# US 2009/0266543 A1 · Gelation Inhibiting Retarders for Highly Reactive Calcium Silicate Based Binder Compositions and Methods of Making and Using Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266543 A1
- Document ID: US20090266543A1
- Status: Published application
- Kind: A1
- Application number: 12/110,885
- Filed: 2008-04-28
- Published: 2009-10-29
- Earliest claimed: 2008-04-28
- Assignees: Halliburton Energy Services, Inc.
- Inventors: B. Raghava Reddy; Bryan K. Waugh; Russell M. Fitzgerald
- Web page: https://patentgrep.com/patent/US20090266543A1

## CPC

- C09K 8/467: containing additives for specific purposes
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C09K 8/5045: {containing inorganic compounds}
- C09K 8/5083: {obtained by reactions only involving carbon-to-carbon unsaturated bonds}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method of servicing a wellbore comprising placing in the wellbore a composition comprising a non-API compliant reactive calcium silicate based hydraulic binder and at least one gelation inhibiting retarder, and allowing the composition to set. A method of servicing a wellbore comprising placing in a wellbore a cement composition comprising an industrial waste product selected from the group consisting of Class C Fly ash, cement kiln dust, and combinations thereof and a gelation inhibitor, and allowing the composition to set. A method of controlling the thickening time of a cementitious composition comprising contacting a material having greater than 15 wt. % of tricalcium aluminate and tetracalcium aluminoferrite with a gelation inhibitor comprising a alkylbenzene sulfonic acid, at least one methallyl sulfonic acid monomer; at least one copolymerizable nonionic monomer, and at least one copolymerizable olefinically unsaturated carboxylic acid monomer.

## Claims

### Claim 1

A method of servicing a wellbore comprising:
placing in the wellbore a composition comprising a non-API compliant reactive calcium silicate based hydraulic binder and at least one gelation inhibiting retarder; and
allowing the composition to set.

### Claim 2 (depends on 1)

The method of claim 1 wherein the reactive calcium silicate based hydraulic binder comprises tricalcium aluminate, tetracalcium aluminoferrite, or combinations thereof.

### Claim 3 (depends on 2)

The method of claim 2 wherein the total amount of tricalcium aluminate and tetracalcium aluminoferrite is greater than about 15 wt. % of the highly reactive binder.

### Claim 4 (depends on 2)

The method of claim 2 wherein the ratio of tricalcium aluminate:tetracalcium aluminoferrite is from about 5:1 to about 0.5:1.

### Claim 5 (depends on 1)

The method of claim 1 wherein the reactive calcium silicate based hydraulic binder comprises non-API Class C flyash, cement kiln dust, blast furnace slag, or combinations thereof.

### Claim 6 (depends on 5)

The method of claim 5 wherein the class C flyash has a lime content of greater than about 15 wt. %.

### Claim 7 (depends on 5)

The method of claim 5 wherein the cement kiln dust has an analytical lime content of from about 15 wt. % to about 60 wt. %.

### Claim 8 (depends on 5)

The method of claim 5 wherein the blast furnace slag has a silica content of from about 25 wt. % to about 45 wt. %, an alumina content of from about 7 wt. % to about 20 wt. %, a magnesia content of from about 1 wt. % to about 20 wt. % , and an analytical lime content of from about 30 wt. % to about 50 wt. %.

### Claim 9 (depends on 1)

The method of claim 1 wherein the reactive calcium silicate based hydraulic binder is present in the wellbore servicing composition in an amount of from about 30 wt. % to about 100 wt. % based on the total solid weight of the composition.

### Claim 10 (depends on 1)

The method of claim 1 wherein the gelation inhibiting retarder is present in the wellbore servicing composition in an amount of from about 0.05 wt. % to about 4.0 wt. % based on the total solid weight of the composition.

### Claim 11 (depends on 1)

The method of claim 1 wherein the gelation inhibiting retarder comprises a copolymer having a molecular weight of from about 1,000 Daltons to about 50,000 Daltons.

### Claim 12 (depends on 11)

The method of claim 11 wherein the copolymer comprises least one sulfonated monomer, at least one carboxylated monomer, and at least one nonionic monomer.

### Claim 13 (depends on 11)

The method of claim 11 wherein the copolymer comprises at least two sulfonated monomers, at least one carboxylated monomer, and at least one nonionic monomer.

### Claim 14 (depends on 11)

The method of claim 11 wherein the copolymer comprises at least one allyloxybenzenesulfonic acid monomer having the general chemical structure (I),
wherein R4 is hydrogen or a C1-C6 alkyl; and X is hydrogen, an alkali or alkaline earth metal or ammonium; at least one methallyl sulfonic acid monomer; at least one copolymerizable nonionic monomer; and at least one copolymerizable olefinically unsaturated carboxylic acid monomer.

