# US 2009/0258113 A1 · Pellet drying process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0258113 A1
- Document ID: US20090258113A1
- Status: Published application
- Kind: A1
- Application number: 12/102,683
- Filed: 2008-04-14
- Published: 2009-10-15
- Earliest claimed: 2008-04-14
- Assignees: Frito-Lay North America, Inc.
- Inventors: David Brian Emerson; Karoline Marie Kensinger Russell; Thomas Anthony Trezza
- Web page: https://patentgrep.com/patent/US20090258113A1

## CPC

- A23L 7/17: by extrusion
- A23P 30/20: Extruding
- A23P 30/30: Puffing or expanding
- Y10S 426/808: Starch base snack product
- A23L: FOODS, FOODSTUFFS OR NON-ALCOHOLIC BEVERAGES, NOT OTHERWISE PROVIDED FOR; PREPARATION OR TREATMENT THEREOF (preservation thereof A23B)
- A23P: SHAPING OR WORKING OF FOODSTUFFS, NOT FULLY COVERED BY A SINGLE OTHER SUBCLASS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for making an expandable half-product or pellet suitable for cooking by microwave oven (or other method such as frying) that results in a non-uniform, random design, while having a distinct pattern or style. The half product design is achieved by inducing stress cracks in the half product. The stress cracks are created by a controlled drying process whereby extruded half-products are first case hardened to create an outer skin that requires an internal build-up of pressure to penetrate. After creation of the outer skin, by drying in an oven or in ambient air, the half-product is heated to permit the vapor pressure of the moisture inside the half-product to break through the outer skin and escape. Such escape points induce stress cracks in random places in the half-product. The general pattern of the stress cracks can be varied by manipulation of the time-temperature profile of the case hardening and stress cracking steps.

## Claims

### Claim 1

A method of inducing stress cracks in an expandable pellet, said method comprising the steps of:
extruding a dough into a pellet having an outer surface;
case hardening said outer surface with a case-hardening time-temperature profile to create an outer skin; and
cracking said outer skin with a stress cracking time-temperature profile.

### Claim 2 (depends on 1)

The method of claim 1, wherein said case hardening time-temperature profile comprises exposing said pellets to ambient air having a temperature of between about 60° F. and about 100° F. for between about 5 minutes and about 15 minutes.

### Claim 3 (depends on 1)

The method of claim 1, wherein said case hardening time-temperature profile comprises exposing said pellets to a temperature of between about 150° F. and about 200° F. for between about 5 minutes and about 15 minutes.

### Claim 4 (depends on 1)

The method of claim 1, wherein said stress cracking time-temperature profile comprises exposing said pellets to a temperature of between about 200° F. and about 400° F. for between about 30 seconds and about 5 minutes.

### Claim 5 (depends on 1)

The method of claim 1, wherein said stress cracking time-temperature profile comprises exposing said pellets to a temperature of between about 200° F. and about 300° F. for between about 10 minutes and about 60 minutes.

### Claim 6 (depends on 1)

The method of claim 1 wherein said stress cracking occurs concurrently with a drying step, wherein said drying step occurs for between about 30 and about 90 minutes in a multi-zone oven having oven temperatures of between about 120° F. and about 200° F.

### Claim 7

A method for making nonuniform pellets by affecting the moisture release, said method comprising the steps of:
extruding a dough into a pellet having an outer surface;
case hardening said outer surface with a first moisture release rate to create an outer skin; and
cracking said outer skin with a second moisture release rate

### Claim 8 (depends on 7)

The method of claim 7, wherein said first moisture release rate occurs from exposing said pellets to ambient air having a temperature of between about 60° F. and about 100° F. for between about 5 minutes and about 15 minutes.

### Claim 9 (depends on 7)

The method of claim 7, wherein said first moisture release rate occurs from exposing said pellets to a temperature of between about 150° F. and about 200° F. for between about 5 minutes and about 15 minutes.

### Claim 10 (depends on 7)

The method of claim 7, wherein said second moisture release rate occurs from exposing said pellets to a temperature of between about 200° F. and about 400° F. for between about 30 seconds and about 5 minutes.

### Claim 11 (depends on 7)

The method of claim 7, wherein said second moisture release rate occurs exposing said pellets to a temperature of between about 200° F. and about 300° F. for between about 10 minutes and about 60 minutes.

### Claim 12 (depends on 7)

The method of claim 7, wherein a moisture gradient after said case hardening whereby said moisture in said outer skin comprises less than about 4% by weight.