# US 2009/0261328 A1 · Thin film transistor and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0261328 A1
- Document ID: US20090261328A1
- Status: Published application
- Kind: A1
- Application number: 12/423,123
- Filed: 2009-04-14
- Published: 2009-10-22
- Earliest claimed: 2008-04-18
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Hidekazu MIYAIRI; Koji DAIRIKI; Yuji EGI; Yasuhiro JINBO; Toshiyuki ISA
- Web page: https://patentgrep.com/patent/US20090261328A1

## CPC

- H10D 86/0231: {using masks, e.g. half-tone masks}
- C23C 16/0272: {Deposition of sub-layers, e.g. to promote the adhesion of the main coating}
- C23C 16/24: Deposition of silicon only
- C23C 16/4404: {Coatings or surface treatment on the inside of the reaction chamber or on parts thereof}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6715: {characterised by the doping profiles, e.g. having lightly-doped source or drain extensions}
- H10D 30/6729: {characterised by the electrodes}
- H10D 30/6732: {Bottom-gate only TFTs}
- H10D 30/6745: {Polycrystalline or microcrystalline silicon}
- H10D 30/6746: {Amorphous silicon}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10D 62/40: Crystalline structures
- H10D 86/40: characterised by multiple TFTs
- H10D 86/60: wherein the TFTs are in active matrices
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Disclosed is a thin film transistor which includes, over a substrate having an insulating surface, a gate insulating layer covering a gate electrode; a semiconductor layer which functions as a channel formation region; and a semiconductor layer including an impurity element imparting one conductivity type. The semiconductor layer exists in a state that a plurality of crystalline particles is dispersed in an amorphous silicon and that the crystalline particles have an inverted conical or inverted pyramidal shape. The crystalline particles grow approximately radially in a direction in which the semiconductor layer is deposited. Vertexes of the inverted conical or inverted pyramidal crystal particles are located apart from an interface between the gate insulating layer and the semiconductor layer.

## Claims

### Claim 1

A method for manufacturing a thin film transistor, the method comprising the steps of:
forming a gate electrode over a substrate having an insulating surface;
forming a gate insulating layer over the gate electrode;
exposing the gate insulating layer to a gas containing nitrogen, allowing a concentration of oxygen in the gate insulating layer to be equal to or lower than 5×1018 cm−3 and a concentration of nitrogen in the gate insulating layer to be equal to or higher than 1×1020 cm−3 and equal to or lower than 1×1021 cm−3;
forming a semiconductor layer over the gate insulating layer;
forming source and drain regions over the semiconductor layer wherein the source and drain regions comprises a semiconductor and an impurity imparting one conductivity type to the semiconductor; and
forming source and drain electrodes over the source and drain regions, respectively.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein the gas containing nitrogen is an ammonia gas.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein the gas containing nitrogen is a mixed gas containing an ammonia gas and a hydrogen gas.

### Claim 4 (depends on 1)

The method according to claim 1,
wherein the formation of the semiconductor layer is performed using a mixed gas which comprises a semiconductor material gas and a diluent gas.

### Claim 5 (depends on 1)

The method according to claim 1,
wherein the formation of the semiconductor layer is performed using a mixed gas which comprises a semiconductor material gas and a diluent gas, and
wherein the semiconductor material gas is selected from a silicon hydride gas, a silicon fluoride gas, and a silicon chloride gas.

### Claim 6 (depends on 1)

The method according to claim 1,
wherein the formation of the semiconductor layer is performed using a mixed gas which comprises a semiconductor material gas and a diluent gas, and
wherein the diluent gas is selected from a hydrogen gas, a nitrogen gas, and an ammonia gas.

### Claim 7

A method for manufacturing a thin film transistor, the method comprising the steps of:
forming a gate electrode over a substrate having an insulating surface;
forming a gate insulating layer over the gate electrode in a treatment chamber;
removing the substrate from the treatment chamber;
coating an inner wall of the treatment chamber with silicon nitride;
providing the substrate into the treatment chamber, allowing a concentration of oxygen in the gate insulating layer to be equal to or lower than 5×1018 cm−3 and a concentration of nitrogen in the gate insulating layer to be equal to or higher than 1×1020 cm−3 and equal to or lower than 1×1021 cm−3;
forming a semiconductor layer over the gate insulating layer;
forming source and drain regions over the semiconductor layer wherein the source and drain regions comprises a semiconductor and an impurity imparting one conductivity type to the semiconductor; and
forming source and drain electrodes over the source and drain regions, respectively.

