# US 2009/0257153 A1 · Binary output reader structure (BORS) with high utilization rate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0257153 A1
- Document ID: US20090257153A1
- Status: Published application
- Kind: A1
- Application number: 12/082,258
- Filed: 2008-04-10
- Published: 2009-10-15
- Earliest claimed: 2008-04-10
- Assignees: Headway Technologies, Inc.
- Inventors: Yue Liu
- Web page: https://patentgrep.com/patent/US20090257153A1

## CPC

- G11B 5/3909: {Arrangements using a magnetic tunnel junction}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- B82Y 40/00: Manufacture or treatment of nanostructures
- G01R 33/093: {using multilayer structures, e.g. giant magnetoresistance sensors (thin magnetic films H01F10/00)}
- G01R 33/098: {comprising tunnel junctions, e.g. tunnel magnetoresistance sensors}
- G11B 5/3912: {Arrangements in which the active read-out elements are transducing in association with active magnetic shields, e.g. magnetically coupled shields (G11B5/3916 takes precedence)}
- H01F 10/3268: {the exchange coupling being asymmetric, e.g. by use of additional pinning, by using antiferromagnetic or ferromagnetic coupling interface, i.e. so-called spin-valve [SV] structure, e.g. NiFe/Cu/NiFe/FeMn}
- H01F 41/302: {for applying spin-exchange-coupled multilayers, e.g. nanostructured superlattices (spin-exchange-coupled multilayers H01F10/32)}
- H01F 41/32: for applying conductive, insulating or magnetic material on a magnetic film {, specially adapted for a thin magnetic film}
- G11B 2005/3996: {large or giant magnetoresistive effects [GMR], e.g. as generated in spin-valve [SV] devices}
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

We disclose a magnetic read head, and method for making it, that operates in a binary rather than an analog mode. This greatly boosts signal amplitude for high area density recording as device dimensions get smaller. The device is well suited to the inclusion of side shields which further reduces side reading errors. The device has a utilization efficiency close to 100%

## Claims

### Claim 1

A method to form a two state magneto-resistive (MR) device, comprising:
providing a bottom shield, having a lower surface that is on a substrate, and depositing in succession, on said bottom shield, a seed layer, a pinning layer, a pinned layer, a spacer layer, a free layer, and a capping layer, thereby forming a MR complex;
patterning said MR complex to form a MR device stack having a front edge that is normal to said bottom shield and a back edge comprising an upper part that is normal to said bottom shield and a lower part that slopes away from said front edge at an angle;
said upper part comprising said capping and free layers and said lower part comprising said seed layer, said pinned and pinning layers, and said spacer layer;
then lapping said front edge to form an air bearing surface (ABS) whose width defines a track width (TW), and whose distance from said back edge defines a stripe height (SH);
said TW value ranging from 0.9 to 2 times said SH value;
forming a back end that extends away from said back edge over said bottom shield; and
ensuring that said free layer has zero magnetization in a direction parallel to said ABS, whereby, in the presence of an external magnetic field, said MR device has one of only two possible resistance values, giving it a utilization rate of at least 80% and an output signal of at least 56 mV at a full dR/R of about 50% and an applied voltage of about 140 mV.

### Claim 2 (depends on 1)

The method of claim 1 wherein, each time said lapping step is completed, SH may deviate from some pre-specified value by up to 20% without affecting subsequent device performance.

### Claim 3 (depends on 1)

The method of claim 1 further comprising filling said back end with insulation and then forming a top shield that covers said capping layer and said insulation.

### Claim 4 (depends on 1)

The method of claim 1 further comprising:
depositing a first layer of insulation on said back edge;
forming a biasing layer of magnetically hard material on said layer of insulation;
magnetizing said biasing layer in a direction normal to said ABS thereby giving said free layer a vertical bias; and
then forming a top shield that covers said capping layer, said biasing layer, and said layer of insulation.

### Claim 5 (depends on 4)

The method of claim 4 wherein said vertical bias ranges from −200 to +200 Oe whereby said free layer is unaffected by the presence of inter-layer coupling fields up to 200 Oe and by a pinned layer strength of at least 1,000 Oe.

### Claim 6 (depends on 4)

The method of claim 4 wherein said vertical bias ranges from −500 to +500 Oe whereby said free layer is unaffected by the presence of inter-layer coupling fields up to 200 Oe and by a pinned layer strength of at least 1,000 Oe.

### Claim 7 (depends on 1)

The method of claim 1 further comprising:
depositing a first layer of insulation on said back edge;
forming a layer of magnetically soft material on said layer of insulation;
then shaping said soft magnetic layer whereby it functions as a pair of opposing side shields that reduce errors due to side reading.

### Claim 8 (depends on 7)

The method of claim 7 wherein said side shields are in direct magnetic contact with said bottom shield.

### Claim 9 (depends on 7)

The method of claim 7 further comprising:
forming a magnetic layer that covers said capping layer and said insulation and that is in magnetic contact with said side shields; and
then forming a top shield that contacts all of said magnetic layer.

