# US 2009/0256272 A1 · Mold Fabrication Method and Projection Optical System Reflection Mirror

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2009/0256272 A1
- Document ID: US20090256272A1
- Status: Published application
- Kind: A1
- Application number: 12/515,406
- Filed: 2007-11-05
- Published: 2009-10-15
- Earliest claimed: 2006-11-21
- Assignees: Konica Minolta Opto, Inc.
- Inventors: Yasuhiro Matsumoto
- Web page: https://patentgrep.com/patent/US20090256272A1

## CPC

- B29D 11/00596: {Mirrors}
- B29C 33/424: {Moulding surfaces provided with means for marking or patterning (for injection moulding B29C45/372)}
- B29L 2011/0058: {Mirrors}
- G02B 5/10: with curved faces
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

There are provided a method of manufacturing a metal mold suitable for forming, for example, a reflection mirror for a projection optical system and a reflection mirror for the projection optical system manufactured by the method thereof. The method includes a first process of cutting or grinding a metal mold material MM to trim the shape of the transfer optical surface and a second process of radiating the electron beam onto the transfer optical surface so as to perform smoothing process. By radiation of the electron beam, tool makes and the like created on the metal mold material MM in the first process can be erased so that the surface can be smoothed while maintaining the shape of the transfer optical surface.

## Claims

### Claim 1

A manufacturing method of a transfer casting metal mold to cast an optical surface of a reflection mirror used in a projection optical system by transfer casting, comprising:
forming a transfer optical surface by cutting or grinding a metal material in a first process;
wherein a power spectrum density function (hereinafter called a PSD function=A/fB) describing a surface status of the transfer optical surface processed by the first process satisfies that:
1×10−8≦A≦1×10−6 (1)
1/1000<f<1 (2)
1<B<3 (3)
wherein, A denotes a constant (μm3−B), f denotes a space frequency (μm−1) of surface roughness and B denotes an exponent of the space frequency.

### Claim 2 (depends on 1)

The manufacturing method of the transfer casting metal mold of claim 1, further comprising:
performing a smoothing process in a second process by polishing the transfer optical surface after the first process.

### Claim 3 (depends on 1)

The manufacturing method of the transfer casting metal mold of claim 1, further comprising:
performing a smoothing process in a second process by radiating an energy beam onto the transfer optical surface after the first process.

### Claim 4 (depends on 3)

The manufacturing method of the transfer casting metal mold of claim 3, wherein the PSD function of the-transfer optical surface smoothed by the second process satisfies the formula that 1×10−8≦A≦1×10−7 . . . (4) and a maximum value of one of undulations is smaller than a twice the value of a minimum value thereof in the PSD function.

### Claim 5 (depends on 4)

The reflection mirror used in the projection optical system having the optical surface cast by the transfer casting metal mold formed by the manufacturing method of claim 4, wherein the PSD function of the optical surface is within a range of the formula (4).

### Claim 6 (depends on 2)

The manufacturing method of the transfer casting metal mold of claim 2, wherein the PSD function of the transfer optical surface smoothed by the second process satisfies the formula that 1×10−8≦A≦1×10−7 . . . (4) and a maximum value of one of undulations is smaller than a twice the value of a minimum value thereof in the PSD function.