# US 2009/0266409 A1 · Conductive compositions and processes for use in the manufacture of semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266409 A1
- Document ID: US20090266409A1
- Status: Published application
- Kind: A1
- Application number: 12/422,409
- Filed: 2009-04-13
- Published: 2009-10-29
- Earliest claimed: 2008-04-28
- Assignees: E.I.Du Pont De Nemours and Company
- Inventors: YUELI Wang; ALAN Frederick Carroll
- Web page: https://patentgrep.com/patent/US20090266409A1

## CPC

- H01B 1/16: the conductive material comprising metals or alloys
- H01B 1/22: the conductive material comprising metals or alloys
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 77/211: {for photovoltaic cells}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Embodiments of the invention relate to a silicon semiconductor device, and a conductive paste for use in the front side of a solar cell device.

## Claims

### Claim 1

A thick film conductive composition comprising:
a) electrically conductive powder;
b) two or more additives, wherein the first additive is selected from the group consisting of: (i) bismuth-containing additive and phosphorus-containing additive; (ii) a metal oxide of one or more of bismuth, and phosphorus; (iii) any compound that can generate the metal oxides of (ii) upon firing; and (iv) mixtures thereof; and wherein the second additive is selected from the group consisting of: (i) a metal oxide additive; (ii) a compound that can generate a metal oxide upon firing;
c) one or more glass frits; dispersed in
d) organic medium.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the bismuth-containing additive is selected from the group consisting of: Bi2O3, and bismuth resinate; and wherein the phosphorus-containing additive is selected from the group consisting of: P2O5, phosphorus-containing surfactant, and organic phosphorus.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the first additive is a bismuth-containing additive.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the first additive is 0.05 to 10 wt % of the thick film composition.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the first additive is 0.15 to 0.5 wt % of the thick film composition.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the second additive is 4 to 8 wt % of the thick film composition.

### Claim 7 (depends on 1)

The composition of claim 1, wherein the conductive powder comprises Ag.

### Claim 8 (depends on 1)

The composition of claim 1, wherein the second additive is selected from the group consisting of: (a) a metal wherein said metal is selected from Zn, Gd, Ce, Zr, Ti, Mn, Sn, Ru, Co, Fe, Cu and Cr; (b) a metal oxide of one or more of the metals selected from Zn, Gd, Ce, Zr, Ti, Mn, Sn, Ru, Co, Fe, Cu and Cr; (c) any compounds that can generate the metal oxides of (b) upon firing; and (d) mixtures thereof.

### Claim 9 (depends on 8)

The composition of claim 8, wherein the Zn-containing additive is ZnO.

### Claim 10 (depends on 1)

The composition of claim 1, wherein the Ag is 70 to 99 wt % of the total solid components of the thick film composition.

### Claim 11 (depends on 1)

A method of manufacturing a semiconductor device comprising the steps of:
(a) providing one or more semiconductor substrates, one or more insulating films, and the thick film composition of claim 1;
(b) applying the insulating film to the semiconductor substrate,
(c) applying the thick film composition to the insulating film on the semiconductor substrate, and
(d) firing the semiconductor, insulating film and thick film composition, wherein, upon firing, the organic vehicle is removed, the silver and glass frits are sintered, and the insulating film is penetrated by components of the thick film composition.

### Claim 12 (depends on 11)

The method of claim 11, wherein the insulating film comprises one or more components selected from: titanium oxide, silicon nitride, SiNx:H, silicon oxide, and silicon oxide/titanium oxide.

### Claim 13 (depends on 11)

A semiconductor device made by the method of claim 11.

### Claim 14 (depends on 1)

A semiconductor device comprising an electrode, wherein the electrode, prior to firing, comprises the composition of claim 1.

### Claim 15 (depends on 14)

A solar cell comprising the semiconductor device of claim 14.