# US 2009/0266447 A1 · Optimization of metallurgical properties of a solder joint

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266447 A1
- Document ID: US20090266447A1
- Status: Published application
- Kind: A1
- Application number: 12/111,524
- Filed: 2008-04-29
- Published: 2009-10-29
- Earliest claimed: 2008-04-29
- Assignees: International Business Machines Corporation
- Inventors: JAMES A. BUSBY; MINHUA LU; VALERIE A. OBERSON; ERIC D. PERFECTO; KAMALESH K. SRIVASTAVA; BRIAN R. SUNDLOF; JULIEN SYLVESTRE; RENEE L. WEISMAN
- Web page: https://patentgrep.com/patent/US20090266447A1

## CPC

- B23K 35/262: {Sn as the principal constituent}
- B23K 2101/36: Electric or electronic devices
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

Semiconductor packaging techniques are provided which optimize metallurgical properties of a joint using dissimilar solders. A solder composition for Controlled Collapse Chip Connection processing includes a combination of a tin based lead free solder component designed for a chip and a second solder component designed for a laminate. The total concentration of module Ag after reflow is less than 1.9% by weight. A method of manufacturing a solder component is also provided.

## Claims

### Claim 1

A solder composition for Controlled Collapse Chip Connection processing comprising a combination of a tin based lead free solder component designed for a chip and a second solder component designed for a laminate with a total concentration of module Ag after reflow being less than 1.9% by weight.

### Claim 2 (depends on 1)

The solder composition of claim 1, wherein a volume ratio of the tin based lead free solder component to the second solder component is 2:1.

### Claim 3 (depends on 1)

The solder composition of claim 1, wherein the tin based lead free solder component is Sn(x)Ag, where (x) represents a percentage of Ag, and the second component is one of SAC and SnCu.

### Claim 4 (depends on 3)

The solder composition of claim 3, wherein a component concentration of Ag, X, is at least 0.5% by weight.

### Claim 5 (depends on 3)

The solder composition of claim 3, wherein (x) is lower than 1.8%.

### Claim 6 (depends on 5)

The solder composition of claim 5, wherein a module concentration of Ag is below 1.9% by weight.

### Claim 7 (depends on 5)

The solder composition of claim 5, wherein a module concentration of Ag is greater than 0.33% by weight and the second solder component is SnCu.

### Claim 8 (depends on 3)

The solder composition of claim 3, wherein (x) is zero and the second solder component is of SAC.

### Claim 9 (depends on 1)

The method of claim 1, wherein the tin based lead free solder component contains Cu.

### Claim 10

A solder composition, comprising:
a tin based lead free solder component having an Ag content of 1.8% or less by weight; and
a second solder component comprising one of SAC and SnCu, wherein
a module concentration comprising a join of the tin based lead free solder component and the second solder component is less than 1.9% Ag by weight.

### Claim 11 (depends on 10)

The solder composition of claim 10, wherein a volume ratio of the tin based lead free solder component to the second solder component is 2:1.

### Claim 12 (depends on 10)

The solder composition of claim 10, wherein the tin based lead free solder component is Sn(x)Ag, where (x) represents a percentage of Ag.

### Claim 13 (depends on 12)

The solder composition of claim 12, wherein (x) is at least 0.5%.

### Claim 14 (depends on 12)

The solder composition of claim 12, wherein (x) is less than 1.8%

### Claim 15 (depends on 10)

The solder composition of claim 10, wherein a module concentration of Ag is below 1.9% by weight.

### Claim 16 (depends on 10)

The solder composition of claim 10, wherein a module concentration of Ag is greater than 0.33% by weight.

### Claim 17 (depends on 10)

The solder composition of claim 10, wherein (x) is zero and the second solder component is of SAC.

### Claim 18 (depends on 10)

The method of claim 10, wherein the first tin based lead free solder component also contains Cu

### Claim 19

A method of manufacturing a solder component, comprising:
providing a first tin based lead free solder component on a chip;
providing a second tin based lead free solder component on a laminate;
reflowing the first and second tin based lead free solder components at a predetermined temperature to form an interconnect structure between the chip and the laminate, wherein the reflowing joins the first and second tin based lead free solder components with an Ag module concentration of less than 1.9% by weight after the reflowing.

### Claim 20 (depends on 19)

The method of claim 19, wherein:
the first tin based lead free solder component is one of Sn(x)Ag and SnCu, (x) is 1.8% or less.

### Claim 21 (depends on 19)

The method of claim 19, wherein the second tin based lead free solder component is one of SAC and SnCu.

### Claim 22 (depends on 19)

The method of claim 19, wherein the first tin based lead free solder component also contains Cu.