# US 2009/0265875 A1 · Laminated pulp disposable paint tray

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0265875 A1
- Document ID: US20090265875A1
- Status: Published application
- Kind: A1
- Application number: 12/194,875
- Filed: 2008-08-20
- Published: 2009-10-29
- Earliest claimed: 2007-08-20
- Inventors: Eric Clamp; Jack Terrazas; Jason Lin
- Web page: https://patentgrep.com/patent/US20090265875A1

## CPC

- B44D 3/126: {Paint roller trays}
- Y10T 428/1303: Paper containing [e.g., paperboard, cardboard, fiberboard, etc.]
- B44D: PAINTING OR ARTISTIC DRAWING, NOT OTHERWISE PROVIDED FOR; PRESERVING PAINTINGS; SURFACE TREATMENT TO OBTAIN SPECIAL ARTISTIC SURFACE EFFECTS OR FINISHES (surface treatment in general, see the relevant places, e.g. applying liquids or other fluent materials B05)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Recycled paper pulp is processed to form a rigid paint tray base. The paint tray base is then laminated with a film, which may be fully or partially recyclable and/or biodegradable. The film prevents saturation of the pulp from the paint's moisture, which would damage the integrity of the pulp. Once the painting is completed, the film may be separated from the pulp base. The pulp base may then be discarded with wastepaper or used for compost. The film may be recycled or disposed of with other non-biodegradable waste.

## Claims

### Claim 1

A tray for holding a liquid paint therein, the tray comprising:
a molded pulp portion comprising at least partially recycled paper and water resistant ingredients, the water resistant ingredients including gum resin added to the recycled paper;
a poly film laminate portion comprising a poly film, the poly film having a melting temperature between 350 and 550° and capable of being stretched to between 300 and 500% of its original length;
wherein the molded pulp portion is between about 0.2 mm and 2 mm thick in the planar areas and about twice that thickness in non-planar areas or curved regions; and
wherein the laminate is between about 0.02 and 0.2 mm thick and applied by heat press without glue between the molded pulp portion and the laminate.

### Claim 2 (depends on 1)

The tray of claim 1, wherein the poly film is comprised of a material selected from the group consisting of polyethylene teraphthalate, polypropylene, polyethylene, or nylon.

### Claim 3 (depends on 1)

The tray of claim 1, wherein the laminate is applied by the heated press at a temperature between 150 and 250° for a time of 10 to 60 seconds.

### Claim 4 (depends on 1)

The tray of claim 1, wherein the poly film laminate is at least partially recyclable, at least partially degradable, and constructed of at least 50% recycled raw material.

### Claim 5 (depends on 1)

The tray of claim 1, wherein the laminate is easily removable from the molded pulp portion by a user without the aid of tools.