# US 2009/0261034 A1 · Vinylidene Fluoride Resin Hollow Fiber Porous Membrane and Method for Production Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0261034 A1
- Document ID: US20090261034A1
- Status: Published application
- Kind: A1
- Application number: 11/991,955
- Filed: 2006-09-12
- Published: 2009-10-22
- Earliest claimed: 2005-09-14
- Inventors: Takeo Takahashi; Yasuhiro Tada; Kenichi Suzuki; Masayuki Hino; Toshiya Mizuno
- Web page: https://patentgrep.com/patent/US20090261034A1

## CPC

- B01D 71/34: Polyvinylidene fluoride
- B01D 67/0027: {by stretching}
- B01D 67/0086: {Mechanical after-treatment}
- B01D 69/02: characterised by their properties
- B01D 69/08: Hollow fibre membranes (manufacture of hollow fibres D01D5/24, D01F1/08)
- C02F 1/444: {by ultrafiltration or microfiltration}
- D01D 5/247: Discontinuous hollow structure or microporous structure
- D01F 6/12: from polymers of fluorinated hydrocarbons
- B01D 2313/24: Specific pressurizing or depressurizing means
- B01D 2323/12: Specific ratios of components used
- B01D 2323/20: Plasticizers
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS

## Abstract

A hollow-fiber porous membrane comprising a hollow-fiber form of vinylidene fluoride resin and satisfying the following properties (A) and (B), is provided as a hollow-fiber porous membrane of vinylidene fluoride resin having an average pore size and a further uniform pore size distribution (A) and a large water permeation rate regardless of good efficiency of blocking minute particles (bacteria) (B), as represented by: (A) a ratio Pmax (1 m)/Pm of at most 4.0 between a maximum pore size Pmax (1 m) measured at a test length of 1 m according to the bubble point method and an average pore size Pm of 0.05-0.20 μm measured according to the half dry method; and (B) a ratio F (L=200 mm, v=70%)/PM2 of at least 3000 (m/day·μm2), wherein the ratio F (L=200 mm, v=70%)/Pm2 denotes a ratio between F (L=200 mm, v=70%) which is a value normalized to a porosity v=70% of a water permeation rate F (100 kPa, L=200 mm) measured at a test length L=200 mm under the conditions of a pressure difference of 100 kPa and a water temperature of 25° C. and a square Pm2 of an average pore size Pm. The hollow-fiber porous membrane is produced by a process, comprising: subjecting a stretched hollow-fiber porous membrane of vinylidene fluoride resin to at least two stages of relaxation treatment in a non-wetting environment.

## Claims

### Claim 1

A hollow-fiber porous membrane, comprising a hollow fiber-form porous membrane of vinylidene fluoride resin and satisfying the following properties (A) and (B):
(A) a ratio Pmax (1 m)/Pm of at most 4.0 between a maximum pore size Pmax (1 m) measured at a test length of 1 m according to the bubble point method and an average pore size Pm of 0.05-0.20 μm measured according to the half dry method; and
(B) a ratio F (L=200 mm, v=70%)/Pm2 of at least 3000 (m/day·μm2), wherein the ratio F (L=200 mm, v=70%)/Pm2 denotes a ratio between F (L=200 mm, v=70%) which is a value normalized to a porosity v=70% of a water permeation rate F (100 kPa, L=200 mm) measured at a test length L=200 mm under the conditions of a pressure difference of 100 kPa and a water temperature of 25° C. and a square Pm2 of an average pore size Pm.

### Claim 2 (depends on 1)

A hollow-fiber porous membrane according to claim 1, wherein the ratio Pmax (1 m)/Pm is at most 3.0.

### Claim 3 (depends on 1)

A hollow-fiber porous membrane according to claim 1, wherein the ratio F (L=200 mm, v=70%)/Pm2 is at least 3500 (m/day·μm2).

### Claim 4

A process for producing a hollow-fiber porous membrane of vinylidene fluoride resin, comprising: subjecting a stretched hollow-fiber porous membrane of vinylidene fluoride resin to at least two stages of relaxation treatment in a non-wetting environment.

### Claim 5 (depends on 4)

A production process according to claim 4, wherein the non-wetting environment for the two stages of relaxation treatment comprises water and/or air.

### Claim 6 (depends on 5)

A production process according to claim 5, wherein the water and/or air comprises water at 50-100° C. and/or air or steam at 80-160° C.

### Claim 7 (depends on 5)

A production process according to claim 5, wherein the non-wetting environment for the two stages of relaxation treatment successively comprise water, and air or steam.

### Claim 8 (depends on 4)

A production process according to claim 4, wherein the two stages of relaxation are performed at relaxation percentages of 2-20% for each stage and totally 4-30%.

### Claim 9 (depends on 4)

A production process according to claim 4, wherein the stretched hollow-fiber porous membrane of vinylidene fluoride resin has been formed by melt-extruding into a hollow-fiber film a starting mixture comprising the vinylidene fluoride resin and at least a plasticizer for vinylidene fluoride resin, followed by cooling, extraction of the plasticizer and stretching.

### Claim 10 (depends on 9)