# US 2009/0266202 A1 · Method for manufacturing metal nanoparticle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266202 A1
- Document ID: US20090266202A1
- Status: Published application
- Kind: A1
- Application number: 11/622,332
- Filed: 2007-01-11
- Published: 2009-10-29
- Earliest claimed: 2006-07-28
- Assignees: National Taiwan University
- Inventors: Yi-Der Tai; Yao-Hsuan Wang; Ming-Hui Chang
- Web page: https://patentgrep.com/patent/US20090266202A1

## CPC

- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- Y10S 977/896: Chemical synthesis, e.g. chemical bonding or breaking
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for manufacturing a metal nanoparticle is provided. The method includes steps of: a) providing a metal salt solution, b) providing a reducing agent, c) providing a protecting agent, d) providing an alkaline solution, e) mixing the salt solution, the reducing agent, the protecting agent and the alkaline solution to form a slurry within a high-gravity field, and f) separating the metal nanoparticle from the slurry.

## Claims

### Claim at position 1

1-27. (canceled)

### Claim 28

A method for generating a metal nanoparticle, comprising steps of:
a) mixing a metal salt solution, an additive and a first alkaline solution having a pH greater than 11.5 within a first high-gravity field to form a first dispersed slurry;
b) mixing the first dispersed slurry with a second alkaline solution with a pH greater than 11.5 with a second high-gravity field to form a second dispersed slurry; and
c) separating the metal nanoparticle from the slurry.

### Claim 29 (depends on 28)

A method as claimed in claim 28 wherein each of the first and second high-gravity fields is ranged from 1 g to 1000 g and provided by centrifugation.

### Claim 30 (depends on 29)

A method as claimed in claim 29, wherein each of the first and second high-gravity fields is ranged from 700 g to 1000 g.

### Claim 31 (depends on 28)

A method as claimed in claim 28, wherein the additive comprises a reducing agent and a protecting agent.

### Claim 32

A method for manufacturing a metal nanoparticle, comprising steps of:
a) providing a metal salt solution;
b) providing a reducing agent;
c) providing a protecting agent;
d) providing an alkaline solution;
e) mixing the salt solution, the reducing agent, the protecting agent and the alkaline solution to form a slurry within a high-gravity field ranged from 700 g to 1000 g and provided by a centrifugation; and
f) separating the metal nanoparticle from the slurry.

### Claim 33

A method for forming a metal nanoparticle, comprising steps of:
a) mixing a metal salt solution, an additive and an alkaline solution having a pH greater than 11.5 within a high-gravity field ranged from 700 g to 1000 g and provided by a centrifugation to form a slurry; and
b) separating the metal nanoparticle from the slurry.