# US 2009/0266505 A1 · Continuous casting method of steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266505 A1
- Document ID: US20090266505A1
- Status: Published application
- Kind: A1
- Application number: 11/991,437
- Filed: 2006-09-05
- Published: 2009-10-29
- Earliest claimed: 2005-09-05
- Assignees: Nippon Steel Corporation
- Inventors: Toshiaki Mizoguchi; Masanobu Hayakawa; Yoshiaki Suematsu; Akira Mikasa
- Web page: https://patentgrep.com/patent/US20090266505A1

## CPC

- B22D 11/10: Supplying or treating molten metal (B22D41/00 takes precedence)
- B22D 41/50: Pouring-nozzles
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

The present invention provides a continuous casting method of steel preventing alumina and other nonmetallic inclusions becoming causes of slivers and argon bubbles becoming causes of blowholes from being entrained and thereby enabling the production of a cast slab superior in surface and internal quality, that is, one giving an inside bore 21 of an immersion nozzle 21 a horizontal sectional shape of an elliptical shape or oblong shape with a length ratio DL/DS of that long axis DL and short axis DS of 1.2 to 3.8, making a direction of that long axis substantially parallel to a long side direction of the casting mold 3, and making the sliding direction of the sliding nozzle 1 a direction perpendicular to said long axis to supply the molten steel in the casting mold 3. Note that a ratio S1/S0 of a sectional area Si at a smallest sectional area part 23 of the inside bore 21 and a sectional area S0 of a nozzle hole 11 of the sliding nozzle 1 is made 0.5 to 0.95

## Claims

### Claim 1

A continuous casting method of steel supplying molten steel from a sliding nozzle provided at a bottom of a tundish through an immersion nozzle to the inside of a casting mold, said continuous casting method of steel characterized by giving an inside bore of the immersion nozzle a horizontal sectional shape of an elliptical shape having the ratio S1/S0 of 0.5 to 0.9, where S1 is the sectional area of the smallest sectional area part of the inside bore, S0 is the sectional of the bore of the sliding nozzle, and making a length ratio DL/DS of that long axis DL and short axis DS 1.2 to 3.8, making a direction of that long axis substantially parallel to a long side direction of the casting mold, and making the sliding direction of the sliding nozzle a direction perpendicular to said long axis to supply the molten steel in the casting mold.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

A continuous casting method of steel as set forth in claim 1, characterized in that two discharge holes are provided at the two sides of the immersion nozzle in the long axis direction so that the discharge holes of the immersion nozzle discharge molten steel toward the short side direction of the facing casting mold.

### Claim 4 (depends on 1)

A continuous casting method of steel as set forth in claim 1, characterized in that a distance between an outer surface of the short axis side of the immersion nozzle and the inner wall of the long length side of the casting mold is made at least 50 mm.

### Claim 5 (depends on 1)

A continuous casting method of steel as set forth in claim 1, characterized by using an electromagnetic stirring apparatus to impart swirlability to the steel in the casting mold during casting.