# US 2009/0261068 A1 · Method for selectively removing coatings from metal substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0261068 A1
- Document ID: US20090261068A1
- Status: Published application
- Kind: A1
- Application number: 12/484,704
- Filed: 2009-06-15
- Published: 2009-10-22
- Earliest claimed: 2006-12-07
- Assignees: General Electric Company
- Inventors: Lawrence Bernard Kool; Michael Howard Rucker; David Edwin Budinger
- Web page: https://patentgrep.com/patent/US20090261068A1

## CPC

- C23C 10/18: using liquids, e.g. salt baths, liquid suspensions
- C23C 10/60: After-treatment
- C23F 1/16: Acidic compositions (C23F1/42 takes precedence)
- C23F 1/44: Compositions for etching metallic material from a metallic material substrate of different composition
- C25F 3/14: locally
- C25F 5/00: Electrolytic stripping of metallic layers or coatings
- F01D 5/005: {Repairing methods or devices}
- F05D 2230/11: by electrochemical methods
- F05D 2230/90: Coating; Surface treatment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

A method for selectively removing an aluminum-poor overlay coating from a substrate of a component, which as a result of its low aluminum content is highly resistant to a selective stripping solution. The method entails diffusing aluminum into the overlay coating to form an aluminum-infused overlay coating having an increased aluminum level in at least an outer surface thereof. The diffusion step is carried out so that the increased aluminum level is sufficient to render the aluminum-infused overlay coating removable by selective stripping. The outer surface of the aluminum-infused overlay coating is then contacted with an aqueous composition to remove the aluminum-infused overlay coating from the substrate. The aqueous composition includes at least one acid having the formula HxAF6, and/or precursors thereof, wherein A is Si, Ge, Ti, Zr, Al, and/or Ga, and x is from 1 to 6.

## Claims

### Claim 1

A method of removing an aluminum-containing overlay coating from a substrate of a component, the overlay coating having an aluminum content of less than 12% by weight and being highly resistant to selective stripping, the method comprising:
diffusing aluminum into the overlay coating to form an aluminum-infused overlay coating having an increased aluminum level in at least an outer surface thereof, the increased aluminum level being sufficient to render the aluminum-infused overlay coating removable by selective stripping; and then
prior to subjected the component and the overlay coating thereof to an oxidizing environment, contacting the outer surface of the aluminum-infused overlay coating with an aqueous composition to remove the aluminum-infused overlay coating from the substrate, the aqueous composition containing at least one acid having the formula HxAF6 and/or a precursor thereof, wherein A is selected from the group consisting of Si, Ge, Ti, Zr, Al, and Ga, and x is 1 to 6.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the step of diffusing aluminum into the overlay coating comprises:
applying at least one layer of a slurry to the overlay coating, the slurry being substantially free of hexavalent chromium and comprising colloidal silica and particles of an aluminum-based powder; and then
heat treating the slurry at a temperature in the range of about 650° C. to about 1100° C.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the slurry further comprises at least one organic stabilizer which contains at least two hydroxyl groups.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the slurry is applied to the surface of the overlay coating by a technique selected from one or more of spraying, slip-casting, brush-painting, dipping, pouring, rolling, and spin-coating, and combinations containing at least one of the foregoing.

### Claim 5 (depends on 2)

The method according to claim 2, wherein heat treating the slurry comprises a graduated heat treatment.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the aqueous composition comprises the compound H2SiF6 or H2ZrF6.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the aqueous composition further comprises at least one additional acid and/or a precursor thereof.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the substrate is immersed in a bath of the aqueous composition.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the bath is maintained at a temperature in the range of about room temperature to about 100° C. while the substrate is immersed therein.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the immersion time about 10 minutes to about 72 hours.

### Claim 11 (depends on 8)

The method according to claim 8, further comprising flowing an electric current through the bath of the aqueous composition while the substrate is immersed therein.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the aqueous composition is maintained at a temperature not greater than 100° C. while the substrate is immersed therein.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the substrate is immersed in the aqueous composition for about 1 minute to about 36 hours.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the electric current flows between at least two electrodes disposed in the solution, and the substrate is between the electrodes.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the overlay coating is an MCrAl(X) overlay coating, where M is an element selected from the group consisting of Ni, Co, Fe, and combinations thereof, and X is an element selected from the group consisting of Y, Ta, Si, Hf, Ti, Zr, B, C, and combinations thereof.

### Claim 16

A method of removing an aluminum-containing overlay coating from a substrate of a gas turbine component, the overlay coating having an aluminum content of less than 12% by weight and being highly resistant to selective stripping, the method comprising:
removing the component from a gas turbine after operation of the gas turbine and after growth of a protective alumina scale on an exposed outer surface of the overlay coating;
diffusing aluminum into the overlay coating to form an aluminum-infused overlay coating having an increased aluminum level in at least an outer surface thereof, the increased aluminum level being sufficient to render the aluminum-infused overlay coating removable by selective stripping; and then
contacting the outer surface of the aluminum-infused overlay coating with an aqueous composition to remove the aluminum-infused overlay coating from the substrate, the aqueous composition including at least one of an acid having the formula HxAF6, and precursors to said acid, A being selected from the group consisting of Si, Ge, Ti, Zr, Al, and Ga, and x being 1 to 6.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the metallic material is a superalloy.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the superalloy is nickel-based or cobalt-based superalloy.

### Claim 19 (depends on 16)

The method according to claim 16, wherein the component is not installed on a gas turbine after the diffusing step and before the contacting step.

### Claim 20 (depends on 19)

The method according to claim 19, further comprising:
after the contacting step and removal of the aluminum-infused overlay coating, depositing a second Al-poor overlay coating on the substrate of the component; and then