# US 2009/0264586 A1 · Aqueous dispersion of an auto-oxidatively drying polyurethane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0264586 A1
- Document ID: US20090264586A1
- Status: Published application
- Kind: A1
- Application number: 12/300,487
- Filed: 2007-05-11
- Published: 2009-10-22
- Earliest claimed: 2006-05-12
- Assignees: Nuplex Resins B.V.
- Inventors: Dirk Emiel Paula Mestach; Fredericus Cornelis Adrianus Bakx
- Web page: https://patentgrep.com/patent/US20090264586A1

## CPC

- C08G 18/0823: {containing carboxylate salt groups or groups forming them}
- C08G 18/36: Hydroxylated esters of higher fatty acids
- C08G 18/6541: {the low-molecular compounds being compounds of group C08G18/34}
- C08G 18/6547: {the low-molecular compounds being compounds of group C08G18/36 or hydroxylated esters of higher fatty acids of C08G18/38}
- C08G 18/6576: {Compounds of group C08G18/69}
- C08G 18/69: Polymers of conjugated dienes {(hydrogenated polymers of conjugated dienes C08G18/6208)}
- C08G 18/755: {and at least one isocyanate or isothiocyanate group linked to a secondary carbon atom of the cycloaliphatic ring, e.g. isophorone diisocyanate}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A process for the preparation of an aqueous dispersion of an auto-oxidatively drying polyurethane, comprising the steps of: a) forming the auto-oxidatively drying polyurethane by reacting an unsaturated fatty acid esterified polyol, a hydroxyl functional polyalkene having one or more unsaturated bonds in the backbone chain between 2 hydroxyl groups, a polyhydroxy carboxylic acid, a polyisocyanate, and optionally a diol having no polyunsaturation; b)optionally adding a neutralizing agent; and c) dispersing the product of step (a) or (b) in water to form an aqueous dispersion. The invention further relates to aqueous dispersions and coating compositions of an auto-oxidatively drying polyurethane, to hybrid dispersions further comprising a co-binder, preferably an acrylic binder as a co-dispersion, as a molecular hybrid or as a blend and to the use thereof for coating fabrics, plastics, wood, or metal.

## Claims

### Claim 1

A process for the preparation of an aqueous dispersion of an auto-oxidatively drying polyurethane, comprising the steps of:
(a) forming an auto-oxidatively drying polyurethane by reacting:
(i) an unsaturated fatty acid esterified polyol,
(ii) a hydroxyl functional polyalkene having one or more unsaturated bonds in the backbone chain between 2 hydroxyl groups,
(iii) a polyhydroxy carboxylic acid,
(iv) a polyisocyanate, and
(v) optionally a diol having no polyunsaturation;
(b) optionally combining a neutralizing agent and the auto-oxidatively drying polyurethane; and
(c) dispersing the product of step (a) or (b) in water to form an aqueous dispersion.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the aqueous dispersion comprises:
(a) from 20 to 80 wt. % of the auto-oxidatively drying polyurethane, wherein:
(i) a concentration of the unsaturated fatty acid esterified polyol is from 1 to 90 wt %;
(ii) a concentration of the hydroxyl functional polyalkene having one or more unsaturated bonds in the backbone chain between 2 hydroxyl groups is from 1 to 90 wt. %;
(iii) a concentration of the polyhydroxy carboxylic acid is from 1 to 10 wt. %;
(iv) a concentration of the polyisocyanate is from 1 to 40 wt. %; and
(v) a concentration of the diol having no polyunsaturation is from 0 to 30 wt. %;
wherein the amounts of components (i) to (v) add up to 100 wt. %;
(b) optionally from 0.5 to 2.5 wt. % of a neutralizing agent; and
(c) from 20 to 80 wt. % of water;
wherein the amounts of (a), (b) and (c) add up to 100 wt. %.

### Claim 3 (depends on 1)

The process according to claim 1, wherein during step (a), (b), or a combination thereof a solvent having a boiling temperature below 200° C. is added, which is removed by distillation before, during, or after step (c).

### Claim 4 (depends on 1)

The process according to claim 1, wherein essentially no solvent other than water is used.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the unsaturated fatty acid esterified polyol (i) has a number average molecular weight of 1,000 g/mol or more.

### Claim 6 (depends on 1)

The process according to claim 1, wherein the unsaturated fatty acid esterified polyol (i) is an unsaturated fatty acid esterified polyester polyol said polyester polyol being the polycondensation product of at least one unsaturated polyfunctional alcohol and at least one di-functional acid or anhydride thereof.

### Claim 7 (depends on 1)

The process according to claim 1, wherein the auto-oxidatively drying polyurethane has a number average molecular weight of 30,000 g/mol or more.

### Claim 8 (depends on 1)

The process according to claim 1, wherein the hydroxyl functional polyalkene (ii) comprises polyalkadiene diol.

