# US 2009/0261085 A1 · Pure ar gas shielded welding mig flux-cored wire and mig arc welding method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0261085 A1
- Document ID: US20090261085A1
- Status: Published application
- Kind: A1
- Application number: 12/417,849
- Filed: 2009-04-03
- Published: 2009-10-22
- Earliest claimed: 2008-04-16
- Assignees: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- Inventors: Reiichi SUZUKI; Yu UMEHARA; Toshihiko NAKANO
- Web page: https://patentgrep.com/patent/US20090261085A1

## CPC

- B23K 35/3053: {Fe as the principal constituent}
- B23K 9/173: and of a consumable electrode
- B23K 35/0244: {Powders, particles or spheres; Preforms made therefrom}
- B23K 35/0266: {flux-cored}
- B23K 35/362: Selection of compositions of fluxes (B23K35/365, B23K35/368 take precedence)
- B23K 35/368: Selection of non-metallic compositions of core materials either alone or conjoint with selection of soldering or welding materials
- B23K 35/383: {mainly containing noble gases or nitrogen}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A pure Ar-MIG welding wire for welding steel according to the present invention is formed of a flux-cored wire. The flux-cored wire is formed in the manner that a formation formed by welding a carbon steel hoop into a pipe shape or a seamless pipe is used as an outer sheath, the outer sheath is filled with a flux, and a wire drawing process is performed. The flux accounts for 7 to 27 mass % of the total wire mass. The wire contains graphite in the amount of 0.16 to 2.00 mass % on the basis of the total wire mass and iron powder in the amount of 20 mass % on the basis of the total flux mass. According to the construction, neither expensive metal resource nor a greenhouse effect gas is used, slag and fume generation is inhibited, and a weld joint having a high static tensile strength and fatigue strength can be obtained.

## Claims

### Claim 1

A flux-cored wire to be used for MIG welding using a pure Ar shielding gas and to be formed with a steel outer sheath filled with a flux, the wire comprising in the flux,
graphite: 0.16 to 2.00 mass % on the basis of the total wire mass; and
iron powder: 20 mass % or more on the basis of the total flux mass.

### Claim 2 (depends on 1)

A flux-cored wire as defined in claim 1, further comprising in the flux, at least one element selected from a group of Ti and Zr in an amount of 0.03 to 5.00 mass % on the basis of the total wire mass.

### Claim 3 (depends on 1)

A flux-cored wire as defined in claim 1, further comprising, on the basis of the total wire mass,
C: 0.16 to 2.00 mass %;
Si: 2.00 mass % or less;
Mn: 10.00 mass % or less;
Al: 1.00 mass % or less;
Mg: 1.00 mass % or less;
Ni: 3.00 mass % or less;
Cr: 3.00 mass % or less;
Nb: 3.00 mass % or less;
V: 3.00 mass % or less;
Mo: 3.00 mass % or less;
Cu: 3.00 mass % or less;
B: 0.0200 mass % or less;
rare earth metals (REM): 0.50 mass % or less;
F: 0.50 mass % or less;
Ca:0.50 mass % or less;
K, Na, and Li: at least one element selected from a group of the elements having a total amount of 1.00 mass % or less;
P: 0.030 mass % or less as an impurity; and
S: 0.030 mass % or less as an impurity.

### Claim 4 (depends on 3)

A flux-cored wire as defined in claim 3, wherein, the content of C is 0.45 to 2.00 mass % on the basis of the total wire mass.

### Claim 5 (depends on 1)

A MIG arc welding method, wherein MIG welding is executed in a manner that the flux-cored wire as defined in claim 1 is used, a pure Ar gas conforming to JIS K 1105 Class 1 or 2 is used as a shielding gas, and an arc is generated between the wire set to the positive pole and a base metal set to the negative pole.

### Claim 6 (depends on 5)

A MIG welding method as defined in claim 5, wherein a pulsed power source is used as a power source that forms the arc.

### Claim 7 (depends on 5)

A MIG welding method as defined in claim 5, wherein the base metal is a steel sheet having a tensile strength of 490 MPa or more.