# US 2009/0266111 A1 · Method of Producing Glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0266111 A1
- Document ID: US20090266111A1
- Status: Published application
- Kind: A1
- Application number: 12/084,857
- Filed: 2006-11-13
- Published: 2009-10-29
- Earliest claimed: 2005-11-15
- Assignees: Nippon Sheet Glass Co., Ltd.; NH Techno Glass Corporation
- Inventors: Yukihito Nagashima; Kengo Maeda
- Web page: https://patentgrep.com/patent/US20090266111A1

## CPC

- C03B 1/00: Preparing the batches (chemical compositions C03C)
- C03C 1/004: {Refining agents (refining C03B5/225)}
- C03C 3/091: containing aluminium
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Provided is a method of producing a glass, including, in order to obtain an excellent refining effect: preparing a raw glass batch including: an antimony compound containing pentavalent antimony; and an oxidizing agent (a cerium oxide, a sulfate, a nitrate); and melting the raw glass batch. In preparing the raw glass batch, it is preferable that the antimony compound be premixed with the oxidizing agent. When the nitrate is used as the oxidizing agent, the raw glass batch is prepared so as to include the antimony compound in an amount of more than 0.5 parts by mass and at most 3 parts by mass, in terms of an amount of antimony pentoxide, per 100 parts by mass of a base glass composition expressed in terms of an amount of an oxide.

## Claims

### Claim 1

A method of producing a glass, comprising:
preparing a raw glass batch comprising: an antimony compound containing pentavalent antimony; and at least one oxidizing agent selected from the group consisting of a nitrate, a sulfate and a cerium oxide; and
melting the raw glass batch,
wherein the raw glass batch is prepared by mixing a mixture obtained by mixing the antimony compound and the oxidizing agent with the remainder of the raw glass batch.

### Claim 2 (depends on 1)

The method of producing a glass according to claim 1,
wherein the raw glass batch comprises the antimony compound containing pentavalent antimony in an amount of more than 0.5 parts by mass and at most 3 parts by mass, in terms of an amount of antimony pentoxide, per 100 parts by mass of a base glass composition expressed in terms of an amount of an oxide,
where the base glass composition expressed in terms of an amount of an oxide is a composition of the raw glass batch in terms of an amount of an oxide, excluding an amount of an oxide that serves as a refining agent or an oxidizing agent.

### Claim 3 (depends on 1)

The method of producing a glass according to claim 1,
wherein the raw glass batch is prepared, as a base glass composition expressed in terms of an amount of an oxide, so as to substantially have a composition of, expressed in mass percentage:
45 to 70% of SiO2;
7.5 to 25% of Al2O3;
4 to 17.5% of B2O3;
0 to 10% of MgO;
0 to 10% of CaO;
0 to 10% of SrO;
0 to 30% of BaO;
5 to 30% of MgO+CaO+SrO+BaO;
0 to 5% of ZnO;
0 to 5% of TiO2;
0 to 5% of ZrO2;
0 to 1% of Cl2; and
0 to 0.5% of SO3,
where the base glass composition expressed in terms of an amount of an oxide is a composition of the raw glass batch in terms of an amount of an oxide, excluding an amount of an oxide that serves as a refining agent or an oxidizing agent.

### Claim 4 (depends on 1)

The method of producing a glass according to claim 1,
wherein the raw glass batch is prepared so as to obtain a glass having a strain point higher than 575° C., and a thermal expansion coefficient in the range from 28×10−7/° C. to 46×10−7/° C.

### Claim 5 (depends on 1)

The method of producing a glass according to claim 1,
wherein the raw glass batch is prepared such that a temperature at which a viscosity of a molten material of the raw glass batch is 102dPa·sec is equal to or higher than 1615° C., and so as to obtain a glass having a strain point higher than 630° C.

### Claim 6 (depends on 1)

The method of producing a glass according to claim 1,
wherein the raw glass batch further comprises a tin oxide.

### Claim 7

A method of producing a glass, comprising:
preparing a raw glass batch comprising: an antimony compound containing pentavalent antimony; and a nitrate; and
melting the raw glass batch,
wherein the raw glass batch comprises the antimony compound in an amount of more than 0.5 parts by mass and at most 3 parts by mass, in terms of an amount of antimony pentoxide, per 100 parts by mass of a base glass composition expressed in terms of an amount of an oxide,
where the base glass composition expressed in terms of an amount of an oxide is a composition of the raw glass batch in terms of an amount of an oxide, excluding an amount of an oxide that serves as a refining agent or an oxidizing agent.

### Claim 8 (depends on 7)

The method of producing a glass according to claim 7,
wherein the raw glass batch comprises the antimony compound in an amount of more than 0.7 parts by mass and at most 3 parts by mass, in terms of an amount of antimony pentoxide, per 100 parts by mass of the base glass composition expressed in terms of an amount of an oxide.

### Claim 9

The method of producing a glass according to claim, 8,
wherein the raw glass batch comprises the antimony compound in an amount of more than 1.5 parts by mass and at most 3 parts by mass, in terms of an amount of antimony pentoxide, per 100 parts by mass of the base glass composition expressed in terms of an amount of an oxide.

### Claim 10 (depends on 7)

The method of producing a glass according to claim 7,
wherein the nitrate is an alkaline earth metal nitrate.