### Claim 9 (depends on 8)

The process according to claim 8, wherein the hydroxyl functional polyalkene (ii) comprises polybutadienediol.

### Claim 10 (depends on 1)

The process according to claim 1, wherein the hydroxyl functional polyalkene (ii)is present in an amount of 2 to 50 wt. % of the combined weight of the hydroxyl functional polyalkene (ii) and the unsaturated fatty acid esterified polyol (i).

### Claim 11 (depends on 1)

The process according to claim 1, wherein the polyhydroxy carboxylic acid (iii) comprises 2,2-dimethylol propionic acid, 2,2-dimethylol butyric acid or 2,2-dimethylol acetic acid.

### Claim 12 (depends on 1)

The process according to claim 1, wherein the auto-oxidatively drying polyurethane formed in step (a) or (b) has a free NCO group content below 3 wt. % on a total solids basis.

### Claim 13 (depends on 1)

The process according to claim 1, wherein the ratio of NCO groups in the polyisocyanate to isocyanate reactive OH groups present in the reaction mixture of step (a) is 1.0 or below.

### Claim 14 (depends on 1)

A process according to claim 1, wherein the product of step (a) or (b) is dispersed without prior chain extension.

### Claim 15 (depends on 1)

An aqueous dispersion of an auto-oxidatively drying polyurethane obtainable by the process according to claim 1.

### Claim 16

An aqueous dispersion of an auto-oxidatively drying polyurethane comprising:
(a) 20 to 80 wt. % of an auto-oxidatively drying polyurethane obtainable by reacting:
(i) 1 to 90 wt. % of an unsaturated fatty acid esterified polyol,
(ii) 1 to 90 wt. % of a hydroxyl functional polyalkene having one or more unsaturated bonds in the backbone chain between 2 hydroxyl groups,
(iii) 1 to 10 wt. % of a polyhydroxy carboxylic acid,
(iv) 1 to 40 wt. % of a polyisocyanate, and
(v) 0 to 30 wt. % of a diol having no polyunsaturation;
wherein the amounts of components (i) to (v) add up to 100 wt. %;
(b) optionally 0.5 to 2.5 wt. % of a neutralizing agent; and
(c) 20 to 80 wt. % of water,
wherein the amounts of (a), (b) and (c) add up to 100 wt. %.

### Claim 17 (depends on 16)

The aqueous dispersion according to claim 16, containing less than 5 wt. % of a solvent other than water.

### Claim 18 (depends on 16)

The aqueous dispersion according to claim 16, further comprising a co-binder.

### Claim 19 (depends on 18)

The aqueous dispersion according to claims 18, wherein the co-binder is combined with the auto-oxidatively drying polyurethane as a co-dispersion, as a molecular hybrids or as a blend.

### Claim 20 (depends on 18)

The aqueous dispersion according to claim 18, wherein the co-binder comprises keto groups, hydrazide groups, or a combination thereof for crosslinking the co-binder, optionally in combination with a separate polyhydrazide crosslinking agent.

### Claim 21 (depends on 16)

The use of the aqueous dispersion according to claims 16 for the manufacture of a coating composition, printing ink composition or adhesive composition.

### Claim 22 (depends on 16)

A coating composition, printing ink composition or adhesive composition, comprising the aqueous dispersion of an auto-oxidatively drying polyurethane according to claim 16.

### Claim 23 (depends on 22)

The use of the coating composition according to claim 22 for coating fabrics, plastics, wood, or metal.

### Claim 24 (depends on 1)

The process according to claim 1, wherein the auto-oxidatively drying polyurethane formed in step (a) or (b) has a free NCO group content below 1 wt. % on a total solids basis.

### Claim 25 (depends on 16)

The aqueous dispersion according to claim 16, containing less than about 2 wt. % of a solvent other than water.

### Claim 26

An aqueous dispersion of an auto-oxidatively drying polyurethane comprising:
(a) 20 to 80 wt. % of an auto-oxidatively drying polyurethane obtainable by reacting:
(i) 10 to 70 wt % of an unsaturated fatty acid esterified polyol,
(ii) 10 to 50 wt % of a hydroxyl functional polyalkene having one or more unsaturated bonds in the backbone chain between 2 hydroxyl groups,
(iii) 1 to 10 wt. % of a polyhydroxy carboxylic acid,
(iv) 1 to 40 wt. % of a polyisocyanate, and
(v) 0 to 30 wt. % of a diol having no polyunsaturation;
wherein the amounts of components (i) to (v) add up to 100 wt. %;
(b) optionally 0.5 to 2.5 wt. % of a neutralizing agent; and
(c) 20 to 80 wt. % of water,
wherein the amounts of (a), (b) and (c) add up to 100 wt. %.

### Claim 27 (depends on 16)

The aqueous dispersion according to claim 16, further comprising an acrylic binder.