not less than 5 mg/m2.

### Claim 4 (depends on 2)

The method for forming a multi-layer coating film of claim 2, wherein, in the pre-treatment, an electrolytic reaction products derived from the rare earth metal compound (A) and the copper compound (D), or an electrolytic reaction products derived from the rare earth metal compound (A) and the zinc compound (E) is present in an amount of not less than 5 mg/m2.

### Claim 5 (depends on 1)

The method for forming a multi-layer coating film of claim 1, wherein, in the pre-treating step, an energizing time is 10 to 300 seconds.

### Claim 6 (depends on 1)

The method for forming a multi-layer coating film of claim 1, wherein, in the electrodeposition coating step, an energizing time is 30 to 300 seconds.

### Claim 7 (depends on 1)

The method for forming a multi-layer coating film of claim 1, wherein the aqueous coating composition has a pH of 5 to 7, and a conductivity of 1500 to 4000 μS/cm.

### Claim 8 (depends on 1)

The method for forming a multi-layer coating film of claim 1, wherein the rare earth metal compound (A) is a compound comprising at least one rare earth metal selected from the group consisting of cerium (Ce), yttrium (Y), neodymium (Nd), praseodymium (Pr) and ytterbium (Yb).

### Claim 9

A multi-layer coating film obtained by a method for forming a multi-layer coating film of which comprises:
dipping a material to be coated in an aqueous coating composition comprising (A) a rare earth metal compound, (B) a base resin having a cationic group, and (C) a curing agent, wherein a content of the rare earth metal compound (A) in the aqueous coating composition is 0.05 to 10% by weight in terms of rare earth metal, based on the solid content of the coating composition;
a pre-treatment which comprises applying a voltage of less than 50 V in the aqueous coating compositions wherein the material to be coated is used as a cathode; and
an electrodeposition coating of applying a voltage of 50 to 450 V in the aqueous coating composition, wherein the material to be coated is used as a cathode.