### Claim 15 (depends on 14)

The method of claim 14 wherein the methallyl sulfonic acid monomer comprises methallyl sulfonic acid, alkali metal salts of methallyl sulfonic acid, alkaline earth metal salts of methallyl sulfonic acid, ammonium salts of methallyl sulfonic acid, or combinations thereof.

### Claim 16 (depends on 14)

The method of claim 14 wherein the copolymerizable nonionic monomer comprises monomers represented by the general chemical structure:
wherein n1 and n2 are independently 0 to 10; R1, R2, R8 and R9 are independently hydrogen, C1-C6 alkyl, or C1-C6 alkyl-substituted aryl; R7 is hydrogen, C1-C6 alkyl, or CO2X, where X is hydrogen, an alkali or alkaline earth metal or C1-C6 alkyl; X1 and X2 are absent or are independently O, C═O, or hydrogen; R3 is absent or is C(═O)R4, OR4, NR5R6, C1-C18 alkyl or hydrogen where R4 is C1-C18 alkyl or hydrogen and R5 and R6 are independently hydrogen, C1-C6 alkyl, or an alkyloxyether or alcohol; and R10 is absent or is C(═O)R11, OR11, NR12R13, C1-C18 alkyl, or hydrogen, where R11 is C1-C18 alkyl or hydrogen, R12 and R13 are independently hydrogen, C1-C6 alkyl, or an alkyloxyether or alcohol.

### Claim 17 (depends on 14)

The method of claim 14 wherein the copolymerizable nonionic monomer comprises C1-C6 alkyl esters of (meth)acrylic acid, the alkali or alkaline earth metal or ammonium salts thereof, acrylamide, C1-C6 alkyl-substituted acrylamides, N-alkyl-substituted acrylamides, N-alkanol-substituted acyrylamides, C1-C6 alkyl esters of unsaturated vinylic acids, C1-C6 alkyl half-esters of unsaturated vinylic acids, C1-C6 alkyl esters of saturated aliphatic monocarboxylic acids, or combinations thereof.

### Claim 18 (depends on 14)

The method of claim 14 wherein the copolymerizable olefinically unsaturated carboxylic acid monomer comprises aliphatic, branched or cyclic, mono- or dicarboxylic acids, alkali metal salts thereof; alkaline earth metal salts thereof; ammonium salts thereof; anhydrides thereof; or combinations thereof.

### Claim 19 (depends on 1)

The method of claim 1 wherein the wellbore servicing composition further comprises non-API compliant Portland cement, API compliant Portland cement, or combinations thereof.

### Claim 20 (depends on 19)

The method of claim 19 wherein the non-API compliant Portland cement is present in an amount of from about 20 wt. % to about 100 wt. % of the total weight of solids in the composition.

### Claim 21 (depends on 19)

The method of claim 19 wherein the API compliant Portland cement is present in an amount of from about 0 wt. % to about 99 wt. % of the total weight of solids in the composition.

### Claim 22 (depends on 1)

The method of claim 1 wherein the wellbore servicing composition further comprises a filler.

### Claim 23 (depends on 22)

The method of claim 22 wherein the filler comprises class F fly ash, sand, silica, or combinations thereof.

### Claim 24 (depends on 22)

The method of claim 22 wherein the filler comprises class F fly ash which is present in an amount of from about 5 wt. % to about 60 wt. % of the total solid weight of the composition.

### Claim 25 (depends on 1)

The method of claim 1 further comprising a set modifier.

### Claim 26 (depends on 1)

The method of claim 1 wherein the wellbore servicing composition has a thickening time of greater than about 1 hour.

### Claim 27 (depends on 1)

The method of claim 1 wherein the wellbore servicing composition has a hydration time of from 0.5 hours to 48 hours.

### Claim 28

A method of servicing a wellbore comprising:
placing in a wellbore a cement composition comprising an industrial waste product selected from the group consisting of Class C Fly ash, cement kiln dust, and combinations thereof and a gelation inhibitor; and
allowing the composition to set.

### Claim 29

A method of servicing a wellbore comprising:
controlling the thickening time of a cementitious composition by contacting a material having greater than 15 wt. % of tricalcium aluminate and tetracalcium aluminoferrite with a gelation inhibitor comprising a alkylbenzene sulfonic acid, at least one methallyl sulfonic acid monomer; at least one copolymerizable nonionic monomer, and at least one copolymerizable olefinically unsaturated carboxylic acid monomer; and
placing the composition in the wellbore and allowing the composition to set.