# US 2009/0261331 A1 · Low temperature thin film transistor process, device property, and device stability improvement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0261331 A1
- Document ID: US20090261331A1
- Status: Published application
- Kind: A1
- Application number: 12/425,228
- Filed: 2009-04-16
- Published: 2009-10-22
- Earliest claimed: 2008-04-17
- Assignees: Applied Materials, Inc.
- Inventors: Ya-Tang Yang; Beom Soo Park; Tae Kyung Won; Soo Young Choi; John M. White
- Web page: https://patentgrep.com/patent/US20090261331A1

## CPC

- H10D 30/6739: {Conductor-insulator-semiconductor electrodes}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method and apparatus for forming a thin film transistor is provided. A gate dielectric layer is formed, which may be a bilayer, the first layer deposited at a low rate and the second deposited at a high rate. In some embodiments, the first dielectric layer is a silicon rich silicon nitride layer. An active layer is formed, which may also be a bilayer, the first active layer deposited at a low rate and the second at a high rate. The thin film transistors described herein have superior mobility and stability under stress.

## Claims

### Claim 1

A method of forming a thin film transistor, comprising:
forming a silicon-rich silicon nitride layer over a substrate at a first rate;
forming a silicon nitride layer over the silicon-rich silicon nitride layer at a second rate;
forming a first amorphous silicon layer over the silicon nitride layer at a third rate; and
forming a second amorphous silicon layer over the first amorphous silicon layer at a fourth rate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the second rate is less than the first rate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the third rate is less than the fourth rate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the silicon-rich silicon nitride layer has a silicon to nitrogen ratio greater than about 0.83:1.

### Claim 5 (depends on 1)

The method of claim 1, wherein the silicon-rich silicon nitride layer has a silicon to hydrogen bond content between about 18 atomic percent and about 30 atomic percent.

### Claim 6 (depends on 1)

The method of claim 1, wherein the silicon-rich silicon nitride layer is thicker than the silicon nitride layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second amorphous silicon layer is thicker than the first amorphous silicon layer.

### Claim 8 (depends on 2)

The method of claim 2, wherein the silicon-rich silicon nitride layer has a silicon to nitrogen ratio greater than about 0.83:1.

### Claim 9

A method of forming a thin film transistor, comprising:
forming a silicon-rich silicon nitride layer on a substrate at a first rate to a first thickness;
forming a bottom gate layer comprising metal over the silicon-rich silicon nitride layer;
forming a silicon nitride layer over the bottom gate layer at a second rate to a second thickness;
forming a first amorphous silicon layer over the silicon nitride layer at a third rate to a third thickness;
forming a second amorphous silicon layer over the first amorphous silicon layer at a fourth rate to a fourth thickness;
forming a doped silicon containing layer over the second amorphous silicon layer to a fifth thickness; and
forming a conductive contact layer over the doped silicon containing layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the second rate is less than the first rate and the third rate is less than the fourth rate.

### Claim 11 (depends on 9)

The method of claim 9, wherein the second thickness is less than the first thickness and the third thickness is less than the fourth thickness.

### Claim 12 (depends on 9)

The method of claim 9, wherein the silicon-rich silicon nitride layer and the silicon nitride layer are deposited in the same chamber.

### Claim 13 (depends on 12)

The method of claim 12, wherein the silicon-rich silicon nitride layer has a silicon to nitrogen ratio greater than about 0.83:1.

### Claim 14 (depends on 13)

The method of claim 13, wherein the silicon-rich silicon nitride layer has a silicon to hydrogen bond content between about 18 atomic percent and about 30 atomic percent.

### Claim 15

A thin-film transistor, comprising:
a silicon-rich silicon nitride layer having a first thickness disposed over a substrate;
a silicon nitride layer having a second thickness less than the first thickness disposed over the silicon-rich silicon nitride layer;
a first amorphous silicon layer having a third thickness disposed over the silicon nitride layer;
a second amorphous silicon layer having a fourth thickness disposed over the first amorphous silicon layer;
a doped silicon-containing layer disposed over the second amorphous silicon layer;
a conductive layer disposed over the doped silicon-containing layer; and
a passivation layer disposed over the conductive layer.

### Claim 16 (depends on 15)

The transistor of claim 15, wherein the silicon-rich silicon nitride layer has a refractive index between about 1.92 and about 1.96.

### Claim 17 (depends on 15)

The transistor of claim 15, wherein the silicon-rich silicon nitride layer has a silicon:nitrogen ratio greater than about 0.85:1.

### Claim 18 (depends on 15)

The transistor of claim 15, wherein the silicon-rich silicon nitride layer and the silicon nitride layer are deposited in the same process chamber.

### Claim 19 (depends on 15)

The transistor of claim 15, wherein the content of Si—H bonds in the silicon-rich silicon nitride layer is between about 21 atomic percent and about 27 atomic percent.

### Claim 20 (depends on 15)

The transistor of claim 15, wherein the silicon-rich silicon nitride layer, the silicon nitride layer, the first amorphous silicon layer, and the second amorphous silicon layer are formed at a temperature less than about 250° C.