# US 2009/0264272 A1 · Method for encapsulating reactive metal hydrides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0264272 A1
- Document ID: US20090264272A1
- Status: Published application
- Kind: A1
- Application number: 12/105,035
- Filed: 2008-04-17
- Published: 2009-10-22
- Earliest claimed: 2008-04-17
- Assignees: Toyota Motor Engineering & Manufacturing North America, Inc.
- Inventors: Rana F. Mohtadi
- Web page: https://patentgrep.com/patent/US20090264272A1

## CPC

- C03C 11/002: {Hollow glass particles}
- C01B 3/0084: Solid storage media characterised by their shape, e.g. porous compacts or hollow particles
- C01B 3/065: by reaction of inorganic compounds with hydrides
- C01B 6/34: Purification; Stabilisation
- Y02E 60/32: Hydrogen storage
- Y02E 60/36: Hydrogen production from non-carbon containing sources, e.g. by water electrolysis
- Y10S 420/90: Hydrogen storage
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A process for encapsulating a metal hydride within a hollow glass sphere is provided. The process includes providing a hollow glass sphere, the hollow glass sphere having a shell enclosing an inner volume. The hollow glass sphere is placed within an enclosed chamber and the chamber is evacuated such that a negative pressure is present therewithin. The hollow glass sphere within the evacuated enclosed chamber is subjected to an external element such that the shell affords for molecules to diffuse therethrough. In some instances, the external element is heat, infrared light and combinations thereof. Thereafter, a metal hydride is provided in the form of a vapor and the evacuated enclosed chamber with the hollow glass sphere is exposed to metal hydride vapor and molecules of the metal hydride diffuse through the shell into the inner volume. Thereafter, the external element is removed from the hollow glass sphere such that diffusion of molecules through the shell is generally prohibited and the metal hydride within the hollow glass sphere is in a dense state.

## Claims

### Claim 1

A process for encapsulating a metal hydride within a hollow glass sphere, the method comprising:
providing a hollow glass sphere, the hollow glass sphere having a shell enclosing an inner volume;
placing the hollow gas sphere into an enclosed chamber;
evacuating the enclosed chamber such that a negative pressure is present within the enclosed chamber;
exposing the hollow glass sphere within the enclosed chamber to an external element such that the shell will allow molecules to diffuse therethrough;
providing a metal hydride in the form of a vapor;
exposing the evacuated enclosed chamber to the metal hydride vapor;
removing the external element from the hollow glass sphere such that diffusion of the metal hydride molecules through the shell of the hollow glass sphere is generally prohibited and any metal hydride within the hollow glass sphere is in a condensed state.

### Claim 2 (depends on 1)

The process of claim 1, wherein the hollow glass sphere is made from metal doped silica based glass.

### Claim 3 (depends on 2)

The process of claim 2, wherein the hollow glass sphere has an average mean diameter between 1 micron and 1 millimeter.

### Claim 4 (depends on 3)

The process of claim 3, wherein the hollow glass sphere has an average mean diameter between 5 and 500 microns.

### Claim 5 (depends on 4)

The process of claim 4, wherein the hollow glass sphere has an average mean diameter between 10 microns and 100 microns.

### Claim 6 (depends on 2)

The process of claim 2, wherein the shell has a thickness between 0.1 to 5 microns.

### Claim 7 (depends on 6)

The process of claim 6, wherein the shell has a thickness between 0.1 to 1 microns.

### Claim 8 (depends on 1)

The process of claim 1, wherein the negative pressure within the enclosed chamber is a vacuum between 10−3 and 10−7 torr.

### Claim 9 (depends on 1)

The process of claim 1, wherein the external element is selected from the group consisting of heat, infrared photons and combinations thereof.

### Claim 10 (depends on 9)

The process of claim 9, wherein the hollow glass sphere is exposed to temperatures between 50 and 600° C.

### Claim 11 (depends on 10)

The process of claim 10, wherein the hollow glass sphere is exposed to temperatures between 300 and 600° C.

### Claim 12 (depends on 1)

The process of claim 1, wherein the hollow glass sphere is exposed to the metal hydride vapor a predetermined amount of time.

### Claim 13 (depends on 1)

The process of claim 1, wherein the condensed metal hydride occupies up to 10% of the inner volume within the hollow glass sphere.

### Claim 14 (depends on 1)

The process of claim 1, wherein the condensed metal hydride occupies generally all of the inner volume within the hollow glass sphere.

### Claim 15 (depends on 1)

The process of claim 1, wherein the vapor of the metal hydride is provided by heating a condensed metal hydride.

### Claim 16

A process for encapsulating a metal hydride within a hollow glass sphere, the method comprising:
providing a plurality of hollow glass spheres, the hollow glass spheres each having a shell enclosing an inner volume;
providing a metal hydride in a condensed state;
placing the hollow gas spheres into a vacuum chamber;
pulling a vacuum of between 10−3 and 10−7 torr on the vacuum chamber;
heating the hollow glass spheres within the vacuum chamber to a temperature of between 50 and 600° C.;
illuminating the hollow glass spheres with an energized infrared light source;
heating the condensed metal hydride to form of a metal hydride vapor;
exposing the hollow glass spheres to the metal hydride vapor for a predetermined amount of time;
cooling the hollow glass spheres that have been exposed to the metal hydride vapor to a temperature below a condensation temperature for the metal hydride; and
de-energizing the infrared light source.