### Claim 11 (depends on 7)

The method of producing a glass according to claim 7,
wherein the raw glass batch comprises the nitrate in an amount from 7.5 to 25 parts by mass, per 100 parts by mass of the base glass composition expressed in terms of an amount of an oxide.

### Claim 12 (depends on 7)

The method of producing a glass according to claim 7,
wherein the raw glass batch is prepared, as the base glass composition expressed in terms of an amount of an oxide, so as to substantially have a composition of, expressed in mass percentage:
45 to 70% of SiO2;
7.5 to 25% of Al2O3;
4 to 17.5% of B2O3;
0 to 10% of MgO;
0 to 10% of CaO;
0 to 10% of SrO;
0 to 30% of BaO;
5 to 30% of MgO+CaO+SrO+BaO;
0 to 5% of ZnO;
0 to 5% of TiO2;
0 to 5% of ZrO2;
0 to 1% of Cl2; and
0 to 0.5% of SO3.

### Claim 13 (depends on 7)

The method of producing a glass according to claim 7,
wherein the raw glass batch is prepared so as to obtain a glass having a strain point higher than 575° C., and a thermal expansion coefficient in the range from 28×10−7/° C. to 46×10−7/° C.

### Claim 14 (depends on 7)

The method of producing a glass according to claim 7,
wherein the raw glass batch is prepared such that a temperature at which a viscosity of a molten material of the raw glass batch is 102dPa·sec is equal to or higher than 1615° C., and so as to obtain a glass having a strain point higher than 630° C.

### Claim 15 (depends on 7)

The method of producing a glass according to claim 7,
wherein the raw glass batch further comprises a tin oxide.

### Claim 16

A method of producing a glass, comprising:
preparing a raw glass batch comprising: an antimony compound containing pentavalent antimony; and a cerium oxide and/or a sulfate; and
melting the raw glass batch.

### Claim 17 (depends on 16)

The method of producing a glass according to claim 16,
wherein the raw glass batch comprises a cerium oxide.

### Claim 18 (depends on 17)

The method of producing a glass according to claim 17,
wherein the raw glass batch comprises the cerium oxide in an amount from 0.1 to 1 parts by mass, per 100 parts by mass of a base glass composition expressed in terms of an amount of an oxide,
where the base glass composition expressed in terms of an amount of an oxide is a composition of the raw glass batch in terms of an amount of an oxide, excluding an amount of an oxide that serves as a refining agent or an oxidizing agent.

### Claim 19 (depends on 16)

The method of producing a glass according to claim 16,
wherein the raw glass batch comprises a sulfate.

### Claim 20 (depends on 19)

The method of producing a glass according to claim 19,
wherein the sulfate is an alkaline earth metal sulfate.

### Claim 21 (depends on 19)

The method of producing a glass according to claim 19,
wherein the raw glass batch comprises the sulfate in an amount from 0.25 to 5 parts by mass, per 100 parts by mass of a base glass composition expressed in terms of an amount of an oxide,
where the base glass composition expressed in terms of an amount of an oxide is a composition of the raw glass batch in terms of an amount of an oxide, excluding an amount of an oxide that serves as a refining agent or an oxidizing agent.

### Claim 22 (depends on 16)

The method of producing a glass according to claim 16,
wherein the raw glass batch comprises the antimony compound containing pentavalent antimony in an amount of more than 0.5 parts by mass and at most 3 parts by mass, in terms of an amount of antimony pentoxide, per 100 parts by mass of a base glass composition expressed in terms of an amount of an oxide,
where the base glass composition expressed in terms of an amount of an oxide is a composition of the raw glass batch in terms of an amount of an oxide, excluding an amount of an oxide that serves as a refining agent or an oxidizing agent.

### Claim 23 (depends on 16)

The method of producing a glass according to claim 16,
wherein the raw glass batch is prepared, as a base glass composition expressed in terms of an amount of an oxide, so as to substantially have a composition of, expressed in mass percentage:
45 to 70% of SiO2;
7.5 to 25% of Al2O3;
4 to 17.5% of B2O3;
0 to 10% of MgO;
0 to 10% of CaO;
0 to 10% of SrO;
0 to 30% of BaO;
5 to 30% of MgO+CaO+SrO+BaO;
0 to 5% of ZnO;
0 to 5% of TiO2;
0 to 5% of ZrO2;
0 to 1% of Cl2; and
0 to 0.5% of SO3,
where the base glass composition expressed in terms of an amount of an oxide is a composition of the raw glass batch in terms of an amount of an oxide, excluding an amount of an oxide that serves as a refining agent or an oxidizing agent.

### Claim 24 (depends on 16)

The method of producing a glass according to claim 16,
wherein the raw glass batch is prepared so as to obtain a glass having a strain point higher than 575° C., and a thermal expansion coefficient in the range from 28×10−7/° C. to 46×10−7/° C.

### Claim 25 (depends on 16)

The method of producing a glass according to claim 16,
wherein the raw glass batch is prepared such that a temperature at which a viscosity of a molten material of the raw glass batch is 102dPa·sec is equal to or higher than 1615° C., and so as to obtain a glass having a strain point higher than 630° C.

### Claim 26 (depends on 16)

The method of producing a glass according to claim 16,
wherein the raw glass batch further comprises a tin oxide.