### Claim 10 (depends on 1)

The method of claim 1 wherein said MR device will operate normally with a resistance area product of up to 1.5 ohm.sq. microns for a reader width down to 20 nm.

### Claim 11 (depends on 1)

The method of claim 1 wherein said angle of slope ranges from 45 to 90 degrees.

### Claim 12 (depends on 1)

The method of claim 1 wherein said angle of slope parallels said bottom shield whereby only said free layer is modified when achieving said designed SH, thereby giving said pinned layer a higher aspect ratio and more stable pinning.

### Claim 13 (depends on 4)

The method of claim 4 further comprising shaping said biasing layer whereby it functions as a pair of opposing side shields thereby reducing errors due to side reading.

### Claim 14 (depends on 1)

The method of claim 1 further comprising giving said MR device an aspect ratio in the range of from 1 to 2 thereby providing greater margin when lapping said front edge as well as improving pinning stabilization.

### Claim 15 (depends on 1)

The method of claim 1 further comprising initializing said read head through use of a strong spin torque effect at low RA (resistance area product) and high current density thereby setting said MR device in a pre-selected state.

### Claim 16

A two state magneto-resistive (MR) device, comprising:
a bottom shield, having a lower surface that is on a substrate;
on said bottom shield, a MR complex that comprises a seed layer, a pinning layer, a pinned layer, a spacer layer, a free layer, and a capping layer;
as part of said MR complex, a MR device stack having a front edge that is normal to said bottom shield and a back edge comprising an upper part that is normal to said bottom shield and a lower part that slopes away from said front edge at an angle;
said upper part comprising said capping and free layers and said lower part comprising said seed layer, said pinned and pinning layers, and said spacer layer;
said front edge being an air bearing surface (ABS) whose width defines a track width (TW), and whose distance from said back edge defines a stripe height (SH);
said TW value ranging from 0.9 to 2 times said SH value;
a back end that extends away from said back edge over said bottom shield; and
said free layer having zero magnetization in a direction parallel to said ABS, whereby, in the presence of an external magnetic field, said MR device has one of only two possible resistance values, giving it a utilization rate of at least 80% and an output signal of at least 56 mV at a full dR/R of about 50% and an applied voltage of about 140 mV.

### Claim 17 (depends on 16)

The MR device described in claim 16 further comprising said back end filled with insulation and a top shield covering said capping layer and said insulation.

### Claim 18 (depends on 16)

The MR device described in claim 16 further comprising:
a first layer of insulation on said back edge;
a biasing layer of magnetically hard material on said layer of insulation;
said biasing layer being magnetized in a direction normal to said ABS thereby giving said free layer a vertical bias; and
a top shield that covers said capping layer, said biasing layer, and said layer of insulation.
said vertical bias ranges from −200 to +200 Oe whereby said free layer is unaffected by the presence of inter-layer coupling fields up to 200 Oe and by a pinned layer strength of at least 1,000 Oe.

### Claim 19 (depends on 18)

The MR device described in claim 18 wherein said vertical bias ranges from −200 to +200 Oe whereby said free layer is unaffected by the presence of inter-layer coupling fields up to 200 Oe and by a pinned layer strength of at least 1,000 Oe.

### Claim 20 (depends on 18)

The MR device described in claim 18 wherein said vertical bias ranges from −500 to +500 Oe whereby said free layer is unaffected by the presence of inter-layer coupling fields up to 200 Oe and by a pinned layer strength of at least 1,000 Oe.

### Claim 21 (depends on 16)

The MR device described in claim 16 further comprising:
a first layer of insulation on said back edge;
a layer of magnetically soft material on said layer of insulation;
said soft magnetic layer being shaped to function as a pair of opposing side shields that reduce errors due to side reading.

### Claim 22 (depends on 21)

The MR device described in claim 21 wherein said side shields are in direct magnetic contact with said bottom shield.

### Claim 23 (depends on 21)

The MR device described in claim 21 further comprising:
a magnetic layer that covers said capping layer and said insulation and that is in magnetic contact with said side shields; and
a top shield that contacts all of said magnetic layer.

### Claim 24 (depends on 16)

The MR device described in claim 16 wherein said MR device will operate normally with a resistance area product of up to 1.5 ohm.sq. microns for a reader width down to 20 nm.

### Claim 25 (depends on 16)

The MR device described in claim 16 wherein said angle of slope ranges from 45 to 90 degrees

### Claim 26 (depends on 16)

The MR device described in claim 16 wherein said angle of slope parallels said bottom shield whereby said pinned layer has a higher aspect ratio and more stable pinning.

### Claim 27 (depends on 16)

The MR device described in claim 16 further comprising giving said MR device an aspect ratio in the range of from 1 to 2 whereby said MR device will function effectively for RA values up to 1.5 and reader widths down to 20 nm, thereby increasing its degree of pinning stabilization.