# US 2009/0265904 A1 · Method for manufacturing boundary acoustic wave device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0265904 A1
- Document ID: US20090265904A1
- Status: Published application
- Kind: A1
- Application number: 12/504,843
- Filed: 2009-07-17
- Published: 2009-10-29
- Earliest claimed: 2007-01-19
- Assignees: Murata Manufacturing Co., Ltd.
- Inventors: Hajime KANDO; Naohiro NODAKE; Masahiko SAEKI; Toshiyuki FUYUTSUME
- Web page: https://patentgrep.com/patent/US20090265904A1

## CPC

- H03H 9/0222: {of interface-acoustic, boundary, pseudo-acoustic or Stonely wave devices}
- H03H 3/08: for the manufacture of resonators or networks using surface acoustic waves
- Y10T 29/42: Piezoelectric device making
- Y10T 29/49005: Acoustic transducer
- Y10T 29/49007: Indicating transducer
- Y10T 29/4908: Acoustic transducer
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for manufacturing a boundary acoustic wave device prevents formation of discontinuous portions in a dielectric film without a significant decrease in the thickness of an IDT when the dielectric film is formed by deposition and without deterioration of electrical characteristics. The method includes the steps of forming an IDT on a piezoelectric substrate, forming a lower dielectric film so as to cover the IDT, conducting a planarizing step so as to smooth the rough surface of the lower dielectric film, and forming an upper dielectric film so as to cover the lower dielectric film of which the rough surface is smoothed.

## Claims

### Claim 1

A method for manufacturing a boundary acoustic wave device comprising the steps of:
forming an IDT on an upper surface of a piezoelectric substrate;
forming a lower dielectric film by deposition so as to cover the IDT;
planarizing to smooth a rough surface of the lower dielectric film; and
forming an upper dielectric film on the lower dielectric film so as to cover the lower dielectric film of which the rough surface are smoothed.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in the planarizing step, a resist layer having a planar upper surface is formed on the lower dielectric film and then uniformly etched from an upper surface of the resist layer, whereby the lower dielectric film is planarized by smoothing the rough surface of the lower dielectric film.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the planarizing step includes polishing the upper surface of the lower dielectric film.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the planarizing step is conducted such that, assuming that a wavelength of a boundary acoustic wave excited by the IDT is denoted by λ, a portion having a distance of about 0.4λ or less between an upper surface of the piezoelectric substrate and the upper surface of the lower dielectric film is disposed in a region where the lower dielectric film is to be positioned on the IDT after the planarizing step.

### Claim 5 (depends on 1)

The method according to claim 1, wherein each of the step of forming the lower dielectric film and the planarizing step is conducted more than once.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the IDT includes a plurality of electrode fingers, and the lower dielectric film is formed to have a thickness that is adjusted so as to prevent creation of elastic discontinuous portions where the lower dielectric film is discontinuous in a propagation direction of a boundary acoustic wave in spaces between the plurality of electrode fingers.

### Claim 7

A method for manufacturing a boundary acoustic wave device comprising the steps of:
forming a thickness-adjusting dielectric film for reducing a difference in thickness between an IDT and a lower dielectric film, on an upper surface of a dielectric substrate;
forming a resist pattern in which a region where the IDT is to be formed is an opening, on the thickness-adjusting dielectric film;
etching the thickness-adjusting dielectric film using the resist pattern as a mask;
forming a metal film for forming the IDT;
forming IDT electrodes by removing the resist film together with the metal film formed on the resist film while leaving the thickness-adjusting dielectric film in spaces between the IDT electrodes;
forming the lower dielectric film by deposition so as to cover a region where the IDT and the thickness-adjusting dielectric film remain;
planarizing to smooth a rough surface of the lower dielectric film; and
forming the upper dielectric film so as to cover the upper surface of the lower dielectric film.

### Claim 8 (depends on 7)

The method according to claim 7, wherein, in the planarizing step, a resist layer having a planar upper surface is formed on the lower dielectric film and then uniformly etched from an upper surface of the resist layer, whereby the lower dielectric film is planarized by smoothing the rough surface of the lower dielectric film.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the planarizing step includes polishing the upper surface of the lower dielectric film.

### Claim 10 (depends on 7)

The method according to claim 7, wherein the planarizing step is conducted such that, assuming that a wavelength of a boundary acoustic wave excited by the IDT is denoted by λ, a portion having a distance of about 0.4λ or less between an upper surface of the piezoelectric substrate and the upper surface of the lower dielectric film is disposed in a region where the lower dielectric film is to be positioned on the IDT after the planarizing step.

### Claim 11 (depends on 7)

The method according to claim 7, wherein each of the step of forming the lower dielectric film and the planarizing step is conducted more than once.

### Claim 12 (depends on 7)

The method according to claim 7, wherein the IDT includes a plurality of electrode fingers, and the lower dielectric film is formed to have a thickness that is adjusted so as to prevent creation of elastic discontinuous portions where the lower dielectric film is discontinuous in a propagation direction of a boundary acoustic wave in spaces between the plurality of electrode fingers.