# US 2009/0261301 A1 · Method for growing silicon single crystal, and silicon wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0261301 A1
- Document ID: US20090261301A1
- Status: Published application
- Kind: A1
- Application number: 12/453,579
- Filed: 2009-05-15
- Published: 2009-10-22
- Earliest claimed: 2005-04-08
- Assignees: Sumco Corporation
- Inventors: Toshiaki Ono; Wataru Sugimura; Masataka Hourai
- Web page: https://patentgrep.com/patent/US20090261301A1

## CPC

- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 29/06: Silicon
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A silicon single crystal is produced by the CZ process by setting a hydrogen partial pressure in an inert atmosphere within a growing apparatus to 40 Pa or more but 400 Pa or less, and by growing a trunk part of the single crystal as a defect-free area free from the Grown-in defects. Therefore, a wafer the whole surface of which is composed of the defect-free area free from the Grown-in defects and which can sufficiently and uniformly form BMD can be easily produced. Such a wafer can be extensively used, since it can significantly reduce generation of characteristic defectives of integrated circuits to be formed thereon and contribute for improving the production yield as a substrate responding to the demand for further miniaturization and higher density of the circuits.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A silicon wafer cut from a single crystal grown by a method for growing a silicon single crystal by the Czochralski process, the method comprising the steps of:
setting hydrogen partial pressure in an inert atmosphere within a growing apparatus to 40 Pa or more and 400 Pa or less; and
growing a trunk part of the single crystal as a defect-free area free from the Grown-in defects.

### Claim 15 (depends on 14)

The silicon wafer according to claim 14, which has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more.

### Claim 16 (depends on 14)

The silicon wafer according to claim 14, which is further subjected to a rapid thermal annealing (RTA) treatment.

### Claim 17 (depends on 14)

The silicon wafer according to claim 14, which is used for a base wafer for SIMOX type substrate.

### Claim 18 (depends on 14)

The silicon wafer according to claim 14, which has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more, and is used for a base wafer for SIMOX type substrate.

### Claim 19 (depends on 14)

The silicon wafer according to claim 14, which is used for an active-layer-side wafer for laminated type SOI substrate.

### Claim 20 (depends on 14)

The silicon wafer according to claim 14, which has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more, and is used for an active-layer-side wafer for laminated type SOI substrate.

### Claim 21

A silicon wafer cut from a single crystal grown by a method for growing a silicon single crystal by the Czochralski process, the method comprising the steps of:
setting hydrogen partial pressure in an inert atmosphere within a growing apparatus to 40 Pa or more and 160 Pa or less; and
growing a trunk part of the single crystal as a vacancy-predominant defect-free area.

### Claim 22

A silicon wafer cut from a single crystal grown by a method for growing a silicon single crystal by the Czochralski process, the method comprising the steps of:
setting hydrogen partial pressure in an inert atmosphere within a growing apparatus to more than 160 Pa and 400 Pa or less; and
growing a trunk part of the single crystal as an interstitial silicon-predominant defect-free area.

### Claim 23 (depends on 21)

The silicon wafer according to claim 21, wherein the grown single crystal has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more.

### Claim 24 (depends on 21)

The silicon wafer according to claim 21, wherein the grown single crystal has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more.

### Claim 25 (depends on 21)

The silicon wafer cut according to claim 21, which is further subjected to a rapid thermal annealing (RTA) treatment.

### Claim 26 (depends on 22)

The silicon wafer cut according to claim 22, which is further subjected to a rapid thermal annealing (RTA) treatment.

### Claim 27 (depends on 21)

The silicon wafer according to claim 21, wherein the wafer is used for a base wafer for SIMOX type substrate.

### Claim 28 (depends on 22)

The silicon wafer according to claim 22, wherein the wafer is used for a base wafer for SIMOX type substrate.

### Claim 29 (depends on 27)

The silicon wafer according to claim 27, wherein the grown single crystal has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more.

### Claim 30 (depends on 28)

The silicon wafer according to claim 28, wherein the grown single crystal has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979).

### Claim 31 (depends on 21)

The silicon wafer according to claim 21, wherein the wafer is used for an active-layer-side wafer for laminated type SOI substrate.

### Claim 32 (depends on 22)

The silicon wafer according to claim 22, wherein the wafer is used for an active-layer-side wafer for laminated type SOI substrate.

### Claim 33 (depends on 31)

The silicon wafer according to claim 31, wherein the grown single crystal grown has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more.

### Claim 34 (depends on 32)

The silicon wafer according to claim 32, wherein the grown single crystal grown has an oxygen concentration of 1.2 1018 atoms/cm3 (ASTM F121, 1979) or more.