### Claim 8 (depends on 7)

The method according to claim 7 further comprising a step of cleaning the treatment chamber,
wherein the cleaning of the treatment chamber is performed after removing the substrate from the treatment chamber and before providing the substrate into the treatment chamber.

### Claim 9 (depends on 7)

The method according to claim 7 further comprising a step of exposing the gate insulating layer to a gas containing nitrogen.

### Claim 10 (depends on 7)

The method according to claim 7 further comprising a step of exposing the gate insulating layer to an ammonia gas.

### Claim 11 (depends on 7)

The method according to claim 7 further comprising a step of exposing the gate insulating layer to a mixed gas containing an ammonia gas and a hydrogen gas.

### Claim 12 (depends on 7)

The method according to claim 7,
wherein the formation of the semiconductor layer is performed using a mixed gas which comprises a semiconductor material gas and a diluent gas.

### Claim 13 (depends on 7)

The method according to claim 7,
wherein the formation of the semiconductor layer is performed using a mixed gas which comprises a semiconductor material gas and a diluent gas, and
wherein the semiconductor material gas is selected from a silicon hydride gas, a silicon fluoride gas, and a silicon chloride gas.

### Claim 14 (depends on 7)

The method according to claim 7,
wherein the formation of the semiconductor layer is performed using a mixed gas which comprises a semiconductor material gas and a diluent gas, and
wherein the diluent gas is selected from a hydrogen gas, a nitrogen gas, and an ammonia gas.

### Claim 15

A method for manufacturing a thin film transistor, the method comprising the steps of:
forming a gate electrode over a substrate having an insulating surface;
forming a gate insulating layer over the gate electrode;
forming a semiconductor layer over the gate insulating layer by using a mixed gas comprising a semiconductor material gas and a nitrogen-containing gas, wherein a concentration of the nitrogen-containing gas is reduced as the formation of the semiconductor layer proceeds;
forming source and drain regions over the semiconductor layer wherein the source and drain regions comprises a semiconductor and an impurity imparting one conductivity type to the semiconductor; and
forming source and drain electrodes over the source and drain regions, respectively.

### Claim 16 (depends on 15)

The method according to claim 15,
wherein the nitrogen-containing gas is selected from a nitrogen gas and an ammonia gas.

### Claim 17 (depends on 15)

The method according to claim 15,
wherein the mixed gas further comprises a diluent gas.

### Claim 18 (depends on 15)

The method according to claim 15,
wherein the mixed gas further comprises a hydrogen gas.

### Claim 19 (depends on 15)

The method according to claim 15,
wherein the semiconductor material gas is selected from a silicon hydride gas, a silicon fluoride gas, and a silicon chloride gas.

### Claim 20

A thin film transistor comprising:
a gate electrode over a substrate having an insulating surface,
a gate insulating layer over the gate electrode;
a first semiconductor layer on and in contact with the gate insulating layer, the first semiconductor layer has an amorphous structure,
a second semiconductor layer which exists in a state that a plurality of crystalline particles is dispersed in the amorphous structure; and
a third semiconductor layer having the amorphous structure over the second semiconductor layer, the third semiconductor layer being provided with an impurity,
wherein the plurality of crystalline particles have an inverted conical or inverted pyramidal shape whose vertex exists on a side of the substrate.

### Claim 21 (depends on 20)

The thin film transistor according to claim 20,
wherein in the first semiconductor layer, a concentration of oxygen which is measured by secondary ion mass spectrometry is less than or equal to 5×1018 cm−3 and a concentration of nitrogen which is measured by secondary ion mass spectrometry ranges 1×1020 cm−3 to 1×1021 cm−3.

### Claim 22 (depends on 20)

The thin film transistor according to claim 20,
wherein a peak of a concentration of nitrogen in the first semiconductor layer, which is measured by secondary ion mass spectrometry, ranges from 3×1020 cm−3 to 1×1021 cm−3, and
wherein in the first semiconductor layer, the concentration of nitrogen is decreased as a distance from the gate insulating layer is increased.

### Claim 23 (depends on 20)

The thin film transistor according to claim 20,
wherein the vertex exists in a region where a concentration of nitrogen in the first semiconductor layer is greater than or equal to 1×1020 cm−3 and less than or equal to 1×1020 cm−3.

### Claim 24 (depends on 20)

The thin film transistor according to claim 20,
wherein the crystalline particles are a single crystal.

### Claim 25 (depends on 20)

The thin film transistor according to claim 20,
wherein the crystalline particles include a twin crystal.