# US 2009/0264590 A1 · High molecular weight coupled block copolymer compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0264590 A1
- Document ID: US20090264590A1
- Status: Published application
- Kind: A1
- Application number: 12/295,297
- Filed: 2007-04-20
- Published: 2009-10-22
- Earliest claimed: 2006-04-21
- Assignees: Kraton Polymers U.S. LLC
- Inventors: Xavier Daniel Dominique Jean Muyldermans; Emmanuelle Coignoul; Catherine Jeanne Solange Mayenez
- Web page: https://patentgrep.com/patent/US20090264590A1

## CPC

- C08L 53/02: of vinyl-aromatic monomers and conjugated dienes
- C08F 297/044: {using a coupling agent}
- C08L 53/025: {modified}
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

High molecular weight coupled block copolymer composition comprising (a) a linear diblock copolymer (I) represented by the general formula (A-B), having a peak apparent molecular weight of from 200,000 to 300,000, (b) a linear di-armed block copolymer (II), represented by the general formula (A-B)2X, (c) a tri-armed block copolymer (III), represented by the formula (A-B)3X, (d) a more than tri-armed block copolymer (IV), represented by the formula (A-B)n>3X, (e) side polymeric structures (SPS) having a peak apparent molecular weight below the linear diblock copolymer (I), wherein A represents a block of predominantly poly(monovinyl aromatic hydrocarbon) and wherein the poly(monovinyl aromatic hydrocarbon) content is in the range of from 20 to 35 wt %; wherein B represents a block of predominantly poly(conjugated diene); wherein X is the residue of a trifunctional and/or tetrafunctional coupling agent; wherein the block copolymer composition has a weight average molecular weight Mw in the range of from 450,000 to 800,000, and wherein the relative amounts of block copolymers corresponds to: I is from 5 to 15 wt %; II and III together are from 70 to 90 wt %, wherein III is above 10 wt %; IV is below 10 wt % and SPS is less than 10 wt % respectively, relative to the weight of the total block copolymer composition, in which the respective components add up to 100%.

## Claims

### Claim 1

High molecular weight coupled block copolymer composition comprising
(a) a linear diblock copolymer (I) represented by the general formula (A-B), having a peak apparent molecular weight of from 200,000 to 300,000,
(b) a linear di-armed block copolymer (II), represented by the general formula (A-B)2X,
(c) a tri-armed block copolymer (III), represented by the formula (A-B)3X,
(d) a more than tri-armed block copolymer (IV), represented by the formula (A-B)n>3X,
(e) side polymeric structures (SPS) having a peak apparent molecular weight below the linear diblock copolymer (I),
wherein A represents a block of predominantly poly(monovinyl aromatic hydrocarbon) and wherein the poly(monovinyl aromatic hydrocarbon) content is in the range of from 20 to 35 wt %; wherein B represents a block of predominantly poly(conjugated diene); wherein X is the residue of a trifunctional and/or tetrafunctional coupling agent; wherein the block copolymer composition has a weight average molecular weight Mw in the range of from 450,000 to 800,000, and wherein the relative amounts of block copolymers corresponds to: I is from 5 to 15 wt %; II and III together are from 70 to 90 wt %, wherein III is above 10 wt %; IV is below 10 wt % and SPS is less than 10 wt % respectively, relative to the weight of the total block copolymer composition, in which the respective components add up to 100%.

### Claim 2 (depends on 1)

High molecular weight coupled block copolymer compositions according to claim 1, having a weight average molecular weight in the range of from 450,000 to 600,000, while the poly(monovinyl aromatic hydrocarbon) content is in the range of from 28 to 32 wt %.

### Claim 3 (depends on 1)

High molecular weight coupled block copolymer compositions according to claim 1, which comprise: (a) a linear diblock copolymer (I) represented by the general formula (A-B), having a peak apparent molecular weight of from 200,000 to 275,000, and wherein (II), (III) and (TV) have a peak apparent molecular weight of twice, three times, respectively more than three times said peak apparent molecular weight value of (A-B).

### Claim 4 (depends on 1)

High molecular weight coupled block copolymer compositions according to claim 1, wherein the monovinyl aromatic hydrocarbon is pure styrene and the conjugated diene is butadiene, isoprene or mixtures thereof.

### Claim 5 (depends on 1)

High molecular weight coupled block copolymer compositions according to claim 1, wherein the poly(conjugated diene) blocks have been hydrogenated up to a degree of at least 80%.

### Claim 6 (depends on 5)

High molecular weight coupled block copolymer compositions according to the claim 5 wherein the ethylene content of the hydrogenated poly(conjugated diene) blocks is in the range from 50 to 65% by weight (based on the poly(conjugated diene) blocks).

### Claim 7 (depends on 1)

High molecular weight coupled block copolymer compositions according to claim 1, wherein the polymer blocks A have a true molecular weight in the range of from 30,000 to 70,000.

### Claim 8 (depends on 1)

Process for the manufacture of the high molecular weight coupled block copolymer compositions according to claim 1, comprising the preparation of a linear diblock copolymer (I) having a peak apparent molecular weight of from 200,000 to 300,000 and coupling the living diblock copolymer with a tetrafunctional and/or trifunctional silane coupling agent and where said coupling agent is used in an equivalent ratio of Si:Li (representing the active end in the initial block copolymer to be coupled) in the range of from 2:1 to 1:1.

### Claim 9 (depends on 8)

Process according to claim 8 wherein the applied coupling agent is methyl tri(methoxy)silane.

### Claim 10 (depends on 1)

Shaped articles and gels derived from the high molecular weight coupled block copolymer compositions according to claim 1, mixed with extender oils, poly(olefins), poly(monovinyl aromatic) resins, hydrocarbon solvents, or mixtures thereof.