# US 2009/0260726 A1 · High strength aluminum alloy fin material for heat exchanger and method for production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0260726 A1
- Document ID: US20090260726A1
- Status: Published application
- Kind: A1
- Application number: 12/488,032
- Filed: 2009-06-19
- Published: 2009-10-22
- Earliest claimed: 2004-02-03
- Assignees: Nippon Light Metal Company, Ltd.
- Inventors: Yoshito OKI; Hideki SUZUKI; Haruo SUGIYAMA; Toshiya ANAMI; Tomohiro SASAKI
- Web page: https://patentgrep.com/patent/US20090260726A1

## CPC

- F28F 21/084: {from aluminium or aluminium alloys}
- B21B 1/28: by cold-rolling {, e.g. Steckel cold mill}
- B21B 3/00: Rolling materials of special alloys so far as the composition of the alloy requires or permits special rolling methods or sequences {; Rolling of aluminium, copper, zinc or other non-ferrous metals}(altering special metallurgical properties of alloys, other than structure consolidation or mechanical properties resulting therefrom C21D, C22F)
- B22D 11/003: {Aluminium alloys}
- B22D 11/0605: {formed by two belts, e.g. Hazelett-process}
- C22C 21/00: Alloys based on aluminium
- C22C 21/02: with silicon as the next major constituent
- C22C 21/10: with zinc as the next major constituent
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/043: of alloys with silicon as the next major constituent
- C22F 1/053: of alloys with zinc as the next major constituent
- B21B 2003/001: {Aluminium or its alloys}
- F28F: DETAILS OF HEAT-EXCHANGE AND HEAT-TRANSFER APPARATUS, OF GENERAL APPLICATION (water and air traps, air venting F16)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

[PROBLEMS] To provide an aluminum alloy fin material for a heat exchanger, which has high strength and high heat conductivity after brazing, and is excellent in the resistance to sagging, erosion and self-corrosion and the in the sacrificial anode effect. [MEANS FOR SOLVING PROBLEMS] A method for producing an aluminum alloy fin material for a heat exchanger which comprises providing a molten aluminum alloy having a chemical composition, in wt %, that Si: 0.5 to 1.5%, Fe: 0.15 to 1.0%, Mn: 0.8 to 3.0%, Zn: 0.5 to 2.5%, with the proviso that the content of Mg as an impurity is limited to 0.05 wt % or less, and the balance: Al and inevitable impurities, casting the molten alloy continuously into a thin slab having a thickness of 5 to 10 mm by the use of a twin belt casting machine, winding up the slab into a roll, cold-rolling the slab into a sheet having a thickness of 0.05 to 2.0 mm, subjecting the sheet to an inter annealing at 350 to 500° C., and cold-rolling the annealed sheet with a cold reduction rate of 10 to 96%, to prepare a sheet having a final thickness of 40 to 200 μm, and optionally subjecting the final sheet to a final annealing (a softening process) at a holding temperature of 300 to 400° C.

## Claims

### Claim 1

A method of producing a high-strength aluminum alloy fin material for heat exchangers having a tensile strength before brazing of at most 240 MPa and a tensile strength after brazing of 150 MPa or more, comprising:
pouring a melt comprising 0.8-1.4 wt % of Si, 0.15-0.7 wt % of Fe, 1.5-3.0 wt % of Mn and 0.5-2.5 wt % of Zn, further having Mg as an impurity limited to at most 0.05 wt % and the remainder comprising impurities and Al;
continuously casting slabs having a thickness of from 5 to 10 mm and winding the slabs into rolls;
cold rolling to a sheet having a thickness of from 0.05 to 0.4 mm;
inter annealing at a temperature of from 350 to 500° C.; and
cold rolling at a cold reduction rate of from 10 to 50% to a final sheet thickness of from 40 to 200 μm.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said continuously casting occurs at a casting speed of from 5 to 15 m/min.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said inter annealing occurs for a period of from 1 to 5 hours.

### Claim 4 (depends on 1)

The method according to claim 1, wherein a heating rate for said inter annealing is at least 30° C./hr.

### Claim 5 (depends on 1)

The method according to claim 1, further comprising annealing a cold rolled sheet obtained by said cold rolling at a temperature of from 300 to 400° C.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the melt comprises 0.9-1.4 wt % of Si, 0.17-0.6 wt % of Fe, 1.8-3.0 wt % of Mn, and 1.0-1.5 wt % of Zn.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the impurities comprise Cu, Cr, Zr, Ti, and V.

### Claim 8 (depends on 7)

The method according to claim 7, wherein Cu is present in an amount of at most 0.2 wt %.

### Claim 9 (depends on 7)

The method according to claim 7, wherein Cr, Zr, Ti and V are present in an amount of at most 0.20 wt %.

### Claim 10 (depends on 1)

A high-strength aluminum alloy fin material for heat exchangers obtained by the process according to claim 1.

### Claim 11

A method of producing a high-strength aluminum alloy fin material for heat exchangers having a tensile strength before brazing of at most 240 MPa and a tensile strength after brazing of 150 MPa or more, comprising
pouring a melt comprising 0.8-1.4 wt % of Si, 0.15-0.7 wt % of Fe, 1.5-3.0 wt % of Mn and 0.5-2.5 wt % of Zn, further having Mg as an impurity limited to at most 0.05 wt % and the remainder consisting of impurities and Al;
continuously casting thin slabs having a thickness of 5-10 mm and winding the slabs into rolls;
cold rolling to a sheet thickness of 0.08-2.0 mm;
inter annealing at a temperature of 350-500° C.;
cold rolling at a cold reduction rate of 50-96% to a final sheet thickness of 40-200 μm; and
annealing at a temperature of 300-400° C.

### Claim 12 (depends on 11)

The method according to claim 11, wherein said inter anneal at 350-500° C. is performed in a continuous annealing furnace with a heating rate of 100° C./min or more and a holding (retention) time of at most 5 minutes.

### Claim 13 (depends on 11)

The method according to claim 11, wherein said continuously casting occurs at a casting speed of from 5 to 15 m/min.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the melt comprises 0.9-1.4 wt % of Si, 0.17-0.6 wt % of Fe, 1.8-3.0 wt % of Mn, and 1.0-1.5 wt % of Zn.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the impurities comprise Cu, Cr, Zr, Ti, and V.

### Claim 16 (depends on 15)

The method according to claim 15, wherein Cu is present in an amount of at most 0.2 wt %.

### Claim 17 (depends on 15)

The method according to claim 15, wherein Cr, Zr, Ti and V are present in an amount of at most 0.20 wt %.

### Claim 18 (depends on 11)

A high-strength aluminum alloy fin material for heat exchangers obtained by the process according to claim 11.